A Comprehensive Study on the Challenges of Using Pure Water Jet as Post-Treatment of Abrasive Water Jet Milled Pockets in Titanium Alloy
Source abstract
Abstract
Abrasive waterjet (AWJ) machining offers the possibility of creating a wide range of features on mechanical parts with different degrees of complexity with a relatively high efficiency. However, after the roughing passes, the surface quality of features such as blind pockets is rather low, with unfavorable implications for surface waviness and form deviations apart from high surface roughness. Apart from the traditional methods for finishing, such as grinding or lapping, it is worth attempting either to improve the surface quality obtained during roughing by an AWJ or to integrate a post-processing step by using a pure WJ in the existing process in order to ameliorate the surface quality. Thus, in the current study, the effect of pure waterjet (WJ) post-processing of machined pockets by AWJ milling on a Ti-6Al-4V workpiece using recycled glass beads was investigated under different conditions. The findings indicate that although the different post-processing treatments by a pure WJ can affect the surface quality on average, these differences are not considerably important, probably due to an insufficient capability of material removal, which hinders the smoothing effect on machined surfaces. Thus, it was indicated that a higher number of post-processing passes under different conditions than those of the roughing pass can be more favorable for efficient post-treatment by a pure WJ.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Erosion and Abrasive Machining · Advanced Surface Polishing Techniques · High-Temperature Coating Behaviors
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Advanced Manufacturing Laboratory, Department of Manufacturing Systems, Faculty of Mechanical Engineering and Robotics, AGH University of Krakow, 30-059 Krakow, Poland
Funding
Polish National Agency for Academic Exchange
References (49)
Show source-provided references
1. High Energy Fluid Jet Machining (HEFJet-Mach): From scientific and technological advances to niche industrial applications10.1016/j.cirp.2014.05.001 ↗
2. Abrasive waterjet machining process: A state of art of review10.1016/j.jmapro.2019.11.030 ↗
3. Thakur, P.M., Raut, D.N., Lade, P.R., and Kudalkar, S. (2023). Development of operations in waterjet technology: A review. Adv. Mater. Process. Technol.10.1080/2374068X.2023.2277983 ↗
4. Titanium alloy milling using abrasive water jet for repair application: Modifications in surface quality and material integrity following plain water jet cleaning10.4028/www.scientific.net/MSF.1016.1374 ↗
5. A comparison of post-processing techniques for Additive Manufacturing components10.1016/j.procir.2022.03.069 ↗
6. Pure waterjet controlled depth machining for stripping ceramic thermal barrier coatings on turbine blades10.1016/j.procir.2019.09.029 ↗
7. An investigation on the efficiency of water-jet technology for graffiti cleaning10.1016/j.culher.2015.11.009 ↗
8. Zahid, M.N., Aziz, R.A., Yusoff, A.R., Yahya, N.M., Aziz, F.A., and Abu, M.Y. (2020). iMEC-APCOMS 2019: Proceedings of the 4th International Manufacturing Engineering Conference and the 5th Asia Pacific Conference on Manufacturing System, Springer. Lecture Notes in Mechanical Engineering.10.1007/978-981-15-0950-6 ↗
9. Effect of Waterjet Cleaning Parameters during Paint Removal Operation on Automotive Steel Components
10. Effect of multiple passes treatment in waterjet peeningon fatigue performance10.1016/j.apsusc.2015.11.195 ↗
11. Influence of waterjet peening and smoothing on the material surface and properties of stainless steel 30410.1016/j.surfcoat.2014.07.013 ↗
12. Soluble Abrasives for Waterjet machining10.1080/10426914.2014.930949 ↗
13. An innovative method to perform maskless plain waterjet milling for pocket generation: A case study in Ti-based superalloys10.1016/j.ijmachtools.2011.04.006 ↗
14. On geometrical accuracy and integrity of surfaces in multi-mode abrasive waterjet machining of NiTi shape memory alloys10.1016/j.cirp.2013.03.021 ↗
15. Preliminary study of abrasive water jet texturing on low thickness UNS A92024 alloy sheets10.1088/1757-899X/1193/1/012027 ↗
16. Multi-scale analysis of the generated damage when machining pockets of 3D woven composite for repair applications using abrasive water jet process: Contamination analysis10.1016/j.compositesa.2020.106118 ↗
17. Surface integrity analysis of plain waterjet milled advanced engineering composite materials10.1016/j.procir.2014.04.063 ↗
