Peculiarities of vacuum annealing of nanocrystalline WC powders
Source abstract
Abstract
Abstract The effect of vacuum annealing temperature on the phase and chemical composition, particle size, and microstrains of nanocrystalline powders of tungsten carbide WC with particles from 20 to 60 nm in size has been studied using X-ray diffraction and electron microscopy methods. It is established that nanocrystalline WC powders stored in air, contain from 1 to 2 wt.% of impurity oxygen. It is found that vacuum annealing of WC nanopowders at a temperature up to 1400 °C is accompanied by appreciable decarburization and variation in the phase composition due to carbon desorption as a result of interaction with impurity oxygen. Annealing leads to coarsening of powder particles caused by intergrowth of aggregated nanoparticles and to decreasing microstrains.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (33)
Show source-provided references
1. Nanocrystalline materials: A study of WC-based hard metals10.1016/S0079-6425(97)00021-2 ↗
2. Processing and properties of nanostructured WC-Co10.1016/0965-9773(92)90063-4 ↗
3. Low and high temperature hardness of WC-6 wt.% Co alloys10.1016/S0263-4368(97)81231-0 ↗
4. Vacuum sintering of WC – 8 wt.% Co hardmetals from WC powders with different dispersity10.1016/j.ijrmhm.2010.10.010 ↗
5. Gusev · 2004
6. Gusev · 2007
7. Nanotechnologies. Properties and applications of nanostructured materials10.1070/RC2007v076n05ABEH003674 ↗
8. Model for milling of powders
9. Tsvetkov · 1980
10. Effect of WC nanoparticle size on the sintering temperature, density, and microhardness of WC-8 wt.% Co alloys10.1134/S0020168509040098 ↗
11. Effect of sintering temperature on the phase composition and microhardness of WC–8 wt % Co cemented carbide10.1134/S002016850706009X ↗
12. Particle size effects on the oxidation of tungsten carbide powders
13. Effect of particle size on the oxidation of WC powders during heating10.1134/S0020168511020099 ↗
14. Determination of oxygen in W-C-Co nanopowders (in Russian)10.1134/S0020168508090100 ↗
15. Preparation and surface composition of tungsten carbide powders with high specific surface area10.1021/cm00017a015 ↗
16. Production of nanocrystalline powders by high-energy ball milling: model and experiment10.1088/0957-4484/19/26/265302 ↗
17. Production of nanocrystalline powder of WC via ball-milling
18. Creation of plasma-chemical equipment for manufacture of ultrafine powders of refractory metals and compounds
19. Phase equilibria in the W – C system and tungsten carbides10.1070/RC2006v075n07ABEH003606 ↗
20. Neutron and x-ray diffraction study and symmetry analysis of phase transformations in lower tungsten carbide W2C10.1103/PhysRevB.76.174115 ↗
21. Determination of the particle sizes, microstrains, and degree of inhomogeneity in nanostructured materials from X-ray diffraction data
22. Oxidation of tungsten and tungsten carbide in dry and humid atmosphere10.1016/S0263-4368(96)00027-3 ↗
23. Interaction of O2 with WC (0001)10.1016/S0039-6028(98)00193-9 ↗
24. Tungsten carbides and W – C phase diagram10.1134/S0020168506020051 ↗
25. The heat of sublimation of carbon10.1021/j150524a001 ↗
26. Thermodynamic Properties of Carbides
27. Kulikov · 1988
28. Properties, Production and Application of Refractory Compounds
29. Nanostructure and atomic ordering in vanadium carbide
30. Mechanism of enlarging the nanoparticles of niobium, molybdenum, and tungsten during annealing in vacuum and hydrogen
31. Klyachko · 1999
32. Decarburization of tungsten carbide during electrochemical application of cobalt coatings in aqueous solutions10.1007/BF00802442 ↗
33. Sintering of nanostructured hard alloys