Abstract In this paper, effect of laser shock peening (LSP) on high temperature oxidation behavior of P91 steel has been studied. P91 samples were subjected to single and triple LSP treatments at a constant laser power density of 3.9 GW.cm−2. Single and triple LSP treatment led to the formation of ultrafine subgrains of sizes ~300 ± 30 and ~105 ± 10 nm respectively at near surface comparing to unpeened P91 sample (~1200 ± 120 nm). Further, unpeened and LSP treated samples were oxidized at temperatures of 600, 650 and 700 °C for time 5 to 200 h in air. Compare to unpeened sample, single and triple peened samples exhibited two and five fold reduction in weight gain after 200 h of oxidation at highest test temperature (700 °C). Improvement of oxidation resistance in LSP treated samples is attributed to the formation of continuous layer of protective oxides such as (Fe,Cr)2O3, Cr2O3 and MnCr2O4 due to enhanced diffusivity of Cr and Mn from bulk during early stage of oxidation. The enhanced diffusivity Cr and Mn in LSP treated samples have been further supported by reduction in apparent activation energy of oxidation, which is evaluated by modelling the time-temperature dependence of weight gain data in purview of kinetics theory.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Surface Treatment and Residual Stress · High-Temperature Coating Behaviors · Metal Alloys Wear and Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (48)

Show source-provided references
1. R. L. Klueh, Elevated temperature ferritic and martensitic steels and their application to future nuclear reactors, Int. Mater. Rev.,50 (2005) 287–210.10.1179/174328005X41140 ↗
2. Physical metallurgy of modern creep-resistant steel for steam power plants: microstructure and phase transformations10.1155/2016/5468292 ↗
3. New martensitic steels for fossil power plant: creep resistance10.1134/S0031918X10020110 ↗
4. Microstructure and long-term creep properties of 9–12% Cr steels10.1016/j.ijpvp.2007.06.010 ↗
5. Oxidation of ferritic and ferritic–martensitic steels in flowing and static supercritical water10.1016/j.corsci.2015.10.017 ↗
6. Influence of temperature on the oxidation behavior of a ferritic-martensitic steel in supercritical water10.1016/j.corsci.2016.10.020 ↗
7. Characterization of steam oxide morphology for advanced heat resistant steel
8. Corrosion behavior of 9–12% Cr ferritic–martensitic steels in supercritical water10.1016/j.corsci.2009.12.032 ↗
9. Influence of the dissolved oxygen content on corrosion of the ferritic–martensitic steel P92 in supercritical water10.1016/j.corsci.2011.11.013 ↗
10. High temperature oxidation and hot corrosion behaviour of 9Cr 1Mo ferritic cold rolled steel in air at 900°C under cyclic condition
11. Investigation on the enhanced oxidation of ferritic/martensitic steel P92 in pure steam10.3390/ma7042772 ↗
12. Characteristics of oxide scale formed on ferritic stainless steels in simulated reheating atmosphere10.1016/j.surfcoat.2014.09.019 ↗
13. Cyclic oxidation behavior of Fe-9Cr-1Mo steel in water vapor atmosphere10.1007/s11771-009-0089-0 ↗
14. High temperature oxidation of 9–12% Cr ferritic/martensitic steels under dual-environment conditions10.1080/1478422X.2017.1374049 ↗
15. Continuous and cyclic oxidation of T91 ferritic steel under steam10.1016/S0010-938X(03)00173-2 ↗
16. Oxidation behavior of ferritic–martensitic and ODS steels in supercritical water10.1016/j.jnucmat.2012.03.009 ↗
17. The early morphological development of the near surface region of pickled grade 91 tubing exposed to steam and its long term implications
18. Improved oxidation resistance of ferritic–martensitic steels in water vapour containing environments via diffusion coatings10.3184/096034012X13315446390033 ↗
19. Corrosion resistance of chromium-coated ferritic-martensitic steel in supercritical water10.5006/1294 ↗
