journal article·2011-06

Tunable surface wettability of ZnO nanorods prepared by two-step method

Jianguo Lv, Jianbo Zhu, Kai Huang, Fanming Meng, Xueping Song, Zhaoqi Sun

Applied Surface Science· Volume 257· Issue 17
Publisher page

Abstract

Abstract Zinc oxide (ZnO) nanorods were deposited on silicon substrate by two-step method. The crystal structure, surface morphology and water contact angle (WCA) were measured by X-ray diffractometer (XRD), field emission scanning electron microscopy (FESEM), and water contact angle apparatus. It is demonstrated that the WCA of the as-grown ZnO nanorods varies between 136° and 43° and the contact angle reduction rate of ZnO nanorods changes rapidly with increasing growth time. The variation of contact angle in the as-grown samples and contact angle reduction rate has been attributed to the combined effects of the proportion of nonpolar planes in the outermost surface, the area fraction of vapor on the surface and the increase of surface energy of ZnO nanorods.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: ZnO doping and properties · Surface Modification and Superhydrophobicity · Advanced Sensor and Energy Harvesting Materials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (28)

Show source-provided references
1. Gau · Science · 1999 · 283 · 4610.1126/science.283.5398.46 ↗
2. Velev · Nature · 2003 · 426 · 51510.1038/426515a ↗
3. Feng · Adv. Mater. · 2006 · 18 · 306310.1002/adma.200501961 ↗
4. Feng · Am. Chem. Soc. · 2004 · 126 · 6210.1021/ja038636o ↗
5. Gong · Nanotechnology · 2009 · 20 · 16560210.1088/0957-4484/20/16/165602 ↗
6. Papadopoulou · J. Phys. Chem. C · 2009 · 113 · 289110.1021/jp8085057 ↗
7. Ran · Langmuir · 2008 · 24 · 995210.1021/la801461j ↗
8. Feng · Angew. Chem. Int. Ed. · 2005 · 44 · 511510.1002/anie.200501337 ↗
9. Jhang · J. Phys. Chem. C · 2007 · 111 · 1452110.1021/jp0744432 ↗
10. Sun · J. Phys. Chem. B · 2001 · 105 · 198410.1021/jp002525j ↗
11. Liu · Langmuir · 2004 · 20 · 565910.1021/la036280o ↗
12. Papadopoulou · Thin Solid Films · 2009 · 518 · 126710.1016/j.tsf.2009.02.077 ↗
13. Kenanakis · Appl. Surf. Sci. · 2008 · 254 · 569510.1016/j.apsusc.2008.03.055 ↗
14. Miyauchi · J. Phys. Chem. B · 2005 · 109 · 1330710.1021/jp051499s ↗
15. Lü · Appl. Surf. Sci. · 2010 · 256 · 472010.1016/j.apsusc.2010.02.080 ↗
16. Li · Appl. Surf. Sci. · 2010 · 256 · 169810.1016/j.apsusc.2009.09.097 ↗
17. Chen · Acta Mater. · 2011 · 59 · 84110.1016/j.actamat.2010.09.070 ↗
18. Li · Mater. Lett. · 2008 · 62 · 150310.1016/j.matlet.2007.09.011 ↗
19. Zhang · Langmuir · 2006 · 22 · 294610.1021/la053428q ↗
20. Li · Appl. Phys. Lett. · 2008 · 92 · 17310410.1063/1.2918447 ↗
21. Zhang · Colloid Interface Sci. · 2010 · 351 · 28810.1016/j.jcis.2010.07.048 ↗
22. Wang · J. Phys. Chem. B · 1999 · 103 · 218810.1021/jp983386x ↗
23. Wenzel · Ind. Eng. Chem. · 1936 · 28 · 98810.1021/ie50320a024 ↗
24. Cassie · Trans. Faraday Soc. · 1944 · 40 · 54610.1039/tf9444000546 ↗
25. Das · Appl. Surf. Sci. · 2009 · 255 · 731910.1016/j.apsusc.2009.03.090 ↗
26. Kwak · J. Phys. Chem. C · 2009 · 113 · 1208510.1021/jp900072s ↗
27. Shibata · J. Phys. Chem. B · 2003 · 107 · 1069610.1021/jp0357830 ↗
28. Li · Sens. Actuators A · 2010 · 158 · 17610.1016/j.sna.2009.12.030 ↗