Abstract

Abstract Four types of silicon carbide/carbon nanotubes composites were prepared with the main aim to develop ceramics with enhanced electrical conductivity. The SiC/CNT composites were prepared by in-situ growth of CNT on the SiC powder grains. Three types of SiC/CNT composites, where the precursor SiC/CNT powder mixture was prepared by Catalytic Chemical Vapour Deposition (CCVD) method and different amounts of Fe catalytic nanoparticles (2.5, 5, 10 wt% Fe), were designed. In addition, one reference material containing 2.5 wt% Fe catalytic nanoparticles but without CCVD application, i.e. without CNT, was prepared in order to correctly assess the role of CNT. The experimental materials were compacted by hot pressing (1850 °C/Ar/60 min/40 MPa). Mechanical properties such as hardness and elastic modulus of experimental materials were determined. Electrical conductivity as a function of CNT content was measured. The effect of the CNT addition on tribological properties (coefficient of friction, wear) of SiC/CNT composites was also observed. Hardness of the reference sample was relatively high (HV1 = 24 GPa) and it decreased down to HV1 = 17–19.8 GPa with presence of CNT. Similarly, the fracture toughness decreased with presence of CNT from 4.99 MPa.m1/2 for the reference sample down to 3.4–4 MPa.m1/2 for the SiC/CNT composites. Nanoindentation showed that hardness HIT of reference sample without CNT was around 26 GPa and with increasing amounts of CNT it decreased down to 21 GPa. The composites had similar modulus of elasticity (EIT = 337–348 GPa), while for the reference sample it was EIT = 434 GPa. Electrical conductivity increased with amount of CNT (1.76 S/m for the reference sample, 484.3 S/m for the composite with 2.5 wt% Fe, and up to 2873.6 S/m for the composite with 10 wt% Fe). Specific wear rate increased with presence of CNT from 7.7 × 10−7 mm3/Nm for the reference sample to 2.4–2.9 × 10−6 mm3/Nm for the composites. Complex wear behavior common for all types of experimental materials was observed: mainly abrasion, mechanical wear (micro-fractures) and tribochemical reactions with created SiO2 layer. In the reference sample the dominant wear mechanism was abrasion, in SiC/CNT composites formation of transferred films in wear tracks consisting of oxides and carbon phases formed by crushing the CNT were observed.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (59)

Show source-provided references
1. Microstructural design of sliding-wear-resistant liquid-phase-sintered SiC: an overview10.1016/j.jeurceramsoc.2007.02.190 ↗
2. Oxidation and burner rig corrosion of liquid phase sintered SiC10.1016/S0955-2219(99)00160-0 ↗
3. Flexural strength and toughness of liquid phase sintered silicon carbide10.1016/S0272-8842(99)00084-X ↗
4. Effects of additives on densification, microstructure and properties of liquid-phase sintered silicon carbide10.1023/A:1004881430804 ↗
5. Bansal · 2005
6. Effect of the counterpart material on wear characteristics of silicon carbide ceramics10.1016/j.ijrmhm.2014.01.006 ↗
7. Unlubricated sliding behaviour of various zirconia-based ceramics10.1016/0955-2219(91)90031-T ↗
8. The friction and wear of ceramic/ceramic and ceramic/metal combinations in sliding contact
9. Micro and macro tribological properties of SiC ceramics in sliding contact10.1016/S0043-1648(01)00595-6 ↗
10. Wear mechanism of silicon carbide: new observations10.1016/0043-1648(94)90107-4 ↗
11. Ceramic–ceramic composite materials with improved friction and wear properties10.1016/0301-679X(92)90122-4 ↗
12. Tribological behaviour of ceramic materials (Si3N4, SiC and Al2O3) in aqueous medium10.1016/j.jeurceramsoc.2003.11.020 ↗
13. The effect of surrounding atmosphere on the friction and wear of alumina, zirconia, silicon carbide and silicon nitride10.1016/0043-1648(89)90068-9 ↗
14. Friction and wear of self-mated SiC and Si3N4 sliding in water10.1016/S0043-1648(01)00648-2 ↗
15. Wear and wear transition in silicon carbide ceramics during sliding10.1111/j.1151-2916.1996.tb08579.x ↗
16. Influence of humidity and doping elements on the friction and wear of SiC in unlubricated sliding10.1016/j.triboint.2003.11.002 ↗
17. Tribological behavior of ceramic materials (Si3N4, SiC and Al2O3) in aqueous medium
