journal article·2004-09

Synthesis and characterisation of pack cemented aluminide coatings on metals

C Houngninou, S Chevalier, J.P Larpin

Applied Surface Science· Volume 236· Issue 1-4
Publisher page

Abstract

Abstract The exposition of metallic materials to high temperature environments leads to their corrosion because of oxidation or sulphidation. One way to protect such materials is to produce an Al 2 O 3 layer which needs to be continuous enough to limit diffusion of oxygen or metallic elements, and withstand this corrosion. Since a few years, it has been proved that aluminide compounds are one of the most effective materials to achieve this goal. Indeed, they possess sufficient Al and many beneficial mechanical properties when exposed to high temperature conditions to make possible the formation of a protective Al 2 O 3 scale. This study is aimed at the elaboration of iron, nickel and molybdenum aluminides by modification of the surface of the base materials by a pack cementation process. The as-cemented alloys were analysed by means of SEM coupled with EDX and by XRD. Cross-section examinations showed, in each case, a progressive diffusion of aluminium through the substrates. The diffusion thickness layer was more or less important depending on the base material and on the coating conditions.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Intermetallics and Advanced Alloy Properties · High-Temperature Coating Behaviors · Advanced ceramic materials synthesis

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (44)

Show source-provided references
1. P. Tomaszewicz, G.R. Wallwork, High Temperature Corrosion, vol. 6, NACE, Houston, 1983, pp. 258–266.
2. R.A. Perkins, High Temperature Corrosion, vol. 6, NACE, Houston, 1983, pp. 345–353.
3. Stoloff · Mater. Sci. Eng. · 1998 · A258 · 110.1016/S0921-5093(98)00909-5 ↗
4. Sundar · Mater. Sci. Eng. · 1998 · A258 · 21910.1016/S0921-5093(98)00937-X ↗
5. G. Sauthoff, State of intermetallics development, in: H.J. Grabke, M. Schütze (Eds.), Oxidation of Intermetallics, Wiley–VCH, 1998, pp. 3–13.10.1002/9783527612413.ch01 ↗
6. G.H. Meier, Research on oxidation and embrittlement on intermetallic compounds in the U.S., in: H.J. Grabke, M. Schütze (Eds.), Oxidation of Intermetallics, Wiley–VCH, 1998, pp. 15–57.10.1002/9783527612413.ch02 ↗
7. Goward · Surf. Coat. Technol. · 1998 · 108–109 · 7310.1016/S0257-8972(98)00667-7 ↗
8. Paidar · Mater. Sci. Eng. A · 1997 · 234–236 · 1510.1016/S0921-5093(97)00149-4 ↗
9. Yamaguchi · Acta Mater. · 2000 · 48 · 30710.1016/S1359-6454(99)00301-8 ↗
10. Stein-Fechner · J. Nucl. Mater. · 1997 · 249 · 3310.1016/S0022-3115(97)00208-0 ↗
11. Mevrel · Mater. Sci. Eng. · 1987 · 88 · 110.1016/0025-5416(87)90060-7 ↗
12. Prescott · Oxid. Met. · 1992 · 38 · 7310.1007/BF00665045 ↗
13. Montealegre · Intermetallics · 2000 · 8 · 43910.1016/S0966-9795(99)00168-5 ↗
14. R.W. Cahn, P. Haasen, E.J. Kramer, Corrosion and environmental degradation of materials, Mater. Sci. Technol. 19 (2000).
