journal article·2018-05

High-intensity low energy titanium ion implantation into zirconium alloy

A.I. Ryabchikov, E.B. Kashkarov, N.S. Pushilina, M.S. Syrtanov, A.E. Shevelev, O.S. Korneva, A.N. Sutygina, A.M. Lider

Publisher page

Abstract

Abstract This research describes the possibility of ultra-high dose deep titanium ion implantation for surface modification of zirconium alloy Zr-1Nb. The developed method based on repetitively pulsed high intensity low energy titanium ion implantation was used to modify the surface layer. The DC vacuum arc source was used to produce metal plasma. Plasma immersion titanium ions extraction and their ballistic focusing in equipotential space of biased electrode were used to produce high intensity titanium ion beam with the amplitude of 0.5 A at the ion current density 120 and 170 mA/cm2. The solar eclipse effect was used to prevent vacuum arc titanium macroparticles from appearing in the implantation area of Zr sample. Titanium low energy (mean ion energy E = 3 keV) ions were implanted into zirconium alloy with the dose in the range of (5.4–9.56) × 1020 ion/cm2. The effect of ion current density, implantation dose on the phase composition, microstructure and distribution of elements was studied by X-ray diffraction, scanning electron microscopy and glow-discharge optical emission spectroscopy, respectively. The results show the appearance of Zr-Ti intermetallic phases of different stoichiometry after Ti implantation. The intermetallic phases are transformed from both Zr0.7Ti0.3 and Zr0.5Ti0.5 to single Zr0.6Ti0.4 phase with the increase in the implantation dose. The changes in phase composition are attributed to Ti dissolution in zirconium lattice accompanied by the lattice distortions and appearance of macrostrains in intermetallic phases. The depth of Ti penetration into the bulk of Zr increases from 6 to 13 μm with the implantation dose. The hardness and wear resistance of the Ti-implanted zirconium alloy were increased by 1.5 and 1.4 times, respectively. The higher current density (170 mA/cm2) leads to the increase in the grain size and surface roughness negatively affecting the tribological properties of the alloy.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Nuclear Materials and Properties · Metal and Thin Film Mechanics · Advanced materials and composites

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (40)

Show source-provided references
1. Yan · Nucl. Eng. Technol. · 2015 · 47 · 32310.1016/j.net.2014.12.015 ↗
2. 4 - Properties of zirconium alloys and their applications in light water reactors (LWRs)
3. S. Banerjee, M.K. Banerjee, Nuclear applications: zirconium alloys, in: Reference Module in Materials Science and Materials Engineering, Elsevier, 2016. 10.1016/B978-0-12-803581-8.02576-5.10.1016/B978-0-12-803581-8.02576-5 ↗
4. Zieliński · Int. J. Hydrogen Energy · 2011 · 36 · 861910.1016/j.ijhydene.2011.04.002 ↗
5. Daum · J. Nucl. Mater. · 2009 · 392 · 45310.1016/j.jnucmat.2009.04.004 ↗
6. Ensor · J. Nucl. Mater. · 2017 · 496 · 30110.1016/j.jnucmat.2017.08.046 ↗
7. Shen · J. Alloy. Compd. · 2016 · 659 · 2310.1016/j.jallcom.2015.11.031 ↗
8. Zinkle · Acta Mater. · 2013 · 61 · 73510.1016/j.actamat.2012.11.004 ↗
9. N.P. Neureiter, B.J. Garrick, R.A. Bari, J. Beard, M. Percy et al., Lessons learned from the Fukushima nuclear accident for improving safety of U.S. nuclear plants, The National academy of Sciences, 2014.
10. Duan · Nucl. Eng. Des. · 2017 · 316 · 13110.1016/j.nucengdes.2017.02.031 ↗
11. Alat · Surf. Coat. Technol. · 2015 · 281 · 13310.1016/j.surfcoat.2015.08.062 ↗
12. Bao · J. Alloy. Compd. · 2018 · 730 · 8110.1016/j.jallcom.2017.09.281 ↗
13. Alat · J. Nucl. Mater. · 2016 · 478 · 23610.1016/j.jnucmat.2016.05.021 ↗
14. Kim · J. Nucl. Mater. · 2012 · 429 · 14310.1016/j.jnucmat.2012.05.001 ↗
15. Stepanova · J. Alloy. Compd. · 2015 · 645 · S27110.1016/j.jallcom.2014.12.244 ↗
17. Kashkarov · Surf. Coat. Technol. · 2016 · 308 · 210.1016/j.surfcoat.2016.07.111 ↗
18. Kashkarov · Appl. Surf. Sci. · 2018 · 432 · 20710.1016/j.apsusc.2017.04.035 ↗
19. Peng · Appl. Surf. Sci. · 2006 · 252 · 219610.1016/j.apsusc.2005.03.230 ↗
20. Poate · 2013
21. Kurzina · Surf. Coat. Technol. · 2007 · 201 · 846310.1016/j.surfcoat.2006.02.062 ↗
22. Wei · Surf. Coat. Technol. · 1996 · 83 · 21810.1016/0257-8972(95)02828-5 ↗
23. Chapter 4 - Diffusion in Multicomponent Alloys
24. Ryabchikov · Vacuum · 2017 · 143 · 44710.1016/j.vacuum.2017.03.011 ↗
25. Stepanov · Rev. Sci. Instrum. · 2014 · 85 · 4852219
26. Valiev · Nucl. Instr. Meth. Phys. Res. B · 1997 · 127 · 26510.1016/S0168-583X(96)00937-8 ↗
27. Velichko · Comp. Mater. Sci. · 2008 · 43 · 27910.1016/j.commatsci.2007.10.011 ↗
28. Hood · J. Nucl. Mater. · 1994 · 217 · 22910.1016/0022-3115(94)90371-9 ↗
29. Neogy · J. Nucl. Mater. · 2003 · 322 · 19510.1016/j.jnucmat.2003.07.002 ↗
30. Kashkarov · J. Alloy. Compd. · 2018 · 732 · 8010.1016/j.jallcom.2017.10.151 ↗
31. Bacon · J. Nucl. Mater. · 1993 · 206 · 24910.1016/0022-3115(93)90127-K ↗
32. Structure investigation of quenched and tempered alloys of the Zr–Ti system
33. Xia · Surf. Coat. Technol. · 2012 · 206 · 209810.1016/j.surfcoat.2011.09.034 ↗
34. Chang · Surf. Coat. Technol. · 2007 · 201 · 670210.1016/j.surfcoat.2006.09.035 ↗
35. Kaczmarek · J. Nano Res. · 2012 · 18–19 · 19510.4028/www.scientific.net/JNanoR.18-19.195 ↗
36. Attia · Tribol. Int. · 2006 · 39 · 132010.1016/j.triboint.2006.02.053 ↗
37. Qua · Wear · 2016 · 356–357 · 1710.1016/j.wear.2016.02.020 ↗
38. Lu · J. Metals · 2011 · 63 · 53
39. Kim · Nucl. Eng. Des. · 2009 · 239 · 282010.1016/j.nucengdes.2009.08.018 ↗
40. Alansari · Surf. Coat. Technol. · 2017 · 309 · 19510.1016/j.surfcoat.2016.11.070 ↗