journal article·2017-02

The erosion performance of cold spray deposited metal matrix composite coatings with subsequent friction stir processing

Tom Peat, Alexander Galloway, Athanasios Toumpis, Philip McNutt, Naveed Iqbal

Publisher page

Abstract

This study forms an initial investigation into the development of SprayStir, an innovative processing technique for generating erosion resistant surface layers on a chosen substrate material. Tungsten carbide – cobalt chromium, chromium carbide – nickel chromium and aluminium oxide coatings were successfully cold spray deposited on AA5083 grade aluminium. In order to improve the deposition efficiency of the cold spray process, coatings were co-deposited with powdered AA5083 using a twin powder feed system that resulted in thick (>300 µm) composite coatings. The deposited coatings were subsequently friction stir processed to embed the particles in the substrate in order to generate a metal matrix composite (MMC) surface layer. The primary aim of this investigation was to examine the erosion performance of the SprayStirred surfaces and demonstrate the benefits of this novel process as a surface engineering technique. Volumetric analysis of the SprayStirred surfaces highlighted a drop of approx. 40% in the level of material loss when compared with the cold spray deposited coating prior to friction stir processing. Micro-hardness testing revealed that in the case of WC-CoCr reinforced coating, the hardness of the SprayStirred material exhibits an increase of approx. 540% over the unaltered substrate and 120% over the as-deposited composite coating. Microstructural examination demonstrated that the increase in the hardness of the MMC aligns with the improved dispersion of reinforcing particles throughout the aluminium matrix.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: High-Temperature Coating Behaviors · Aluminum Alloys Composites Properties · Advanced ceramic materials synthesis

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (59)

