journal article·2024-09

Effect of cobalt content on the microstructure, microtexture, and mechanical properties of W-Ni-Fe-xCo alloys during solid-phase-sintering and liquid-phase-sintering

Yanzhang Dai, Kun Li, Jianpeng Zou, Bin Liu, Yong Liu, Yuankui Cao, Huichao Cheng

Publisher page

Abstract

Compared the effect of Co content on the microstructure, microtexture, and mechanical properties of W-Ni-Fe-xCo alloys during solid-phase-sintering and liquid-phase-sintering. The results indicated there is a non-uniform distribution of W and γ phases, accompanied by the presence of little voids during solid-phase-sintering at 1420 °C. Adding Co element enhances the wetting between the W and γ phases, and reduces the liquid-phase-sintering temperature, shrinking the size and quantity of pores. The W phase transforms into ball-shaped particles with completed liquid-phase-sintering at 1440 °C. With increased Co content, W grain size decreases, matrix fraction volume increases, and C w-w continuity and dihedral angle decrease. The mechanical properties of the alloys improve with sintering temperature and Co content, the tensile strength and elongation reached 989 MPa and 13.7% due to the elimination of holes and the W content increased within γ phase. The relationship among W content in γ phase, strength, elongation, and microhardness with Co content were revealed. The solution strengthening effect increases, which drives the co-deformation of W and γ phases, thereby increasing the strength and elongation. The addition of Co element and the atomic diffusion at high temperature made the fibre microtexture more concentrated.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (30)

Show source-provided references
1. Sintered tungsten heavy alloys: review of microstructure, strength, densification, and distortion
2. On the remarkable fracture toughness of 90 to 97W-NiFe alloys revealing powerful new ductile phase toughening mechanisms10.1016/j.actamat.2020.01.012 ↗
3. A novel dissolution-precipitation mechanism during liquid phase sintering and its strengthening effects in W-Ni-Fe alloys with low W contents10.1016/j.matdes.2022.110841 ↗
4. Influence of cobalt content on the microstructure and texture evolution of hot-pressed sintered tungsten heavy alloy
5. Recent progress in research on tungsten materials for nuclear fusion applications in Europe10.1016/j.jnucmat.2012.08.018 ↗
6. Microstructure, grain growth behavior and mechanical properties of W-CoCuFeNi tungsten heavy alloys prepared by infiltration10.1016/j.ijrmhm.2021.105572 ↗
7. Recent progress in processing of tungsten heavy alloys10.1155/2014/764306 ↗
8. Effect of cobalt addition on microstructure and mechanical properties of tungsten heavy alloys10.1007/s12666-017-1074-1 ↗
9. On the main mechanisms for defeating AP projectiles, long rods and shaped charge jets10.1016/j.ijimpeng.2008.09.003 ↗
10. Microstructure and mechanical properties of hot isostatic pressed tungsten heavy alloy with FeNiCoCrMn high entropy alloy binder10.1016/j.jmrt.2022.12.078 ↗
11. Effect of cold swaging and heat treatment on properties of the P/M 91W-6Ni-3Co heavy alloy10.2298/SOS0803319K ↗
12. Effect of swaging on microstructure and mechanical properties of liquid-phase sintered 93W-4.9 (Ni, Co)-2.1 Fe alloy10.1016/j.ijrmhm.2014.01.016 ↗
13. Processing and microstructural characterization of liquid phase sintered tungsten–nickel–cobalt heavy alloys10.1016/j.ijrmhm.2014.12.009 ↗
14. Investigation of deformation and heat treatment effects on properties of PM 92.5 W-5Ni-2.5 Fe heavy alloys10.1179/003258904225015509 ↗
15. Evolution of cobalt-free tungsten heavy alloys for kinetic energy penetrators10.1179/0032589913Z.000000000137 ↗
16. Impact of mechanical activation on sintering kinetics and mechanical properties of ultrafine-grained 95W-Ni-Fe tungsten heavy alloys10.1016/j.jallcom.2018.09.176 ↗
17. A review on lower sintering temperature tungsten alloys
18. Fine-grained 93W-5.6Ni-1.4Fe heavy alloys with enhanced performance prepared by spark plasma sintering10.1016/j.msea.2013.02.069 ↗
19. Effects of sintering temperature on fine-grained tungsten heavy alloy produced by high-energy ball milling assisted spark plasma sintering10.1016/j.ijrmhm.2012.02.017 ↗
20. Effect of composition, heat treatment and deformation on mechanical properties of tungsten heavy alloys10.1016/j.msea.2018.07.070 ↗
21. Microstructure and mechanical properties of mechanically alloyed and solid-state sintered tungsten heavy alloys10.1016/S0921-5093(00)00968-0 ↗
22. Investigation of the rotary swaging and heat treatment on the behavior of W-and γ-phases in PM 92.5 W–5Ni–2.5 Fe–0.26 Co heavy alloy10.1016/j.msea.2008.05.021 ↗
23. Microstructure and mechanical properties of super-strong nanocrystalline tungsten processed by high-pressure torsion10.1016/j.actamat.2006.05.005 ↗
24. Effect of Mn addition in W-Ni-cu heavy alloy processed through hot press sintering techniques on microstructure, microtexture and grain boundary character evolution
25. Grain boundary diffusion and grain boundary phase transition in tungsten in the temperature range of activated sintering10.1515/ijmr-2023-0169 ↗
26. Texture and differential stress development in W/Ni-co composite after rotary swaging10.3390/ma13122869 ↗
27. Hosford · 2010
28. Suwas · 2014
29. Tungsten heavy alloy: deformation texture and recrystallization of tungsten particles10.1016/S0263-4368(02)00035-5 ↗