journal article·2018-11Open access

Erasing and rewriting of titanium oxide colour marks using laser-induced reduction/oxidation

Tahseen Jwad, Marc Walker, Stefan Dimov

Abstract

Abstract Laser-induced oxidation of metallic surfaces such as titanium is used in many application areas for colour marking due to its selectivity, cleanness and processing speed. However, as the generated colours are permanent this reduces the flexibility and applicability of this laser processing technology. Therefore, a method is reported in this paper to erase selectively the oxide-based colours using laser-induced oxygen reduction. Especially, the colour marks are reprocessed in a low oxygen environment employing a nanosecond laser. A low fluence was used in order to diffuse oxygen out into the atmosphere and yield a lower form of metal oxides or a pure metal. Any cumulative fluence exceeding 25 J/cm2 was sufficient to erase any laser-induced colours on titanium substrates. The XPS analysis revealed that all fields were mainly comprised of TiO2 prior to erasing with only small contributions from Ti2O3 and TiO/TiN. Following the proposed laser-induced oxygen reduction, the relative concentration of TiO2 decreased substantially while the overall amount of Ti in the near surface region increased. The results clearly show that the erasing of oxide-based colour marks is only due to oxygen diffusion back into the atmosphere and there were not any signs of laser ablation.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Laser Material Processing Techniques · Advanced Surface Polishing Techniques · Laser-induced spectroscopy and plasma

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (44)

Show source-provided references
1. I.W. Boyd, Laser processing of thin films and microstructures: oxidation, deposition, and etching of insulators, Springer series in materials science, vol. viii, Springer-Verlag, Berlin, New York, 1987, 320p.10.1007/978-3-642-83136-2 ↗
2. V. Veiko et al., Thermochemical action of laser radiation, in: Soviet Physics Doklady, 1973.
3. V. Veiko, et al., Thermochemical action of laser radiation, in: Soviet Physics Doklady, 1973.
4. Coloring of titanium by pulsed laser processing in air10.1016/S0040-6090(02)00632-6 ↗
5. Oxidation of titanium through Nd:YAG laser irradiation10.1016/S0169-4332(02)00447-6 ↗
6. Laser surface processing of titanium in air: influence of scan traces overlapping10.2351/1.1567747 ↗
7. Pulsed laser growth and characterization of thin films on titanium substrates10.1016/j.apsusc.2007.02.136 ↗
8. Nanosecond pulsed laser irradiation of titanium: oxide growth and effects on underlying metal10.1016/j.surfcoat.2013.12.052 ↗
9. Composition analysis of oxide films formed on titanium surface under pulsed laser action by method of chemical thermodynamics10.1088/1555-6611/aa5c11 ↗
10. Growth of amorphous Ti2O3 layers by laser-induced oxidation10.1063/1.95424 ↗
11. Laser-produced Ti/Ti-oxide thin-film structures10.1063/1.95933 ↗
12. Compositional and micro-scratch analyses of laser induced colored surface of titanium10.1016/j.optlaseng.2016.03.026 ↗
13. Optical-constants of transition-metals - Ti, V, Cr, Mn, Fe Co, Ni, and Pd10.1103/PhysRevB.9.5056 ↗
14. Optical-properties of Al, Fe, Ti, Ta, W, and Mo at submillimeter wavelengths10.1364/AO.27.001203 ↗
15. Ion · 2005
16. Bäuerle · 2011
17. Brunette · 2001
18. Standard Practice for Permanent Marking of Orthopaedic Implant Components, 2013.
19. Standard Practice for Surface Preparation and Marking of Metallic Surgical Implants.
20. Solubility of metal oxides in deep eutectic solvents based on choline chloride10.1021/je060038c ↗
21. Z. Hongyu, Laser-induced colours on metal surfaces, in: SIMTech Technical Report PT/01/005/AM, 2001.
22. New laser surface treatments: cleaning, de-rusting, de-oiling, de-painting, de-oxidizing and de-greasing10.1117/12.281099 ↗
23. Laser decoration of precious metals10.3103/S1062873817120310 ↗
24. Laser coloration of titanium films: new development for jewelry and decoration10.1016/j.optlastec.2017.01.036 ↗
25. Lugomer · 1990
26. J. Kumstel, B. Kirsch, Polishing titanium- and nickel-based alloys using cw-laser radiation. Lasers in Manufacturing (Lim 2013), 2013, 41, 355–364.10.1016/j.phpro.2013.03.089 ↗
27. Characteristics of laser-heated titanium in a nitrogen atmosphere10.1007/BF03054105 ↗
28. Surface nitridation of titanium by pulsed Nd : YAG laser irradiation10.1016/S0169-4332(01)00612-2 ↗
29. Selectable surface nitridation of titanium using focused pulsed Nd:YAG laser irradiation with nitrogen gas blow10.1016/j.surfcoat.2014.02.068 ↗
30. Comparison of surface films formed on titanium by pulsed Nd:YAG laser irradiation at different powers and wavelengths in nitrogen atmosphere10.1016/j.apsusc.2010.02.040 ↗
31. An investigation of pulsed laser cutting of titanium alloy sheet10.1016/j.optlaseng.2005.09.003 ↗
32. Inert gas cutting of titanium sheet with pulsed mode CO2 laser10.1016/j.optlaseng.2004.12.009 ↗
33. Otto · 1984
34. Laser-induced surface metallization of ceramic Plzt10.1007/BF00616056 ↗
35. Laser-induced surface reduction of the high-Tc superconductor Yba2cu3o7-X10.1007/BF00617937 ↗
36. Laser writing and rewriting on Yba2cu3o7 films10.1063/1.105310 ↗
37. Rewriting of low electrical resistance lines on TiO2 film by writing and erasing with femtosecond and CW fiber lasers10.1016/j.apsusc.2014.06.062 ↗
38. Laser-induced oxidation of titanium substrate: analysis of the physicochemical structure of the surface and sub-surface layers10.1016/j.apsusc.2014.11.062 ↗
39. Substrate cracking in Ti-6Al-4V driven by pulsed laser irradiation and oxidation10.1016/j.surfcoat.2017.05.001 ↗
40. Cracks growth behaviors of commercial pure titanium under nanosecond laser irradiation for formation of nanostructure-covered microstructures (with sub-5-mu m)10.1016/j.apsusc.2016.06.083 ↗
41. Evaluation of uniform color spaces developed after the adoption of Cielab and Cieluv10.1111/j.1520-6378.1994.tb00070.x ↗
42. Structure formation on titanium during oxidation induced by cumulative pulsed Nd:YAG laser irradiation10.1007/s00339-002-2054-8 ↗
43. Resolving surface chemical states in XPS analysis of first row transition metals, oxides and hydroxides: Sc, Ti, V, Cu and Zn10.1016/j.apsusc.2010.07.086 ↗
44. The thickogram: a method for easy film thickness measurement in XPS10.1002/1096-9918(200006)29:6<403::AID-SIA884>3.0.CO;2-8 ↗