Abstract Laser shock peening with femtosecond laser was used to improve the corrosion resistance of biomedical NiTi alloy without protective coating in the air environment. The energy dispersive X-ray analysis (EDX) and X-ray diffraction (XRD) based analysis showed that the laser ablation could produce titanium oxide layer and femtosecond laser shock peening (FsLSP) can generate residual stress in the surface layer of NiTi alloy. The FsLSP improved the corrosion resistance of NiTi in 3.5% NaCl solution and Hank’s solution and also prevented the formation of corrosion cracks and pits during corrosion testing. The reasons for the improvement of corrosion behavior may be the generation of residual stress and titanium oxide film during the laser surface treatment.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Surface Treatment and Residual Stress · Diamond and Carbon-based Materials Research · Metal and Thin Film Mechanics

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (36)

Show source-provided references
1. Biocompatibility and corrosion behavior of the shape memory NiTi alloy in the physiological environments simulated with body fluids for medical applications10.1016/j.msec.2010.06.007 ↗
2. Reduction of Ni release and improvement of the friction behaviour of NiTi orthodontic archwires by oxidation treatments10.1007/s10856-011-4292-9 ↗
3. Corrosion behaviour of NiTi alloy10.1016/j.electacta.2008.08.001 ↗
4. Effects of carbon and nitrogen plasma immersion ion implantation on in vitro and in vivo biocompatibility of titanium alloy10.1021/am302961h ↗
5. Preparation, characterization, corrosion behavior and cytocompatibility of NiTiO3 nanosheets hydrothermally synthesized on biomedical NiTi alloy10.1016/j.msec.2018.12.124 ↗
6. Electrophoretic deposition of graphene oxide on NiTi alloy for corrosion prevention10.1016/j.vacuum.2018.12.032 ↗
7. Microstructure and corrosion resistance behavior of ceramic coatings on biomedical NiTi alloy prepared by micro-arc oxidation10.1016/j.apsusc.2008.04.068 ↗
8. Surface characterization and tribological performance of laser shock peened steel surfaces10.1016/j.surfcoat.2018.07.087 ↗
9. Improvement of abrasion resistance in artificial seawater and corrosion resistance in NaCl solution of 7075 aluminum alloy processed by laser shock peening10.1016/j.optlaseng.2016.10.016 ↗
10. Investigation of multiple laser shock peening on the mechanical property and corrosion resistance of shipbuilding 5083Al alloy under a simulated seawater environment10.1364/AO.57.006300 ↗
11. Gradient twinning microstructure generated by laser shock peening in an AZ31B magnesium alloy10.1016/j.apsusc.2018.06.176 ↗
12. Enhancement of abrasion and corrosion resistance of duplex stainless steel by laser shock peening10.1016/j.jmatprotec.2012.01.023 ↗
13. Experimental investigation of laser shock peening using femtosecond laser pulses10.2351/1.3573370 ↗
14. Investigation on femto-second laser irradiation assisted shock peening of medium carbon (0.4% C) steel10.1016/j.apsusc.2015.12.058 ↗
15. On femtosecond laser shock peening of stainless steel AISI 31610.1016/j.apsusc.2017.11.145 ↗
16. Femtosecond laser peening of 2024 aluminum alloy without a sacrificial overlay under atmospheric conditions10.2351/1.4967013 ↗
17. Effects of femtosecond laser shock peening in distilled water on the surface characterizations of NiTi shape memory alloy10.1016/j.apsusc.2018.12.087 ↗
18. In vitro response of bone marrow mesenchymal stem cells (hBMSCs) on laser-induced periodic surface structures for hard tissue replacement: Comparison between tantalum and titanium10.1016/j.optlaseng.2018.07.008 ↗
19. Corrosion and characterisation of dual phase Mg–Li–Ca alloy in Hank’s solution: the influence of microstructural features10.1016/j.corsci.2013.10.028 ↗
20. Corrosion behavior of biodegradable Mg-based alloys via femtosecond laser surface melting10.1016/j.apsusc.2018.04.088 ↗
21. High energy femtosecond laser peening of 2024 aluminum alloy10.1016/j.procir.2018.08.141 ↗
22. Biocompatibility of the micro-patterned NiTi surface produced by femtosecond laser10.1016/j.apsusc.2012.08.011 ↗
23. Structural transformation and residual stresses in surface layers of α+ β titanium alloys nanotextured by femtosecond laser pulses10.1007/s00339-014-8954-6 ↗
24. Non-contact ultrasonic acquisition of femtosecond laser-driven ablative Mbar-level shock waves on Ti alloy surface10.1063/1.4942833 ↗
25. Wear and corrosion properties of a low carbon steel processed by means of SMAT followed by lower temperature chromizing treatment10.1016/j.surfcoat.2006.05.019 ↗
26. Electrodeposition of polypyrrole onto NiTi and the corrosion behaviour of the coated alloy10.1016/j.corsci.2009.09.008 ↗
27. Surface characteristics and electrochemical corrosion behavior of fluorinated diamond-like carbon (F-DLC) films on the NiTi alloys10.1016/j.nimb.2009.05.049 ↗
28. Effect of laser shock peening on microstructure and hot corrosion of TC11 alloy10.1016/j.surfcoat.2017.12.003 ↗
29. Effect of surface treatment of NiTi alloy on its corrosion behavior in Hanks’ solution
30. In situ hydrothermal synthesis of oxide film on NiTi for improving corrosion resistance in Hanks’ solution10.1016/j.scriptamat.2006.10.014 ↗
31. Effect of post-weld heat-treatment on the oxide film and corrosion behaviour of laser-welded shape memory NiTi wires10.1016/j.corsci.2011.11.020 ↗
32. Improvement of corrosion resistance of AA2024-T3 using femtosecond laser peening without protective and confining medium10.1016/j.corsci.2018.08.030 ↗
33. Investigation of corrosion behaviour of aluminium alloy subjected to laser shock peening without a protective coating10.1155/2015/705306 ↗
34. Corrosion resistance of porous NiTi biomedical alloy in simulated body fluids10.1088/0964-1726/25/9/095024 ↗
35. Corrosion products and mechanism on NiTi shape memory alloy in physiological environment10.1557/JMR.2010.0051 ↗
36. Assessment of nickel titanium and beta titanium corrosion resistance behavior in fluoride and chloride environments10.2319/091712-740.1 ↗