18. The effect of pressure fluctuations on the cutting ability of pure water jet
19. Roughening of metallic biomaterials by abrasiveless waterjet peening: Characterization and viability10.1016/j.wear.2011.01.024 ↗
20. The effects of waterjet peening on a random-topography metallic implant surface10.1016/j.euromechsol.2018.03.022 ↗
21. Application of the Taguchi method to areal roughness-based surface topography control by waterjet treatments10.1016/j.apsadv.2023.100548 ↗
22. Experimental investigations on the surface characteristics of abrasive waterjet-milled pockets in aluminium 6061-T6 alloy
23. Surface improvement of laser clad Ti–6Al–4V using plain waterjet and pulsed electron beam irradiation10.1016/j.jmatprotec.2014.11.035 ↗
24. Salinas, L.C., Moussaoui, K., Hejjaji, A., Salem, M., Hor, A., and Zitoune, R. (2021, January 14–16). Multi-scale characterization of material and surface integrity of Inconel 718 when milling by Abrasive Water Jet process: Context of repair application. Proceedings of the ESAFORM 2021—24th International ESAFORM Conference on Material Forming, Liege, Belgium.10.25518/esaform21.4212 ↗
25. Investigation of Waterjet Phases on Material Removal Characteristics10.1016/j.procir.2020.02.319 ↗
26. A study on abrasive waterjet multi-stage machining of ceramics10.1016/j.procir.2022.03.119 ↗
27. Analysis of Alloy 718 surfaces milled by abrasive waterjet and post-processed by plain waterjet technology
28. Surface properties and fatigue failure analysis of alloy 718 surfaces milled by abrasive and plain waterjet10.1007/s00170-017-0979-5 ↗
29. Effect of process parameters of Plain Water Jet on the cleaning quality, surface and material integrity of Inconel 718 milled by Abrasive Water Jet10.1016/j.triboint.2022.108094 ↗
30. Plain water jet cleaning of titanium alloy after abrasive water jet milling: Surface contamination and quality analysis in the context of maintenance10.1016/j.wear.2021.203833 ↗
31. The Impact of Plain Waterjet Machining on the Surface Integrity of Aluminium 747510.1016/j.procir.2014.04.065 ↗
32. Surface modification of Ti6Al7Nb employing pure waterjet and abrasive waterjet polishing for implant application: Comparison study10.1088/2051-672X/ac577e ↗
33. Advantages of water droplet machining over abrasive waterjet cutting of carbon fiber reinforced polymer10.1016/j.mfglet.2022.07.041 ↗
34. Experimental comparison of material removal rates in abrasive waterjet cutting and a novel droplet stream technique
35. Waterjet and Water-Air Jet Surface Processing of a Titanium Alloy: A Parametric Evaluation10.1115/1.4000837 ↗
36. Poloprudský, J., Schüler, M., and Bergs, T. (2022, January 2–3). Erosion of an Air-injected Plain Waterjet (iPWJ). Proceedings of the 2022 WJTA Conference and Expo, New Orleans, LA, USA.
37. Ultrasonic pulsed waterjet surface peening of an industrial aluminum-based metal matrix composite10.1016/j.surfcoat.2021.127795 ↗
38. Water droplet erosion assessment in the initial stages on AISI 316 L using kernel average misorientation10.1016/j.triboint.2023.109165 ↗
39. Nag, A., Srivastava, M., Petru, J., Vanova, P., Srivastava, A.K., and Hloch, S. (2023). Comparison of continuous and pulsating water jet during piercing of ductile material. Materials, 16.10.3390/ma16093558 ↗
40. Post processing of additively manufactured 316L stainless steel by multi-jet polishing method10.1016/j.jmrt.2023.01.054 ↗
41. Experimental research into alternative abrasive material for the abrasive water-jet cutting of titanium
42. Radomska-Zalas, A. (2023). Experimental research on the use of a selected multi-criteria method for the cutting of titanium alloy with an abrasive waterjet. Materials, 16.10.3390/ma16155405 ↗
43. (1996). Geometrical Product Specifications (GPS) (Standard No. ISO 4288:1996).
44. Improving surface hardness of austenitic stainless steel using waterjet peening process10.1007/s00170-012-3962-1 ↗
45. Molnar, V. (2022). Tribological properties and 3D topographic parameters of hard turned and ground surfaces. Materials, 15.10.3390/ma15072505 ↗
46. Parametric and nonparametric description of the surface topography in the dry and MQCL cutting conditions10.1016/j.measurement.2018.02.052 ↗
47. Prediction of the functional performance of machined components based on surface topography: State of the art10.1007/s11665-016-2293-z ↗
48. Topographical analysis of machined surfaces after grinding with different cooling-lubrication techniques10.1016/j.triboint.2019.105962 ↗
49. Comprehensive study on Inconel 718 surface topography after grinding10.1016/j.triboint.2021.106919 ↗