An atomic-scale and high efficiency finishing method of zirconia ceramics by using magnetorheological finishing
Source abstract
Abstract
Abstract Zirconia ceramics is a valuable crucial material for fabricating functional components applied in aerospace, biology, precision machinery, military industry and other fields. However, the properties of its high brittleness and high hardness could seriously reduce its finishing efficiency and surface quality by conventional processing technology. In this work, we present a high efficiency and high-quality finishing process by using magnetorheological finishing (MRF), which employs the permanent magnetic yoke with straight air gap as excitation unit. The sub-nanoscale surface roughness and damage free surface can be obtained after magnetorheological finishing. The XRD results and SEM morphologies confirmed that the mechanical shear removal with ductile modes are the dominant material removal mechanism for the magnetorheological finishing of zirconia ceramic. With the developed experimental apparatus, the effects of workpiece speed, trough speed and work gap on material removal rate and surface roughness were systematically investigated. Zirconia ceramics finished to ultra-smooth surface with surface roughness less than Ra 1 nm was repeatedly achieved during the parametric experiments. Additionally, the highest material removal rate exceeded 1 mg/min when using diamond as an abrasive particle. Magnetorheological finishing promises to be an adaptable and efficient method for zirconia ceramics finishing.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced Surface Polishing Techniques · Advanced materials and composites · Bone Tissue Engineering Materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (30)
Show source-provided references
1. Effect of core ceramic grinding on fracture behaviour of bilayered zirconia veneering ceramic systems under two loading schemes10.1016/j.dental.2016.06.007 ↗
2. Effect of polishing method on surface roughness and bacterial adhesion of zirconia-porcelain veneer10.1016/j.ceramint.2016.11.036 ↗
3. An overview of zirconia ceramics: Basic properties and clinical applications10.1016/j.jdent.2007.07.008 ↗
4. Effect of process parameters on MRR, TWR and surface topography in ultrasonic machining of alumina-zirconia ceramic composite10.1016/j.ceramint.2014.04.137 ↗
5. Microstructure and mechanical properties of in-situ grown mullite toughened 3Y-TZP zirconia ceramics fabricated by gelcasting10.1016/j.ceramint.2017.09.151 ↗
6. Zirconia ceramic and Nb joints brazed with Mo-particle-reinforced Ag-Cu-Ti composite fillers: Interfacial microstructure and formation mechanism10.1016/j.ceramint.2017.04.133 ↗
7. The ultra-precision Ud-lap grinding of flat advanced ceramics10.1016/j.jmatprotec.2015.10.003 ↗
8. Study on cutting force model in ultrasonic vibration assisted side grinding of zirconia ceramics10.1016/j.ijmachtools.2016.01.004 ↗
9. Controlled material removal mode and depth of micro cracks in precision grinding of fused silica – A theoretical model and experimental verification10.1016/j.ceramint.2017.05.327 ↗
10. Nanofinishing of a typical 3D ferromagnetic workpiece using ball end magnetorheological finishing process10.1016/j.ijmachtools.2012.07.002 ↗
11. Effect of lapping slurry on critical cutting depth of spinel10.1016/j.apsusc.2015.04.092 ↗
12. Optimized pre-thinning procedures of ion-beam thinning for TEM sample preparation by magnetorheological polishing10.1016/j.ultramic.2017.05.016 ↗
13. Magnetorheological polishing using a permanent magnetic yoke with straight air gap for ultra-smooth surface planarization10.1016/j.precisioneng.2014.11.001 ↗
14. Magnetorheological (MR) polishing of alumina-reinforced zirconia ceramics using diamond abrasives for dental application10.1080/10426914.2011.654155 ↗
15. Analyzing and improving surface texture by dual-rotation magnetorheological finishing10.1016/j.apsusc.2015.11.009 ↗
16. Atomic-scale finishing of carbon face of single crystal SiC by combination of thermal oxidation pretreatment and slurry polishing10.1016/j.apsusc.2017.10.159 ↗
17. Study on planarization machining of sapphire wafer with soft-hard mixed abrasive through mechanical chemical polishing10.1016/j.apsusc.2016.07.155 ↗
18. Microstructural changes in ground 3Y-TZP and their effect on mechanical properties10.1016/j.actamat.2011.07.024 ↗
19. In vitro cell proliferation and mechanical behaviors observed in porous zirconia ceramics10.3390/ma9040218 ↗
20. Mechanical performance of polymer-infiltrated zirconia ceramics10.1016/j.jdent.2017.01.008 ↗
21. Mechanical behavior of a Y-TZP ceramic for monolithic restorations: Effect of grinding and low-temperature aging10.1016/j.msec.2016.02.049 ↗
22. Preparation and optical properties of infrared transparent 3Y-TZP ceramics
23. Surface quality of yttria-stabilized tetragonal zirconia polycrystal in CAD/CAM milling, sintering, polishing and sandblasting processes10.1016/j.jmbbm.2016.08.021 ↗
24. Microstructural changes produced by abrading Y-TZP in presintered and sintered conditions10.1016/j.jdent.2012.06.009 ↗
25. Clinical and laboratory surface finishing procedures for zirconia on opposing human enamel wear: A laboratory study10.1016/j.jmbbm.2015.06.007 ↗
26. Effect of abrasive grinding on the strength of Y-TZP10.1016/j.jeurceramsoc.2009.02.011 ↗
27. Sintering of zirconia ceramics by intense high-energy electron beam10.1016/j.ceramint.2016.05.198 ↗
28. Sintering kinetic window for yttria-stabilized cubic zirconia10.1016/j.jeurceramsoc.2015.12.044 ↗
29. Determination of fracture toughness of zirconia ceramics with different yttria concentrations by SEVNB method10.1016/j.ceramint.2017.04.064 ↗
30. Characterization of three commercial Y-TZP ceramics produced for their high-translucency, high-strength and high-surface area10.1016/j.ceramint.2015.09.033 ↗