Friction stir processing of dual certified 304/304L austenitic stainless steel for improved cavitation erosion resistance

Xiujuan Jiang, Nicole Overman, Nathan Canfield, Kenneth Ross

Publisher page

Abstract

Abstract Cavitation erosion is known to be prevalent in equipment in hydraulic environments. Understanding cavitation erosion and improving the erosion resistance of commonly used materials is of interest for both scientific and economic reasons. In this study, friction stir processing was employed to modify commercial dual certified AISI 304/304L austenitic stainless steel plates. The cavitation erosion behavior of the processed plates was evaluated and compared to that of the unprocessed steel. A temperature control algorithm was employed to maintain a target tool temperature during the processing. The cross sections of the processed nuggets were evaluated using optical microscopy, scanning electron microscopy and Vickers hardness testing. Erosion testing by cavitation liquid jet was performed conforming to ASTM G134 on specimens cut out of the nuggets of the commercially unprocessed and the processed 304/304L steel. The tool temperature was found to affect the microstructure and the cavitation erosion behavior. Friction stir processed steel showed greater than 3× improvement in cavitation erosion resistance (defined as the reciprocal of the mass loss of a given material) than the unprocessed 304/304L. Surface erosion patterns and erosion rates were characterized and the mechanisms of material removal were discussed.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced Welding Techniques Analysis · Cavitation Phenomena in Pumps · Aluminum Alloys Composites Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (35)

Show source-provided references
1. A review of cavitation in hydraulic machinery10.1016/S1001-6058(16)60638-8 ↗
2. The development of advanced hydroelectric turbines to improve fish passage survival10.1577/1548-8446(2001)026<0014:TDOAHT>2.0.CO;2 ↗
3. Cavitation erosion in hydraulic turbine components and mitigation by coatings: current status and future needs10.1007/s11665-011-0051-9 ↗
4. A method for propeller blade optimization and cavitation inception mitigation10.5957/jspd.2015.31.2.88 ↗
5. Explosive welding of a near-equiatomic nickel-titanium alloy to low-carbon steel10.1016/0921-5093(94)90379-4 ↗
6. Cavitation erosion of NiTi explosively welded to steel10.1016/0043-1648(94)07029-6 ↗
7. NiTi cladding on stainless steel by TIG surfacing process: Part I10.1016/S0257-8972(03)00345-1 ↗
8. Effect of phase transformation on cavitation erosion resistance of some ferrous alloys10.1016/S0921-5093(03)00306-X ↗
9. Cavitation wear behaviour of austenitic stainless steels with different grain sizes10.1016/j.wear.2004.03.024 ↗
10. Surface modification of hydroturbine steel using friction stir processing10.1016/j.apsusc.2013.01.006 ↗
11. Improvement of cavitation erosion resistance of a duplex stainless steel through friction stir processing (FSP)10.1016/j.wear.2012.10.005 ↗
12. Improvement in cavitation erosion resistance of AISI 316L stainless steel by friction stir processing10.1016/j.apsusc.2014.04.132 ↗
13. ASTM G32-16, Standard Test Method for Cavitation Erosion Using Vibratory Apparatus, ASTM International, West Conshohocken, PA, 2016, www.astm.org.
14. Laboratory testing methods of cavitation erosion
15. Designation: G134-95: Standard Test Method for Erosion of Solid Materials by a Cavitating Liquid Jet, Annual Book of ASTM Standards, Section 3: Metals Test Methods and Analytical Procedures, Vol. 03.02, West Conshohocken, PA, 2010, pp. 558–571.
16. Mishra · 2014
17. Ross · 2013 · 301
18. Ross · 2013 · 321
19. The temperature-dependance of the lattice parameters of iron, cobalt, and nickel in the high temperature range
20. Effects of heat input in friction stir welding on microstructure and mechanical properties of AA3003-H18 plates10.1016/S1003-6326(15)63826-2 ↗
21. Influence of heat input on friction stir welding for the ODS Steel MA956
22. Thiruvengadam · 1964
23. Correlation of cavitation erosion behavior with mechanical properties of metals10.1016/0043-1648(90)90122-Q ↗
24. Correlation between cavitation erosion resistance and cyclic mechanical properties of different metallic materials
25. Towards numerical prediction of cavitation erosion10.1098/rsfs.2015.0013 ↗
26. Cavitation-induced damage of soft materials by focused ultrasound bursts: a fracture-based bubble dynamics model10.1121/1.4961364 ↗
27. Metals Handbook, Vol. 11, Failure Analysis and Prevention, American Society for Metals, 1986, pp. 160–164.
28. N.A. Klymyshyn, K.A. Ross, J.E. Deibler, N.P. Barrett, Evaluating Canister Repair Technologies to Address Stress Corrosion Cracking, EPRI (electrical power research institute) ESCP (extended storage collaboration program) Fall Meeting, 2017.
29. Friction stir processing of stainless steel for ascertaining its superlative performance in bioimplant applications10.1021/acsami.7b11064 ↗
30. S.A. Rose, The effect of cooling rate of friction stir welded high strength low alloy steel, 2013.
31. Friction stir processing technology: a review10.1007/s11661-007-9459-0 ↗
32. Cavitation erosion of metallic materials
33. Unraveling the anomalous grain size dependence of cavitation10.1103/PhysRevLett.117.215503 ↗
34. Effect of grain size on cavitation in superplastic Zn-Al eutectoid10.1007/BF00543735 ↗
35. Cavitation erosion of stainless steels10.1016/0043-1648(82)90278-2 ↗