Show source-provided references
1. Papyrin · 2006
2. Champagne · 2007
3. A review on detonation gun sprayed coatings
4. Residual stress in HVOF thermally sprayed thick deposits10.1016/j.surfcoat.2003.06.003 ↗
5. Wear and corrosion behaviour of thermally sprayed cermet coatings10.1016/S0257-8972(00)01141-5 ↗
6. Slurry erosion behaviour of HVOF sprayed WC-10Co-4Cr and Al 2O 3+13TiO 2 coatings on a turbine steel10.1016/j.wear.2012.04.016 ↗
7. Bonding mechanism in cold gas spraying10.1016/S1359-6454(03)00274-X ↗
8. Residual stress induced by cold spray coating of magnesium AZ31B extrusion10.1016/j.matdes.2014.03.054 ↗
9. Effect of the thickness of cold sprayed aluminium alloy coating on the adhesive bond strength with an aluminium alloy substrate10.1016/j.surfcoat.2015.02.048 ↗
10. WC-based cermet coatings produced by cold gas dynamic and pulsed gas dynamic spraying processes10.1016/j.surfcoat.2007.05.095 ↗
11. Cold spray deposition of WC-17 and 12Co cermets onto aluminum10.1016/j.surfcoat.2013.07.011 ↗
12. SiO 2 and MoSi 2 formation on Inconel 625 surface via SiC coating deposited by cold spray10.1016/j.surfcoat.2011.12.010 ↗
13. Multiple strengthening mechanisms of cold-sprayed cBNp/NiCrAl composite coating10.1016/j.surfcoat.2011.04.065 ↗
14. Preparation of aluminum coatings containing homogenous nanocrystalline microstructures using the cold spray process10.1007/s11666-008-9180-6 ↗
15. Microstructural and macroscopic properties of cold sprayed copper coatings10.1063/1.1573740 ↗
16. Nanostructure formation by mechanical attrition10.1016/0965-9773(95)00027-5 ↗
17. Formation of metastable phases in cold-sprayed soft metallic deposit10.1016/j.surfcoat.2004.10.063 ↗
18. Grain refinement in a single titanium powder particle impacted at high velocity10.1016/j.scriptamat.2008.06.020 ↗
19. A study on processing, characterization and erosion wear behavior of silicon carbide particle filled ZA-27 metal matrix composites10.1016/j.matdes.2013.10.069 ↗
20. Contribution of Orowan strengthening effect in particulate-reinforced metal matrix nanocomposites10.1016/j.msea.2006.10.184 ↗
21. Effect of particle concentration on the structure and tribological properties of submicron particle SiC reinforced Ni metal matrix composite (MMC) coatings produced by electrodeposition10.1016/j.apsusc.2011.12.069 ↗
22. Abrasive wear behaviour of conventional and nanocomposite HVOF-sprayed WC–Co coatings10.1016/S0043-1648(99)00032-0 ↗
23. Influence of SiC particles on mechanical properties of Mg based composite10.1016/S0263-8223(00)00031-3 ↗
24. Mechanical properties and microstructure of cast oxide-dispersion-strengthened aluminum10.1016/0921-5093(94)09741-0 ↗
25. Sliding wear behaviour of conventional and nanostructured HVOF sprayed WC-Co coatings10.1016/j.wear.2005.02.059 ↗
26. Erosion-corrosion behaviour of WC-based MMCs in liquid-solid slurries10.1016/j.wear.2005.02.037 ↗
27. Erosive wear behaviour of aluminium based composites10.1016/S0261-3069(97)00081-2 ↗
28. A study of the erosion-corrosion behavior of nano-Cr2O 3 particles reinforced Ni-based composite alloying layer in aqueous slurry environment10.1016/j.vacuum.2010.10.009 ↗
29. Fabrication of aluminum-alumina metal matrix composites via cold gas dynamic spraying at low pressure followed by friction stir processing10.1016/j.msea.2012.06.066 ↗
30. Improvement of wear resistance of sprayed layer on 52100 steel by friction stir processing10.1016/j.apsusc.2014.08.033 ↗
31. Damage study of cold-sprayed composite materials for application to electrical contacts10.1007/s11666-012-9756-z ↗
32. Miranda · 2008
33. Friction stir welding and processing
34. Modification of thermally sprayed cemented carbide layer by friction stir processing10.1016/j.surfcoat.2010.01.021 ↗
35. Microstructural evaluation of cold spray deposited wc with subsequent friction stir processing10.1007/978-3-319-48173-9_23 ↗
36. Modification of a cold sprayed SiCp/Al5056 composite coating by friction stir processing10.1016/j.surfcoat.2016.04.016 ↗
37. The effect of sand concentration on the erosion of materials by a slurry jet10.1016/0043-1648(89)90116-6 ↗
38. Erosion-corrosion resistance of engineering materials in various test conditions10.1016/j.wear.2009.01.052 ↗
39. Mg based nano-composites fabricated by friction stir processing10.1016/j.scriptamat.2005.11.056 ↗
40. Development of a process envelope for friction stir welding of DH36 steel – a step change10.1016/j.matdes.2014.04.066 ↗
41. Effect of friction stir processing on fatigue behavior of A356 alloy10.1016/j.scriptamat.2004.04.014 ↗
42. Effect of multiple-pass friction stir processing on microstructure and tensile properties of a cast aluminum-silicon alloy10.1016/j.scriptamat.2006.01.010 ↗
43. Fundamental aspects of nano-reinforced composites10.1016/j.compscitech.2005.01.014 ↗
44. Effect of friction stir processing (FSP) on microstructure and properties of Al-TiC in situ composite10.1016/j.msea.2011.02.085 ↗
45. Wear behaviour of a Mg alloy subjected to friction stir processing10.1016/j.wear.2013.02.023 ↗
46. Influence of multi-pass friction stir processing on the microstructure and mechanical properties of Al-5083 alloy10.1016/j.msea.2015.10.057 ↗
47. Size dependent strengthening in particle reinforced aluminium10.1016/S1359-6454(01)00327-5 ↗
48. A quantitative method for measuring nanocomposite dispersion10.1016/j.polymer.2009.12.031 ↗
49. Quantitative dispersion analysis of inclusions in polymer composites10.1021/am301459q ↗
50. Quantification of the layer dispersion degree in polymer layered silicate nanocomposites by transmission electron microscopy10.1016/j.polymer.2008.02.028 ↗
51. Slurry wear and cavitation erosion of thermal-sprayed cermets10.1016/j.wear.2004.09.006 ↗
52. Comparison of slurry and dry erosion behaviour of some HVOF thermal sprayed coatings10.1016/S0043-1648(99)00034-4 ↗
53. a. Agrawal, Surface modification of hydroturbine steel using friction stir processing10.1016/j.apsusc.2013.01.006 ↗
54. Tribological enhancement of AISI 420 martensitic stainless steel through friction-stir processing10.1016/j.wear.2013.01.007 ↗
55. Erosion of surfaces by solid particles10.1016/0043-1648(60)90055-7 ↗
56. Erosion-corrosion of HVOF-sprayed Fe-based amorphous metallic coating under impingement by a sand-containing NaCl solution10.1016/j.corsci.2013.07.006 ↗
57. Effect of impact angle on the slurry erosion-corrosion of Stellite 6 and SS31610.1016/j.wear.2014.08.006 ↗
58. Erosion of 2014 Al reinforced with SiC or Al2O3 particles10.1016/0921-5093(92)90185-4 ↗
59. Solid particle erosion of HVOF sprayed WC-Co/NiCrFeSiB coatings10.1016/j.wear.2010.03.019 ↗