Tribological performance of sub-100-nm femtosecond laser-induced periodic surface structures on titanium
Source abstract
Abstract
Abstract Sub-100-nm laser-induced periodic surface structures (LIPSS) were processed on bulk titanium (Ti) surfaces by femtosecond laser pulse irradiation in air (30 fs pulse duration, 790 nm wavelength). The laser peak fluence, the spatial spot overlap, and the number of overscans were optimized in a sample-scanning geometry in order to obtain large surface areas (5 mm × 5 mm) covered homogeneously by the LIPSS. The laser-processed regions were characterized by optical microscopy (OM), white light interference microscopy (WLIM) and scanning electron microscopy (SEM). The friction coefficient of the nanostructured surfaces was tested during 1000 cycles under reciprocal sliding conditions (1 Hz, 1.0 N normal load) against a 10-mm diameter ball of hardened 100Cr6 steel, both in paraffin oil and in engine oil used as lubricants. Subsequently, the corresponding wear tracks were qualified by OM, SEM, and energy dispersive X-ray analyses (EDX). The results of the tribological tests are discussed and compared to that obtained for near wavelength-sized fs-LIPSS, processed under somewhat different irradiation conditions. Some constraints for a beneficial effect of LIPSS on the tribological performance are provided.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Laser Material Processing Techniques · Adhesion, Friction, and Surface Interactions · Laser-induced spectroscopy and plasma
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (26)
Show source-provided references
1. Colorizing metals with femtosecond laser pulses10.1063/1.2834902 ↗
2. Controlled nanostructures formation by ultrafast laser pulses for color marking applications10.1364/OE.18.002913 ↗
3. Tailoring the wetting response of silicon surfaces via fs structuring10.1007/s00339-008-4757-y ↗
4. Femtosecond laser modification of material wetting properties: a brief review10.1166/sam.2012.1298 ↗
5. Friction properties of the DLC film with periodic structures in nano-scale10.2474/trol.1.44 ↗
6. Control of tribological properties of diamond-like carbon films with femtosecond-laser-induced nanostructuring10.1016/j.apsusc.2007.09.037 ↗
7. Ripple formation in various metals and super-hard tetrahedral amorphous carbon films in consequence of femtosecond laser irradiation10.1007/s00339-012-7146-5 ↗
8. Towards friction control using laser-induced periodic surface structures10.1016/j.phpro.2011.03.099 ↗
9. Microstructure and lubricating property of ultra-fast laser pulse textured silicon carbide seals10.1007/s00339-012-6822-9 ↗
10. Femtosecond laser-induced periodic surface structures on steel and titanium alloy for tribological applications10.1007/s00339-014-8229-2 ↗
11. Tribological performance of femtosecond laser-induced periodic surface structures
12. Tribological performance of femtosecond laser-induced periodic surface structures on titanium and a high toughness bearing steel10.1016/j.apsusc.2014.08.111 ↗
13. Friction reduction through sub-micron laser surface modifications
14. Subwavelength ripple formation on the surfaces of compound semiconductors irradiated with femtosecond laser pulses10.1063/1.1586457 ↗
15. Structure formation on the surface of indium phosphide irradiated by femtosecond laser pulses10.1063/1.1827919 ↗
16. Surface electromagnetic-waves in optics10.1117/12.56133 ↗
17. Laser-induced periodic surface structure. I. Theory10.1103/PhysRevB.27.1141 ↗
18. On the role of surface plasmon polaritons in the formation of laser-induced periodic surface structures upon irradiation of silicon by femtosecond-laser pulses10.1063/1.3261734 ↗
19. Ultrashort excitations of surface polaritons and waveguide modes in semiconductors10.1134/S0030400X08070114 ↗
20. Surface plasmon polariton model of high-spatial frequency laser-induced periodic surface structure generation in silicon10.1063/1.4730381 ↗
21. Plasmonic formation mechanism of periodic 100-nm-structures upon femtosecond laser irradiation of silicon in water10.1063/1.4887808 ↗
22. Surface patterning on insulators upon femtosecond laser ablation10.1016/S0169-4332(02)01443-5 ↗
23. Sub-100-nm laser-induced periodic surface structures upon irradiation of titanium by Ti:sapphire femtosecond laser pulses in air10.1007/s00339-012-7140-y ↗
24. Femtosecond laser damage of a high reflecting mirror10.1016/S0040-6090(02)00074-3 ↗
25. Femtosecond laser-induced removal of silicon nitride layers from doped and textured silicon wafers used in photovoltaics10.1016/j.tsf.2013.07.005 ↗
26. Czichos · 2010