journal article·2014-01Open access

The effect of increasing V content on the structure, mechanical properties and oxidation resistance of Ti–Si–V–N films deposited by DC reactive magnetron sputtering

F. Fernandes, A. Loureiro, T. Polcar, A. Cavaleiro

Abstract

In the last years, vanadium rich films have been introduced as possible candidates for self-lubrication at high temperatures, based on the formation of V2O5 oxide. The aim of this investigation was to study the effect of V additions on the structure, mechanical properties and oxidation resistance of Ti–Si–V–N coatings deposited by DC reactive magnetron sputtering. The results achieved for TiSiVN films were compared and discussed in relation to TiN and TiSiN films prepared as reference. All coatings presented a fcc NaCl-type structure. A shift of the diffraction peaks to higher angles with increasing Si and V contents suggested the formation of a substitutional solid solution in TiN phase. Hardness and Young's modulus of the coatings were similar regardless on V content. The onset of oxidation of the films decreased significantly to 500 °C when V was added into the films; this behaviour was independent of the Si and V contents. The thermogravimetric isothermal curves of TiSiVN coatings oxidized at temperatures below the melting point of ?-V2O5 (?685 °C) showed two stages: at an early stage, the weight increase over time is linear, whilst, in the second stage, a parabolic evolution can be fitted to the experimental data. At higher temperatures only a parabolic evolution was fitted. ?-V2O5 was the main phase detected at the oxidized surface of the coatings. Reduction of ?-V2O5 to ?-V2O5 phase occurred for temperatures above its melting point
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Metal and Thin Film Mechanics · Advanced materials and composites · High-Temperature Coating Behaviors

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (45)