20. Effect of grain refinement on corrosion of ferritic–martensitic steels in supercritical water environment10.1002/maco.200905446 ↗
21. Improve oxidation resistance at high temperature by nanocrystalline surface layer10.1038/srep13027 ↗
22. Naraparaju · 2013
23. Ren · 2008 · 1
24. Improvement in high temperature oxidation resistance of 9 %Cr ferritic–martensitic steel by enhanced diffusion of Mn10.1007/s11085-015-9596-6 ↗
25. Effect of surface mechanical attrition treatment on microstructure and oxidation behavior in T91 steel at high temperature10.2355/isijinternational.54.1935 ↗
26. Laser shock peening for suppression of hydrogen-induced martensitic transformation in stress corrosion cracking10.1115/1.4036530 ↗
27. Effect of a grain-refined microalloyed steel substrate on the formation mechanism of a tight oxide scale10.1016/j.corsci.2014.04.006 ↗
28. Diffusion of chromium in nanocrystalline iron produced by means of surface mechanical attrition treatment10.1016/S1359-6454(03)00260-X ↗
29. Grain-size effects on the high-temperature oxidation behavior of chromium steels10.1007/s11085-010-9192-8 ↗
30. Effect of grain size on the oxidation of Fe–13Cr–5Ni alloy at 973 Kin Ar–21 vol% O210.1016/j.corsci.2014.11.020 ↗
31. Oxidation behavior of the weld metals, heat affected zone and base metal in the weldments of 2.25Cr-1Mo steel10.1016/0010-938X(93)90087-W ↗
32. Improving the high temperature oxidation resistance of Ni-based superalloy GH202 induced by laser shock processing10.1016/j.jmatprotec.2016.11.040 ↗
33. Effect of laser shock peening on the high temperature oxidation resistance of titanium10.1016/j.surfcoat.2017.07.042 ↗
34. Laser peening process and its impact on materials properties in comparison with shot peening and ultrasonic impact peening10.3390/ma7127925 ↗
35. Study on the effect of multiple laser shock peening on residual stress and microstructural changes in modified 9Cr-1Mo (P91) steel10.1016/j.surfcoat.2018.11.027 ↗
36. Corrosion study on laser shock peened 316L SS in simulated body fluid and chloride medium10.1007/s40516-018-0066-2 ↗
37. Surface roughness and the corrosion resistance of 21Cr ferritic stainless steel10.1016/j.corsci.2012.06.031 ↗
38. Effect of surface roughness on corrosion behavior of the superalloy IN718 in simulated marine environment10.1016/j.jallcom.2018.01.042 ↗
39. Resolving surface chemical states in XPS analysis of first row transition metals, oxides and hydroxides: Cr, Mn, Fe, Co and Ni10.1016/j.apsusc.2010.10.051 ↗
40. Pour-Ali, Ali-Reza Kiani-Rashid, A. Babakhani, M. Norouzi, S. Virtanen, New insights into the effects of surface nanocrystallization on the oxidation of 321 austenitic stainless steel in a humid oxygen environment at 1000 °C, Corros. Sci., 147 (2019) 231–245.10.1016/j.corsci.2018.11.024 ↗
41. In-situ Raman and X-ray photoelectron spectroscopic studies on the pitting corrosion of modified 9Cr-1Mo steel in neutral chloride solution10.1016/j.apsusc.2017.09.179 ↗
42. Investigation on early formation and evolution of oxide scales on ferritic–martensitic steels in supercritical water10.1016/j.corsci.2018.02.036 ↗
43. X-ray photoelectron spectroscopy studies of chromium compounds10.1002/sia.1983 ↗
44. Temperature dependence of oxidation behavior of a ferritic–martensitic steel in supercritical water at 600–700 °C10.1007/s11085-016-9647-7 ↗
45. High temperature oxidation behavior of ferritic steel in supercritical water at 550–700°C10.1080/09603409.2018.1468524 ↗
46. L. Sun and W. Yan, Estimation of oxidation kinetics and oxide scale void position of ferritic-martensitic steels in supercritical water, Adv. Mater. Sci. Eng., (2017), p. 1–12, https://doi.org/10.1155/2017/9154934, Article ID 9154934.10.1155/2017/9154934 ↗
47. Steam oxidation of ferritic steels: kinetics and microestructure
48. Kaplin · 2014