Magnesium (Mg) coated with four kinds of polymers, poly (l-lactic acid) (PLLA)-high molecular weight (HMW), PLLA-low molecular weight (LMW), poly (ɛ-caprolactone) (PCL)-HMW and PCL-LMW, and uncoated Mg were immersed under cell culture condition to study the degradation/corrosion behavior of the polymer-coated Mg. The releases of Mg2+ are measured during the immersion. Surface morphology and chemical composition are observed and identified by SEM and EDX. The tomography is obtained by X-ray CT observation and degradation rate is calculated by image analysis after 10-day immersion. All kinds of polymer-coated Mg showed significantly low release of Mg2+ (p < 0.05) in the whole immersion process comparing to that of uncoated Mg. In SEM and EDX results show, a corrosion layer can be observed on both polymer-coated and uncoated Mg after immersion. There is no obvious difference on the morphology and chemical composition of the corrosion layer between polymer-coated and uncoated Mg, indicating the corrosion/degradation process and corrosion product of Mg substrate are not changed by the polymer films under the present condition compared with uncoated Mg. Concerning the tomography and degradation rate of 10-day immersion, it can be found that the polymer-coated Mg shows a significantly low corrosion rate (p < 0.05) compared with that of uncoated Mg. PLLA coated Mg shows relatively uniform corrosion than PCL coated Mg and uncoated Mg. The largest pitting corrosion depth of PCL-LMW is about 3 times as large as the PLLA-LMW, which might be attributed to the difference of polymer microstructure. It is suggested that PLLA coating might be a suitable option for retarding the loss of mechanical properties of Mg substrate. Highlights ► Degradation behavior of 4 kinds of polymer-coated Mg under cell culture condition. ► All kinds of polymer coating effectively decreased Mg2+ release. ► SEM and EDX analysis revealed corrosion layer underneath the polymer coating. ► X-ray CT showed corrosion depth of PLLA-coated Mg 3 times smaller than PCL-coated.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Magnesium Alloys: Properties and Applications · Corrosion Behavior and Inhibition · Orthopaedic implants and arthroplasty
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (30)
Show source-provided references
1. G.B. Stroganov, E.M., Savitsky, N.M., Tikhova, V.F., Terekhova, M.V., Volkov, K.M. Sivash et al., US Patent (1972) 3,687,135.
2. Xu · J. Biomed. Mater. Res. A · 2007 · 83 · 70310.1002/jbm.a.31273 ↗
3. In vitro corrosion behaviour of Mg alloys in a phosphate buffered solution for bone implant application10.1007/s10856-007-3219-y ↗
4. Li · Biomaterials · 2008 · 29 · 132910.1016/j.biomaterials.2007.12.021 ↗
5. Di Mario · J. Intervent. Cardiol. · 2004 · 17 · 39110.1111/j.1540-8183.2004.04081.x ↗
6. Waksman · Catheter. Cardiovasc. Interv. · 2006 · 68 · 60710.1002/ccd.20727 ↗
7. Witte · Biomaterials · 2006 · 27 · 101310.1016/j.biomaterials.2005.07.037 ↗
8. Witte · Biomaterials · 2005 · 26 · 355710.1016/j.biomaterials.2004.09.049 ↗
9. Peng · Biomaterials · 2010 · 31 · 39810.1016/j.biomaterials.2009.09.065 ↗
10. Heublein · Heart · 2003 · 89 · 65110.1136/heart.89.6.651 ↗
11. Zhang · Acta Biomater. · 2010 · 6 · 175610.1016/j.actbio.2009.11.024 ↗
12. Zhang · Acta Biomater. · 2010 · 6 · 62610.1016/j.actbio.2009.06.028 ↗
13. Huan · Mater. Sci.-Mater. Med. · 2010 · 9 · 262310.1007/s10856-010-4111-8 ↗
14. Chen · Transac. Nonferr. Metal Soc. · 2008 · 18 · s36110.1016/S1003-6326(10)60232-4 ↗
15. Gu · Acta Biomater. · 2011 · 7 · 188010.1016/j.actbio.2010.11.034 ↗
16. Hiromoto · Corros. Sci. · 2008 · 50 · 290610.1016/j.corsci.2008.08.013 ↗
17. Song · Acta Biomater. · 2010 · 6 · 173610.1016/j.actbio.2009.12.020 ↗
18. Xu · Biomaterials · 2009 · 30 · 151210.1016/j.biomaterials.2008.12.001 ↗
19. Xu · J. Mater. Sci.-Mater. Med. · 2009 · 20 · 85910.1007/s10856-008-3648-2 ↗
20. Chen · Biomed. Mater. · 2011 · 6 · 02500510.1088/1748-6041/6/2/025005 ↗
21. Gu · Biomed. Mater. · 2009 · 4 · 04410910.1088/1748-6041/4/4/044109 ↗
22. Influence of surface modification on the in vitro corrosion rate of magnesium alloy AZ3110.1002/jbm.a.32205 ↗
23. Wong · Biomaterials · 2010 · 31 · 208410.1016/j.biomaterials.2009.11.111 ↗
24. Li · J. Mater. Sci. · 2010 · 45 · 603810.1007/s10853-010-4688-9 ↗
25. Effect of inorganic salts, amino acids and proteins on the degradation of pure magnesium in vitro10.1016/j.msec.2008.12.015 ↗
26. Xu · Colloids Surf. B · 2012 · 93 · 6710.1016/j.colsurfb.2011.12.009 ↗
27. Tuba · FME Transac. · 2009 · 37 · 33
28. Renouf-Glauser · Biomacromolecules · 2006 · 7 · 61210.1021/bm050746v ↗
29. Proikakis · Polym. Degrad. Stab. · 2006 · 91 · 61410.1016/j.polymdegradstab.2005.01.060 ↗
30. Xin · Acta Biomater. · 2011 · 7 · 145210.1016/j.actbio.2010.12.004 ↗