Long-Term Durability of Cement-Treated Soil Used in Offshore Airport Island Construction
Source abstract
Abstract
In port and harbour areas, soft soils such as dredged soil can be solidified by mixing them with cement and other solidifiers in a pumping pipe. This method is known as pneumatic flow mixing. In this method, the soil and solidifiers are stirred and mixed using the turbulence effect of the plug flow generated in the pipe. The authors investigate the long-term durability of the treated soil on the artificial island where this method was first fully introduced. This paper summarises the results of five investigations on the island immediately after construction and 4, 10, 15, and 20 years after construction. No reduction in the unconfined compressive strength or needle penetration gradient was observed in the treated soil. Some degradation was observed at the top and bottom exposed surfaces of the treated soil, similar to that of soil subjected to other treatments. In addition to needle penetration and chemical tests, elemental mapping using an electron beam microanalysis was performed to determine the degree of degradation. The depth of degradation 20 years after construction was 18–25 mm. Although the amount of cement added in the pneumatic flow mixing method was relatively small, this value was within the range of degradation depths over time investigated in previous studies and did not represent a significant degradation.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Geotechnical Engineering and Soil Stabilization · Earthquake and Tsunami Effects · Landfill Environmental Impact Studies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Geotechnical Engineering Department, Port and Airport Research Institute, National Institute of Maritime, Port and Aviation Technology, 3-1-1 Nagase, Yokosuka 2390826, Japan
Facility Service, Central Japan International Airport Co., Ltd., 1-1 Centrair, Tokoname 4798703, Japan
References (25)
Show source-provided references
1. Takahashi, H. (2023). Ground Improvement for Coastal Engineering, CRC Press.
2. Kitazume, M. (2017). The Pneumatic Flow Mixing Method, CRC Press/Balkema.10.1201/9781315375014 ↗
3. Utilization of pneumatic flow tube mixing technique (PFTM) for processing and stabilization of contaminated harbor sediment10.1080/1064119X.2016.1257668 ↗
4. Long-term strength and durability of soil cement10.1061/(ASCE)0899-1561(2001)13:3(161) ↗
5. Kitazume, M., Nakamura, T., Terashi, M., and Ohishi, K. (2003, January 10–12). Laboratory tests on long-term strength of cement treated soil. Proceedings of the 3rd International Conference on Grouting and Ground Treatment, New Orleans, LA, USA.10.1061/40663(2003)31 ↗
6. Hayashi, H., Nishikawa, J., Ohishi, K., and Terashi, M. (2003, January 10–12). Field observation of long-term strength of cement treated soil. Proceedings of the 3rd International Conference on Grouting and Ground Treatment, New Orleans, LA, USA.10.1061/40663(2003)32 ↗
7. Ikegami, M., Ichiba, T., Ohishi, K., and Terashi, M. (2002, January 28–29). Long-term strength change of cement treated soil at Daikoku Pier. Proceedings of the Soft Ground Engineering in Coastal Areas, Yokosuka, Japan.10.1201/9781439833919.ch27 ↗
8. Sulphate attack and ettringite formation in the lime and cement stabilized marine clays10.1016/j.oceaneng.2004.08.012 ↗
9. Nakamura, T., and Kitazume, M. (2006). Technical Note of the Port and Airport Research Institute, Port and Airport Research Institute. (In Japanese).
10. Deterioration mechanism of cement-treated soil under seawater
11. Committee on Geocement (2014). A study on long term stability of soil–cement columns improved by geocement, cement and concrete. Cem. Concr., 804, 9–14. (In Japanese).
12. Deterioration of soil-cement piles in a saltwater region and its influence on the settlement of composite foundations10.1061/(ASCE)CF.1943-5509.0000713 ↗
13. Thirty-seven-year investigation of quicklime-treated soil produced by deep mixing method10.1680/jgrim.17.00044 ↗
14. Kitazume, M., Joyo, T., and Mizoguchi, M. (2006, January 20–22). Characteristics of soil improved by pneumatic flow mixing method after 4 years (translated by authors). Proceedings of the 61st Annual Conference of the Japan Society of Civil Engineers, Kusatsu, Japan. (In Japanese).
15. Morikawa, Y., Yokoe, S., and Kito, J. (2012, January 5–7). Characteristics of soil improved by pneumatic flow mixing method after 10 years (translated by authors). Proceedings of the 67th Annual Conference of the Japan Society of Civil Engineers, Nagoya, Japan. (In Japanese).
16. Morikawa, Y., Takahashi, H., Yokoe, S., and Kito, J. (2018, January 29–31). Characteristics of soil improved by pneumatic flow mixing method after 15 years (translated by authors). Proceedings of the 73rd Annual Conference of the Japan Society of Civil Engineers, Sapporo, Japan. (In Japanese).
17. Sato, T., and Kato, H. (2002, January 16–19). Application of the pneumatic flow mixing method to land development for Central Japan International Airport. Proceedings of the 2002 International Symposium on Underwater Technology, Tokyo, Japan.
18. Development of a pneumatic flow mixing method and its application to Central Japan International Airport construction10.1680/grim.2003.7.3.139 ↗
19. Sato, T. (2004). Technical Note of the Port and Airport Research Institute, Port and Airport Research Institute. (In Japanese).
20. Japanese Geotechnical Society (2015). Japanese Geotechnical Society Standards—Laboratory Testing Standards of Geomaterials, Japanese Geotechnical Society. JGS 0511.
21. Japanese Geotechnical Society (2018). Japanese Geotechnical Society Standards–Geotechnical and Geoenvironmental Investigation Methods, Japanese Geotechnical Society. JGS 3431.
22. Japanese Geotechnical Society (2018). Japanese Geotechnical Society Standards–Laboratory Testing Standards of Geomaterials, Japanese Geotechnical Society. JGS 0211.
23. Japanese Geotechnical Society (2018). Japanese Geotechnical Society Standards–Laboratory Testing Standards of Geomaterials, Japanese Geotechnical Society. JGS 0212.
24. Maruto Co., Ltd. (2006). Penetrometer for Soft Rock: Model SH-70 Instruction Manual, Maruto Co., Ltd.. (In Japanese).
25. Takahashi, H., Morikawa, Y., and Uemura, T. (2021, January 1–17). Trial tests to promote degradation of cement treated soil by percolation technique. Proceedings of the Deep Mixing, Online.