Direct bonding of silicon and quartz glass using VUV/O3 activation and a multistep low-temperature annealing process
Source abstract
Abstract
Abstract Low-temperature direct bonding is a promising method to integrate two or more dissimilar materials into one composite without large thermal stresses. In this paper, we describe a bonding process for silicon and quartz glass via vacuum ultraviolet/ozone (VUV/O3) activation and a multistep, low-temperature annealing process. A strong bonding strength and a bonding interface without any microcracks were obtained after annealing at 200 °C. The surfaces and bonding interface were characterized. After the organic contaminants were removed by VUV/O3, the treated surfaces were very hydrophilic. In addition, the VUV/O3-induced surface oxidation increased, resulting in oxide asperities on the substrates. These newly generated surface asperities might possess a strong deformability based on the water stress corrosion effect, leading to gap closure after low-temperature annealing. Moreover, a model for the mechanism of the VUV/O3-activated bonding was proposed.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: 3D IC and TSV technologies · Electronic Packaging and Soldering Technologies · Synthesis and properties of polymers
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (26)
Show source-provided references
1. Extended-nanofluidics: fundamental technologies, unique liquid properties, and application in chemical and bio analysis methods and devices10.1021/ac4026303 ↗
2. Mechanisms for low-temperature direct bonding of Si/Si and quartz/quartz via VUV/O3 activation10.1039/C7RA13095C ↗
3. A high performance micro-pressure sensor based on a double-ended quartz tuning fork and silicon diaphragm in atmospheric packaging10.1088/0957-0233/26/6/065101 ↗
4. Room-temperature direct bonding of silicon and quartz glass wafers10.1063/1.4985130 ↗
5. Efficient photoresist residue removal with 172 nm excimer radiation10.4028/www.scientific.net/SSP.255.122 ↗
6. Effect of VUV lamp on wafer charging by single-wafer wet clean10.1149/08002.0081ecst ↗
7. Direct homo/heterogeneous bonding of silicon and glass using vacuum ultraviolet irradiation in air10.1149/2.0161804jes ↗
8. Vacuum ultraviolet irradiation treatment for reducing gold-gold bonding temperature10.2320/matertrans.MF201313 ↗
9. Bo Ma, H. Kuwae, A. Okada, Weixin Fu, S. Shoji, J. Mizuno, VUV/O3 assisted single crystal quartz bonding with amorphous SiO2 intermediate layer for manufacturing optical low pass filter, in: 2016 Int. Conf. Electron. Packag., IEEE, 2016, pp. 447–450.10.1109/ICEP.2016.7486866 ↗
10. Low-temperature direct heterogeneous bonding of polyether ether ketone and platinum10.1016/j.msec.2017.05.058 ↗
11. B.V. Crist, Handbook of Monochromatic XPS Spectra, The Elements of Native Oxides, 2000.
12. Investigation of nitric oxide and Ar annealed SiO2/SiC interfaces by x-ray photoelectron spectroscopy10.1063/1.371363 ↗
13. XPS study of SiO thin films and SiO-metal interfaces10.1088/0953-8984/1/31/019 ↗
14. XPS study on the early stages of oxidation of Si(100) by atomic oxygen10.1016/0039-6028(89)90377-4 ↗
15. Theoretical study of the adsorption of oxygen on Si(100)10.1116/1.572658 ↗
16. Durable flame retardant finish for silk fabric using boron hybrid silica sol10.1016/j.apsusc.2016.06.119 ↗
17. Preparation of durable hydrophobic cellulose fabric from water glass and mixed organosilanes10.1016/j.apsusc.2010.08.081 ↗
18. Hydrophobicity recovery of polydimethylsiloxane after exposure to corona discharges10.1016/S0032-3861(97)00484-9 ↗
19. Reactive magnetron sputtering of Si–C–N films with controlled mechanical and optical properties10.1016/S0925-9635(03)00078-5 ↗
20. Mechanisms for room temperature direct wafer bonding10.1063/1.4794319 ↗
21. Room-temperature direct bonding using fluorine containing plasma activation10.1149/1.3560510 ↗
22. Silicon direct bonding via low-temperature wet chemical surface activation10.1039/C6RA05189H ↗
23. Water stress corrosion in bonded structures10.1149/06405.0121ecst ↗
24. A review of hydrophilic silicon wafer bonding10.1149/2.007403jss ↗
25. Measurement of bonding energy in an anhydrous nitrogen atmosphere and its application to silicon direct bonding technology10.1063/1.4716030 ↗
26. A comparative study: void formation in silicon wafer direct bonding by oxygen plasma activation with and without fluorine10.1149/2.0311612jss ↗