journal article·2011-11

Microstructure and mechanical properties of ultrafine WC–Ni–VC–TaC–cBN cemented carbides fabricated by spark plasma sintering

Huiyong Rong, Zhijian Peng, Xiaoyong Ren, Chengbiao Wang, Zhiqiang Fu, Longhao Qi, Hezhuo Miao

Publisher page

Abstract

Abstract Ultrafine WC–Ni–VC–TaC cemented carbides with different amounts of cubic boron nitride (cBN) were fabricated by spark plasma sintering, and the microstructure and mechanical properties of the as-prepared cermets were investigated. Scanning electron microscopy observations showed that the size of WC grains in the cermet samples was 0.2–0.4 μm. After the addition of cBN, the samples were still quite dense with the highest relative density of almost 98% when the addition fraction of cBN was 50 vol.%, although some micropores might exist in the samples. X-ray diffraction results indicated that no phase transformation of cBN was detected. The relative density and hardness of the cemented carbides increased with the addition fraction of cBN, but their strength decreased. When the fraction of cBN increased from 0 up to 50 vol.%, the hardness of the samples increased from 2100 to 3200 HV, but the flexural strength decreased from 1950 to 1250 MPa.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (28)

Show source-provided references
1. Rotating wheel abrasion of WC/Co hardmetals10.1016/j.wear.2004.09.028 ↗
2. Rapid sintering of ultrafine WC–Ni cermets10.1016/j.ijrmhm.2005.07.002 ↗
3. Properties of ultrafine grain binderless cemented carbide RCCFN10.1016/0263-4368(95)92676-B ↗
4. Improvement of adhesive strength and surface roughness of diamond films on Co-cemented tungsten carbide tools10.1016/S0925-9635(02)00345-X ↗
5. A study of diamond film deposition on WC–Co inserts for graphite machining: effectiveness of SiC interlayers prepared by HFCVD10.1016/j.diamond.2008.03.017 ↗
6. Alloyed W–(Co, Ni, Fe)–C phases for reaction sintering of hardmetals10.1016/j.ijrmhm.2010.06.003 ↗
7. Liquid phase sintering and oxidation resistance of WC–Ni–Co–Cr cemented carbides10.1016/j.ijrmhm.2010.02.010 ↗
8. An in situ WC–Ni composite fabricated by the SHS method
9. Identification of optimum binder phase compositions for improved WC hard metals10.1016/0025-5416(88)90502-2 ↗
10. Sparking plasma sintering of nanometric tungsten carbide10.1016/j.ijrmhm.2008.06.004 ↗
11. Effects of addition carbides on the grain size of WC–Co alloy10.2497/jjspm.19.67 ↗
12. Zackrisson · Int J Refract Met Hard Mater · 1998 · 16 · 41710.1016/S0263-4368(98)00048-1 ↗
13. Development of WC base cemented carbides to use Ni instead of Co
14. WC grain growth and grain growth inhibition in nickel and iron binder hardmetals10.1016/S0263-4368(01)00070-1 ↗
15. Delanoe · 2005 · 2 · 642
16. Frisk · 2005 · 2
17. Effect of Cr and V on phase equilibria in Co–WC based hardmetals10.3139/146.101632 ↗
18. Frisk · 2009 · HM 1 · 1
19. Hashiya · 2009 · HM 55 · 1
20. Microstructure and mechanical properties of WC Ni–Si based cemented carbides developed by powder metallurgy10.1016/j.ijrmhm.2010.04.003 ↗
21. Making hardmetal even harder with dispersed cBN10.1016/S0026-0657(07)70124-8 ↗
22. Cubic boron nitride based metastable coatings and nanocomposites10.1016/j.tsf.2009.09.109 ↗
23. Liquid phase sintering of tough coated hard particles10.1016/j.ijrmhm.2005.05.018 ↗
24. Microstructure, hardness and toughness of nanostructured and conventional WC–Co composites10.1016/S0965-9773(98)00123-8 ↗
25. Determination of three-dimensional grain size distribution by linear intercept measurement10.1016/S1359-6454(97)00442-4 ↗
26. Hardness and deformation of cemented tungsten carbide10.1016/0025-5416(78)90163-5 ↗
27. Fabrication of WC-8 wt.%Co hard materials by two rapid sintering processes10.1016/j.ijrmhm.2006.09.001 ↗
28. Consolidation of ultra fine WC and WC–Co hard materials by pulsed current activated sintering and its mechanical properties10.1016/j.ijrmhm.2005.11.004 ↗