Abstract

Abstract Ti–Al coatings with ∼14.7, 18.1, 25.2 and 29.7 at.% Al contents were fabricated on pure Ti substrate by laser cladding. The laser cladding Ti–Al coatings were analyzed with X-ray diffraction (XRD), scanning electron microscope (SEM) and X-ray energy dispersive spectroscopy (EDS). It was found that with the increase of Al content, the diffraction peaks shifted gradually to higher 2 θ values. The laser cladding Ti–Al coatings with 14.7 and 18.1 at.% Al were composed of α-Ti and α 2 -Ti 3 Al phases, while those with 25.2 and 29.7 at.% Al were composed of α 2 -Ti 3 Al phase. With the increase of Al content, the cross-sectional hardness increased, while the fracture toughness decreased. For the laser cladding Ti–Al coatings, when the Al content was ≤18.1 at.%, the wear mechanism was adhesive wear and abrasive wear; while when the Al content ≥25.2 at.%, the wear mechanism was adhesive wear, abrasive wear and microfracture. With the increase of Al content, the wear rate of laser cladding Ti–Al coatings decreased under 1 N normal load, while the wear rate firstly decreased and then increased under a normal load of 3 N. Due to its optimized combination of high hardness and high fracture toughness, the laser cladding Ti–Al coating with 18.1 at.% Al showed the best anti-wear properties at higher normal load.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Intermetallics and Advanced Alloy Properties · High Entropy Alloys Studies · Titanium Alloys Microstructure and Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (29)

Show source-provided references
1. Characterization of titanium alloy Ti–6Al–4V for chemical, marine and industrial applications10.1016/j.matchar.2003.10.006 ↗
2. Research progress on laser surface modification of titanium alloys10.1016/j.apsusc.2004.08.011 ↗
3. Friction and wear behavior of Ti following laser surface alloying with Si, Al and Si+Al10.1016/S0043-1648(00)00363-X ↗
4. Wear resistance of a laser surface alloyed Ti–6Al–4V alloy10.1016/S0257-8972(00)00680-0 ↗
5. Laser nitriding of pure titanium with Ni, Cr for improved wear performance10.1016/S0043-1648(97)00204-4 ↗
6. Effects of nitrogen gas flow rates on the microstructure and properties of laser-nitrided IMI318 titanium alloy (Ti–4V–6Al)10.1016/S0924-0136(97)00408-1 ↗
7. Surface treatment of titanium by laser irradiation to improve resistance to dry-sliding friction10.1016/S0043-1648(99)00254-9 ↗
8. Study on the microstructure and wear resistance of the composite coatings fabricated on Ti–6Al–4V under different processing conditions10.1016/j.apsusc.2006.02.026 ↗
9. Microstructures and wear properties of composite coatings produced by laser alloying of Ti–6Al–4V with graphite and silicon mixed powders10.1016/j.matlet.2005.07.082 ↗
10. Surface modification of pure Ti by laser alloying with B and Ni mixed powders10.1002/adem.200400221 ↗
11. Ti–6Al–4V strengthened by laser melt injection of WCp particles10.1016/S1359-6454(02)00366-X ↗
12. SiCp/Ti6Al4V functionally graded materials produced by laser melt injection10.1016/S1359-6454(02)00049-6 ↗
13. Sliding wear resistance of metal matrix composite layers prepared by high power laser10.1016/j.surfcoat.2004.09.003 ↗
14. Microstructure and wear resistance of laser clad Ti5Si3/NiTi2 intermetallic composite coating on titanium alloy10.1016/S0921-5093(02)00076-X ↗
15. Wear resistance of laser clad Ti2Ni3Si reinforced intermetallic composite coatings on titanium alloy10.1016/j.apsusc.2004.01.045 ↗
16. Martensite formation in Ti–Al layers produced by laser surface alloying10.1179/mst.1991.7.9.827 ↗
17. Laser surface alloying of titanium with aluminium10.1007/BF00725833 ↗
18. Processing aspects of laser surface alloying of titanium with aluminium10.1179/mst.1991.7.4.353 ↗
19. Hardness and toughness of MoSi2 and MoSi2–SiC composite prepared by reactive sintering of powders10.1016/S0921-5093(98)00517-6 ↗
20. Decomposition of the α-phase in titanium-rich Ti–Al alloys10.1007/BF02644528 ↗
21. Direct laser sintering of iron–graphite powder mixture10.1016/j.msea.2004.05.070 ↗
22. Structural formation of aluminide phases on titanium substrate10.1016/j.surfcoat.2003.10.070 ↗
23. J.L. Murray, Phase Diagrams of Binary Titanium Alloys, ASM International, Metals Park, OH, 1987.
24. R.I. Jaffee, Titanium–aluminum alloys, US Pat: 2,880,087 (1959).
25. The embrittlement and fracture of Ti–8pctAl alloy
26. M.J. Blackburn, M.P. Smith, Titanium alloys of the Ti3Al type, US Pat: 4,292,077 (1981).
27. D.R. Askeland, P.P. Phulé, Mechanical properties and behavior, The Science and Engineering of Materials, fourth edition, Brooks/Cole, 2002.
28. Effect of alloying elements and heat treatment on the fracture toughness of Ti–Al–Nb alloys10.1016/S1359-6454(97)00207-3 ↗
29. P.J. Blau, Glossary of terms, Friction, Lubrication, and Wear Technology, vol. 18, ASM Handbook, ASM International, 1992.