journal article·2019-12

Interfacial oxidation protection and thermal-stable sinter Ag joining on bare Cu substrate by single-layer graphene coating

Chuantong Chen, Zheng Zhang, Dongjin Kim, Bowen Zhang, Masami Tanioku, Takao Ono, Kazuhiko Matsumoto, Katsuaki Suganuma

Publisher page

Abstract

Abstract In the next generation power electronics packaging, sinter Ag joining technology has become popular for use as a die attach and is receiving greater attention. Herein, it is reported that sinter Ag particles joining performed directly on a bare Cu substrate coated by a single-layer graphene can provide satisfactory interfacial oxidation protection and mechanical reliability. The shear strength obtained in our research achieved 25.4 MPa in low temperature, pressure-free sintering in air. The Cu oxide layer appeared solely at the location of Cu grain boundaries during sintering and was much smaller than when performed on substrates without graphene coating. The bonding mechanism was realized by Ag nanoparticles (AgNPs) self-generated from the Ag paste during the sintering process which tightly bonded to the graphene surface upon interacting with the Cu oxide. A subsequent high temperature (250 °C) aging test demonstrated that die shear strength maintains its value as-sintered for 750 h. Furthermore, the thickness of Cu oxide with graphene coating was about one fourth of that without graphene and this difference increased with aging time. This study puts forward an exciting solution for sinter Ag joining directly on Cu-based substrates in high temperature for longer lifetime in power electronic packaging applications.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Electronic Packaging and Soldering Technologies · Aluminum Alloys Composites Properties · 3D IC and TSV technologies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (54)