Show source-provided references
1. Oxidation behaviour of nanoscale TiAlN/VN multilayer coatings10.1016/j.surfcoat.2003.09.031 ↗
2. The effect of increasing V content on structure, mechanical and tribological properties of arc evaporated Ti–Al–V–N coatings10.1016/j.ijrmhm.2008.06.008 ↗
3. Influence of high-temperature oxide formation on the tribological behaviour of TiN and VN coatings10.1016/j.wear.2006.11.006 ↗
4. Tribological behavior of PACVD TiN coatings in the temperature range up to 500°C10.1016/S0257-8972(02)00626-6 ↗
5. Low-friction TiN coatings deposited by PACVD10.1016/S0257-8972(02)00642-4 ↗
6. Tribological properties, phase generation and high temperature phase stability of tungsten- and vanadium-oxides deposited by reactive MSIP–PVD process for innovative lubrication applications10.1016/S0257-8972(00)00963-4 ↗
7. The effect of (Ti+Al):V ratio on the structure and oxidation behaviour of TiAlN/VN nano-scale multilayer coatings10.1016/j.surfcoat.2003.09.041 ↗
8. Influence of oxide phase formation on the tribological behaviour of Ti–Al–V–N coatings10.1016/j.surfcoat.2005.08.044 ↗
9. A new low-friction concept for Ti1−xAlxN based coatings in high-temperature applications10.1016/j.surfcoat.2004.08.022 ↗
10. A new low friction concept for high temperatures: lubricious oxide formation on sputtered VN coatings10.1007/s11249-004-8083-z ↗
11. Calorimetric evidence for frictional self-adaptation of TiAlN/VN superlattice coatings10.1016/j.surfcoat.2003.09.024 ↗
12. Oxidation of vanadium nitride and titanium nitride coatings10.1016/j.susc.2006.12.010 ↗
13. Friction and wear properties of CrAlN and CrVN films deposited by cathodic arc ion plating method10.1016/S0257-8972(03)00937-X ↗
14. Tribo-oxidation of cathodic arc ion-plated (V,Ti)N coatings sliding against a steel ball under both unlubricated and boundary-lubricated conditions10.1016/j.surfcoat.2004.02.027 ↗
15. Increase of hardness and oxidation resistance of VN coating by nanoscale multilayered structurization with AlN10.1016/j.matlet.2007.12.040 ↗
16. Influence of phase transition on the tribological performance of arc-evaporated AlCrVN hard coatings10.1016/j.surfcoat.2008.10.003 ↗
17. Self-lubricating CrAlN/VN multilayer coatings at room temperature10.1016/j.apsusc.2013.04.068 ↗
18. A study of mechanical and tribological properties of self-lubricating TiAlVN coatings at elevated temperatures10.1016/j.triboint.2013.06.007 ↗
19. Temperature dependent friction and wear of magnetron sputtered coating TiAlN/VN10.1016/j.wear.2011.01.054 ↗
20. Influence of deposition conditions on the microstructure and mechanical properties of Ti–Si–N films by DC reactive magnetron sputtering10.1016/S0040-6090(02)00833-7 ↗
21. Influence of sputtering conditions on the structure and properties of Ti–Si–N thin films prepared by r.f.-reactive sputtering10.1016/S0257-8972(03)00710-2 ↗
22. The issue of the reproducibility of deposition of superhard nanocomposites with hardness of ≥50GPa10.1016/j.surfcoat.2004.11.023 ↗
23. Study of the structural changes induced by air oxidation in Ti–Si–N hard coatings10.1016/j.surfcoat.2007.09.017 ↗
24. Mechanical properties and oxidation resistance of nanocomposite TiN–SiNx physical-vapor-deposited thin films10.1016/S0257-8972(99)00481-8 ↗
25. Characterisation of Ti1−xSixNy nanocomposite films10.1016/S0257-8972(00)00947-6 ↗
26. Improving the properties of titanium nitride by incorporation of silicon10.1016/S0257-8972(98)00560-X ↗
27. Mechanical and tribological properties of nanocomposite TiSiN coatings10.1016/j.surfcoat.2009.11.034 ↗
28. Structure–performance relations in nanocomposite coatings10.1016/S0257-8972(01)01389-5 ↗
29. The tribological and structural characterization of nano-structured Ti–Si–N films coated by pulsed-d.c. plasma enhanced CVD10.1016/j.vacuum.2005.01.003 ↗
30. The tension of metallic films deposited by electrolysis10.1098/rspa.1909.0021 ↗
31. Raman microscopic studies of residual and applied stress in PVD hard ceramic coatings and correlation with X-ray diffraction (XRD) measurements10.1016/j.surfcoat.2003.10.014 ↗
32. Structural analysis of Ti1−xSixNy nanocomposite films prepared by reactive magnetron sputtering10.1016/S0257-8972(99)00450-8 ↗
33. Mechanical properties and oxidation resistance of nanocomposite TiN–SiNx physical-vapor-deposited thin films10.1016/S0257-8972(99)00481-8 ↗
34. Wet oxidation of Ti34Si23B4310.1063/1.369342 ↗
35. Moving species in Ti34Si23N43 oxidation10.1016/S0040-6090(99)00178-9 ↗
36. Oxidation Behavior and mechanisms of TiAlN/VN coatings10.1007/s11661-007-9293-4 ↗
37. Oxidation and diffusion processes during annealing of AlCrVN hard coatings10.1116/1.2841508 ↗
38. Oxidation kinetics of TiN thin films10.1063/1.328659 ↗
39. Microstructures and optical properties of β-V 2 O 5 nanorods prepared by magnetron sputtering10.1088/0022-3727/42/14/145402 ↗
40. X-ray and Raman study of spray pyrolysed vanadium oxide thin films10.1016/j.vibspec.2011.07.003 ↗
41. Anatase-TiO2 nanomaterials: morphological/size dependence of the crystallization and phase behavior phenomena10.1021/jp065661i ↗
42. Raman, Infrared, X-ray, and EELS Studies of Nanophase Titania
43. Structure of a high-pressure phase of vanadium pentoxide beta-V2O510.1107/S0108768104012881 ↗
44. V2O5 phase diagram revisited at high pressures and high temperatures10.1016/j.jallcom.2006.04.042 ↗
45. The high-temperature oxidation behavior of vanadium–aluminum alloys10.1007/BF01151591 ↗