Oxidation behavior and mechanism of powder metallurgy Rene95 nickel based superalloy between 800 and 1000°C
Source abstract
Abstract
Abstract The oxidation behaviors of powder metallurgy (PM) Rene95 Ni-based superalloy in the temperature range of 800–1000 °C are investigated in air by virtue of isothermal oxidation testing, X-ray diffraction, scanning electron microscopy and energy dispersive X-ray spectroscopy. The results show that the oxidation kinetics follows a square power law as the time extends at each temperature. The oxidation layers are detected to be composed of Cr2O3, TiO2 and a small amount of NiCr2O4. The cross-sectional morphologies indicate that the oxidation layer consists of three parts: Cr-rich oxide layer, Cr and Ti duplex oxide layer, and oxidation affected zone. Theoretical analyses of oxidation kinetics and thicknesses of oxidation layers confirm that the activation energy of oxidation of PM Rene95 superalloy is 165.32 kJ mol−1 and the oxidation process is controlled by diffusions of oxygen, Cr, and Ti. Accordingly, a diffusion-controlled mechanism is suggested to understand the oxidation behaviors of PM Rene95 superalloy at elevated temperatures.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: High-Temperature Coating Behaviors · Advanced materials and composites · High Temperature Alloys and Creep
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (25)
Show source-provided references
1. Comparison of prediction methods for low-cycle fatigue life of HIP superalloys at elevated temperatures for turbopump reliability10.1016/j.msea.2009.04.044 ↗
2. On the mechanism of quench cracking in Rene 95 nickel-based superalloy10.1016/j.msea.2005.05.032 ↗
3. Microstructure, properties and heat treatment process of powder metallurgy superalloy FGH9510.1016/S1006-706X(06)60097-6 ↗
4. Oxidation behavior of two nickel-base superalloys used as elevated temperature valves in spark ignited engines and diesel exhaust recirculation (EGR) applications
5. Oxidation behavior of Ni3Al and FeAl intermetallics under low oxygen partial pressures10.1016/S0966-9795(01)00132-7 ↗
6. High temperature oxidation of Nb, NbC and Ni3Nb and oxygen enhanced crack growth10.1016/S1359-6462(99)00336-X ↗
7. Modelling and analysis of the oxidation influence on creep behaviour of thin-walled structures of the single-crystal nickel-base superalloy René N5 at 980°C10.1016/j.actamat.2009.11.004 ↗
8. Thermal oxidation of Ti6Al4V alloy: microstructural and electrochemical characterization10.1016/j.matchemphys.2009.09.007 ↗
9. The effect of yttrium and thorium on the oxidation behavior of Ni–Cr–Al alloys10.1007/BF00604042 ↗
10. Isothermal oxidation resistance comparison between air plasma sprayed, vacuum plasma sprayed and high velocity oxygen fuel sprayed CoNiCrAlY bond coats10.1016/j.surfcoat.2010.01.031 ↗
11. High-temperature oxidation of FGH96 P/M superalloy10.1016/S1006-7191(07)60014-3 ↗
12. Quantitative interpretation of the parabolic and nonparabolic oxidation behavior of nitride ceramic10.1016/j.jeurceramsoc.2008.06.015 ↗
13. Oxidation kinetics of microcrystalline Ni–11.5Cr–4.5Co–0.5Al superalloy sheet fabricated by electron beam physical vapor deposition at 800°C10.1016/j.matlet.2007.05.036 ↗
14. adhesion and growth kinetics of protective scales on metals and alloys10.1007/BF00656571 ↗
15. Enhanced oxidation of nickel in atomic oxygen10.1016/0925-8388(95)01643-0 ↗
16. The influence of aliovalent impurities on the oxidation kinetics of nickel at high temperatures10.1016/j.jpcs.2004.07.011 ↗
17. The degradation of (Ni, Pd) Al coatings on superalloy IN738 during isothermal oxidation10.1016/j.surfcoat.2003.12.004 ↗
18. The oxidation behavior of the new nickel-based superalloy Inconel 740 with and without Na2SO4 deposit10.1016/j.surfcoat.2003.12.003 ↗
19. Research and improvement on structure stability and corrosion resistance of nickel-base superalloy INCONEL alloy 74010.1016/j.matdes.2005.03.015 ↗
20. The corrosion of INCONEL alloy 740 in simulated environments for pulverized coal-fired boiler10.1016/j.matchemphys.2004.04.006 ↗
21. High temperature oxidation studies of detonation-gun-sprayed Cr3C2–NiCr coating on Fe- and Ni-based superalloys in air under cyclic condition at 900°C10.1016/j.jallcom.2008.04.087 ↗
22. Surface orientation dependent oxidation behavior of aluminized DS CM 247 LC nickel-base superalloy10.1016/j.surfcoat.2003.09.066 ↗
23. Oxidation behavior of a single-crystal Ni-base superalloy between 900 and 1000°C in air10.1016/j.jallcom.2009.10.261 ↗
24. Representation of mixed reactive gases on free energy (Ellingham–Richardson) diagrams10.1007/BF02915078 ↗
25. Vacancy injection during oxidation—a re-examination of the evidence10.1016/0001-6160(78)90053-6 ↗