Show source-provided references
1. Silicon carbide as a platform for power electronics10.1126/science.1168704 ↗
2. Review of silicon carbide power devices and their application10.1109/TIE.2017.2652401 ↗
3. GaN technology for power electronic applications: a review10.1007/s11664-016-4435-3 ↗
4. P. G. Neudeck, R. S. Okojie, L-Y; Chen. High-temperature electronics-a role for wide bandgap semiconductors, Proc. IEEE, 90 (2002)1065–1076.10.1109/JPROC.2002.1021571 ↗
5. Wide bandgap semiconductor materials for high temperature electronics10.1016/S0040-6090(98)01672-1 ↗
6. Growth of interfacial intermetallic compound layer in diffusion-bonded sac–cu solder joints during different types of thermomechanical excursion10.1007/s11664-017-5786-0 ↗
7. Microstructure evolution and shear behavior of the solder joints for flip-chip LED on ENIG substrate10.1007/s11664-015-3774-9 ↗
8. Effect of La on the Cu–Sn intermetallic compound (IMC) growth and solder joint reliability10.1016/S0925-8388(01)01747-9 ↗
9. Thermal cycling aging effects on Sn–Ag–Cu solder joint microstructure, IMC and strength10.1016/j.tsf.2004.05.092 ↗
10. Metal-metal bonding process using Ag metallo-organic nanoparticles10.1016/j.actamat.2005.01.047 ↗
11. Low temperature low-pressure die attach with hybrid silver particle paste10.1016/j.microrel.2011.07.088 ↗
12. Joining of silver nanomaterials at low temperatures: processes, properties, and applications10.1021/acsami.5b02134 ↗
13. Identifying the development state of sintered silver (Ag) as a bonding material in the microelectronic packaging via a patent landscape study10.1115/1.4033069 ↗
14. High-temperature reliability of low-temperature and pressureless micron ag sintered joints for die attachment in high-power device10.1007/s10854-018-8903-9 ↗
15. High-temperature reliability of sintered microporous Ag on electroplated Ag, Au, and sputtered Ag metallization substrates10.1007/s10854-017-8087-8 ↗
16. Effect of electroplated Au layer on bonding performance of Ag pastes10.1016/j.jallcom.2017.09.279 ↗
17. Correlation between interfacial microstructure and bonding strength of sintered nanosilver on ENIG and electroplated Ni/Au direct-bond-copper (DBC) substrates10.1016/j.jallcom.2016.03.133 ↗
18. Low-temperature and pressureless sinter joining of Cu with micron/submicron Ag particle paste in air10.1016/j.jallcom.2018.11.251 ↗
19. A novel multiscale silver paste for die bonding on bare copper by low-temperature pressure-free sintering in air10.1016/j.matdes.2017.11.054 ↗
20. Sintering of Ag paste for power devices die attach on cu surfaces
21. Novel interface material used in high power electronic die-attaching on bare Cu substrates10.1007/s10854-016-5208-8 ↗
22. Effects of reducing solvent on copper, nickel, and aluminum joining using silver nanoparticles derived from a silver oxide paste10.2320/matertrans.MI201411 ↗
23. Polymer-protected Cu-Ag mixed nps for low-temperature bonding application10.1007/s11664-012-2008-7 ↗
24. Low-temperature Cu-to-Cu bonding using silver nanoparticles stabilised by saturated dodecanoic acid10.1016/j.msea.2014.07.002 ↗
25. Focusing on luminescent graphene quantum dots: current status and future perspectives10.1039/c3nr33849e ↗
26. Graphene: status and prospects10.1126/science.1158877 ↗
27. Thermal conductivity of isotopically modified graphene10.1038/nmat3207 ↗
28. The rise of graphene10.1038/nmat1849 ↗
29. Superior thermal conductivity of single-layer graphene10.1021/nl0731872 ↗
30. W. Cai, M.L., Y. Zhu, X. Li, S. Chen, L. Shi, R. S. Ruoff, Thermal transport in suspended and supported monolayer graphene grown by chemical vapor deposition. Nano Lett., 10 (2010) 1645–1651.10.1021/nl9041966 ↗
31. Thermal conductivity of graphene in corbino membrane geometry10.1021/nn9016229 ↗
32. Thermal conductivity of suspended pristine graphene measured by Raman spectroscopy10.1103/PhysRevB.83.081419 ↗
33. PH sensor based on chemical-vapor-deposition-synthesized graphene transistor array10.7567/JJAP.52.06GK04 ↗
34. Silane-catalysed fast growth of large single-crystalline graphene on hexagonal boron nitride10.1038/ncomms7499 ↗
35. Macroscale and microscale fracture toughness of microporous sintered ag for applications in power electronic devices10.1016/j.actamat.2017.02.065 ↗
36. Die-attaching silver paste based on a novel solvent for high-power semiconductor devices10.1007/s10853-015-9659-8 ↗
37. Layer-by-layer growth of graphene layers on graphene substrates by chemical vapor deposition10.1016/j.tsf.2011.04.229 ↗
38. Synthesis of freestanding graphene on sic by a rapid-cooling technique10.1103/PhysRevLett.117.205501 ↗
39. Negative thermal expansion coefficient of graphene measured by Raman spectroscopy10.1021/nl201488g ↗
40. Thermal expansion coefficients of graphite crystals10.1016/0008-6223(72)90011-5 ↗
41. Thermal shock performance of DBA/AMB substrates plated by Ni and Ni-P layers for high-temperature applications of power device modules10.3390/ma11122394 ↗
42. XPS study of the Cu@Cu2O core-shell nanoparticles10.1016/j.apsusc.2008.08.110 ↗
43. J. Ghijsen, L. H. Tjeng, J. Van Elp, H. Eskes, J. Westerink, G. A. Sawatzky, M. T. Czyzyk, Electronic structure of Cu2O and CuO., Phys. Rev. B, 38 (1998) 11322.10.1103/PhysRevB.38.11322 ↗
44. Influence of impregnation times on the dispersion of CuO on anatase10.1016/j.molcata.2005.08.021 ↗
45. Low-temperature copper bonding strategy with graphene interlayer10.1021/acsnano.7b07739 ↗
46. Ab initio study of the lattice thermal conductivity of Cu2O using the generalized gradient approximation and hybrid density functional methods10.1103/PhysRevB.96.014304 ↗
47. Assessing the thermoelectric properties of Cuxo (X=1 to 2) thin films as a function of composition10.1063/1.4923031 ↗
48. Printable elastic conductors by in situ formation of silver nanoparticles from silver flakes10.1038/nmat4904 ↗
49. Microstructure and mechanical properties of sintered ag particles with flake and spherical shape from nano to micro size10.1016/j.matdes.2018.11.062 ↗
50. Bonding technology based on solid porous ag for large area chips10.1016/j.scriptamat.2017.11.035 ↗
51. Nano-volcanic eruption of silver10.1038/srep34769 ↗
52. Deformation behavior of sintered nanocrystalline silver layers10.1016/j.actamat.2015.06.040 ↗
53. In situ transmission electron microscopy and scanning transmission electron microscopy studies of sintering of ag and pt nanoparticles10.1016/j.actamat.2014.08.028 ↗
54. Relating rates of catalyst sintering to the disappearance of individual nanoparticles during ostwald ripening10.1021/ja208324n ↗