18. Brinson · 1987 · 1 · 226
19. EDM-future steps towards the machining of ceramics10.1016/S0007-8506(07)60759-8 ↗
20. Microstructure and the fracture toughness of the Al2O3–Fe composites10.1016/S1044-5803(01)00113-9 ↗
21. Mechanical and tribological properties of electrically conductive SiC based cermets
22. Improved sliding-wear resistance in in situ-toughened silicon carbide10.1111/j.1551-2916.2005.00628.x ↗
23. Wear-resistant ultra-fine-grained ceramics10.1016/j.actamat.2004.09.020 ↗
24. Dry sliding wear behavior of nano-sized SiC pins against SiC and Si3N4 discs10.1016/j.wear.2006.06.009 ↗
25. Friction and wear behavior of pressureless liquid phase sintered SiC ceramic10.1016/j.matdes.2014.09.031 ↗
26. The effects of the surrounding atmosphere on the friction and wear of alumina, zirconia, silicon carbide and silicon nitride10.1016/0043-1648(89)90068-9 ↗
27. Friction and wear of self-mated SiC and Si3N4 sliding in water10.1016/S0043-1648(01)00648-2 ↗
28. Wear and wear transition in silicon carbide ceramics during sliding10.1111/j.1151-2916.1996.tb08579.x ↗
29. Wear mechanism of silicon carbide: new observations10.1016/0043-1648(94)90107-4 ↗
30. Influence of humidity and doping elements on the friction and wear of SiC in unlubricated sliding10.1016/j.triboint.2003.11.002 ↗
31. Influence of small amount of sintering additives on unlubricated sliding wear properties of SiC ceramics10.1016/j.ceramint.2011.06.018 ↗
32. The relationship between wear behaviour and brittleness index in engineering ceramics and dispersion-reinforced ceramic composites
33. Helical microtubules of graphitic carbon10.1038/354056a0 ↗
34. Carbon nanotubes in analytical sciences10.1007/s00604-005-0439-z ↗
35. Mechanical properties and electrical conductivity in a carbon nanotube reinforced silicon nitride composite, ScienceDirect10.1016/j.ceramint.2011.07.038 ↗
36. Direct synthesis of long single-walled carbon nanotube10.1126/science.1066996 ↗
37. Vertically aligned carbon nanotube arrays10.1063/1.2206152 ↗
38. New one-dimensional conductors: graphitic microtubules10.1103/PhysRevLett.68.1579 ↗
39. Synthesis of carbon nanotubes by catalytic chemical vapour deposition: a review on carbon sources, catalysts and substrates10.1016/j.mssp.2015.08.013 ↗
40. Single-shell carbon nanotubes of 1-nm diameter10.1038/363603a0 ↗
41. Harris · 1999
42. Application of carbon nanotubes to silicon nitride matrix reinforcements10.1016/j.cap.2005.07.024 ↗
43. CNT-reinforced ceramics and materials10.1016/S1369-7021(04)00508-5 ↗
44. Toughening behavior in a carbon nanotube reinforced silicon nitride composite10.1016/j.msea.2008.04.058 ↗
45. Direct observation of toughening mechanisms in carbon nanotube ceramic matrix composites10.1016/j.actamat.2003.10.050 ↗
46. Dimethylformamide: an effective dispersant for making ceramic-carbon nanotube composites10.1088/0957-4484/19/19/195710 ↗
47. Tribological properties of hot-pressed alumina–CNT composites10.1016/S0043-1648(03)00216-3 ↗
48. A study of the electrical properties nanotube-NiFe2O4 composites: effect of the surface treatment of the carbon nanotubes10.1016/j.carbon.2004.08.019 ↗
49. Electrical properties of nanoceramics reinforced with ropes of single-walled carbon nanotubes10.1063/1.1600511 ↗
50. Current understanding of the growth of carbon nanotubes in catalytic chemical vapour deposition,SciVerse, ScienceDirect10.1016/j.carbon.2013.02.046 ↗
51. Dry impregnation in fluidized bed: drying and calcination effect on nanoparticles dispersion and location in a porous support10.1016/j.cherd.2007.10.004 ↗
52. A critical evaluation of indentation techniques for measuring fracture toughness. I. Direct crack measurements10.1111/j.1151-2916.1981.tb10320.x ↗
53. International Standard ISO 20808 · 2004
54. Thermal characterization and physicochemical properties of Fe2O3–Mn2O3/Al2O3 system10.1016/S0040-6031(01)00652-9 ↗
55. Vapor-liquid-solid mechanism of single crystal growth
56. Model of carbon nanotube growth through chemical vapor deposition10.1016/S0009-2614(99)01216-6 ↗
57. Instability in the tribochemical wear of silicon carbide in unlubricated sliding contacts10.1016/0043-1648(94)90080-9 ↗
58. Wear mechanisms and tribo mapping of Al2O3and SiC in dry sliding10.1016/0043-1648(94)90350-6 ↗
59. Yan · 2015 · 1