15. Chan · Intermetallics · 2001 · 9 · 81710.1016/S0966-9795(01)00065-6 ↗
16. Xu · Scripta Mater. · 2000 · 41 · 97510.1016/S1359-6462(00)00327-4 ↗
17. Lee · Mater. Sci. Eng. · 2003 · A339 · 10910.1016/S0921-5093(02)00112-0 ↗
18. Rommerskirchen · Mater. Corros. · 1996 · 47 · 64610.1002/maco.19960471109 ↗
19. Li · J. Mater. Sci. · 2001 · 36 · 97910.1023/A:1004884009018 ↗
20. Rao · Intermetallics · 2003 · 11 · 11910.1016/S0966-9795(03)00071-2 ↗
21. Lang · Intermetallics · 2003 · 11 · 69710.1016/S0966-9795(03)00067-0 ↗
22. Lang · Intermetallics · 2003 · 11 · 13510.1016/S0966-9795(02)00190-5 ↗
23. G. Béranger, J.C. Colson, F. Dabosi, Corrosion des matériaux à haute température, Les éditions de physique, Paris, 1987.
24. J. Bénard, L’oxydation des métaux, Gauthier-Villars et Cie, Paris, 1962.
25. F. Fitzer, J. Schlichting, Coatings containing chromium, aluminium and silicon for high temperature alloys, High Temperature Corrosion, vol. 6, NACE, Houston, 1983, pp. 604–614.
26. P. Sarrazin, A. Galerie, J. Fouletier, Les mécanismes de la corrosion sèche: une approche cinétique, EDP Sciences, Paris, 2000.10.1051/978-2-7598-0243-2 ↗
27. I. Rommerskirchen, V. Kolarik, Oxidation of β-NiAl, undoped and doped with Ce, Y, Hf, in: H.J. Grabke, M. Schütze (Eds.), Oxidation of Intermetallics, Wiley–VCH, 1998, pp. 109–120.10.1002/9783527612413.ch07 ↗
28. J.C. Yang, TEM investigations of metastable aluminas on oxidised NiAl, in: Proceedings of the Third International Conference on the Microscopy of Oxidation, Newcomb and Little Ed., 1996, pp. 256–264.
29. R. Klumpes, C.H.M. Marrée, E. Schramm, J.H.W.d. Wit, The influence of chromium on the oxidation of β-NiAl at 1000°C, in: H.J. Grabke, M. Schütze (Eds.), Oxidation of Intermetallics, Wiley–VCH, 1998, pp. 99–107.10.1002/9783527612413.ch06 ↗
30. Levin · Surf. Coat. Technol. · 1998 · 106 · 20910.1016/S0257-8972(98)00529-5 ↗
31. Tsai · Thin Solid Films · 2000 · 366 · 16410.1016/S0040-6090(00)00723-9 ↗
32. Kim · Surf. Coat. Technol. · 2002 · 161 · 21810.1016/S0257-8972(02)00498-X ↗
33. Maragoudakis · Mater. Lett. · 2002 · 53 · 40610.1016/S0167-577X(01)00515-8 ↗
34. Christoglou · Surf. Coat. Technol. · 2002 · 155 · 5110.1016/S0257-8972(02)00044-0 ↗
35. Xiang · J. Mater. Sci. · 2001 · 36 · 567310.1023/A:1012534220165 ↗
36. Hearley · Surf. Coat. Technol. · 2000 · 123 · 21010.1016/S0257-8972(99)00511-3 ↗
37. Hodge · Intermetallics · 2001 · 9 · 58110.1016/S0966-9795(01)00047-4 ↗
38. Voudouris · Surf. Coat. Technol. · 2001 · 141 · 27510.1016/S0257-8972(01)01193-8 ↗
39. Basuki · Mater. Sci. Eng. · 1997 · A224 · 2710.1016/S0921-5093(96)10556-6 ↗
40. Zheng · Oxid. Met. · 1998 · 49 · 1910.1023/A:1018870105824 ↗
41. Das · Metall. Mater. Trans. · 1998 · 29A · 217310.1007/s11661-998-0042-0 ↗
42. Chien · Mater. Sci. Eng. · 1996 · A206 · 21510.1016/0921-5093(95)09899-2 ↗
43. Costa · Surf. Coat. Technol. · 1996 · 88 · 16510.1016/S0257-8972(96)02921-0 ↗
44. Huang · Mater. Sci. Eng. · 2002 · A328 · 23810.1016/S0921-5093(01)01699-9 ↗