Cavitation erosion resistance of microarc oxidation coating on aluminium alloy
Source abstract
Abstract
Abstract Two ceramic coatings are prepared on 2124 aluminum alloy by microarc oxidation (MAO) technology. To explore the cavitation erosion resistance of the MAO coating, cavitation tests were performed by using a rotating-disk test rig. The mass losses, surface morphologies, chemical compositions and the phase constituents of the samples after cavitation tests were examined by using digital balance, scanning electron microscopy (SEM), energy dispersive spectroscopy (EDS) and X-ray diffraction (XRD), respectively. The results indicate that the MAO coatings can extend the incubation period of aluminum alloy, and thus enhance the cavitation erosion resistance as compared to the untreated aluminum alloy samples. After duration of 63 h cavitation test, a lot of erosion pits and the particles in various shapes can be observed on the surfaces of the aluminum alloy samples, while only a few erosion pits are observed on the MAO coatings. Moreover, the mean depths of erosion on the MAO coatings are lower in the first 30 h and are independent on erosion time. The results show that the cavitation erosion of MAO coating is governed by water mechanical impaction, resulting from the effects of brittle fracture of the MAO coating.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: High-Temperature Coating Behaviors · Metal and Thin Film Mechanics · Cavitation Phenomena in Pumps
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (37)
Show source-provided references
1. Brennen · 2005
2. The cavitation erosion of Fe–Mn–Al alloys
3. Cavitation erosion behavior of as-welded Cu12Mn8Al3Fe2Ni alloy
4. Investigation of Al2O3- and SSiC-ceramic under lubricated, reciprocating sliding contact and cavitation erosion10.1002/mawe.200500860 ↗
5. Experimental test results for four high-speed, high-pressure, orifice-compensated hybrid bearings10.1115/1.2927031 ↗
6. Theoretical and experimental comparisons for rotordynamic coefficients of a high-speed, high-pressure, orifice-compensated hybrid bearing10.1115/1.2831244 ↗
7. Cavitation erosion of laser surface alloyed coatings on Al–12%Si10.1016/0043-1648(94)06584-5 ↗
8. Cavitation erosion and corrosion behaviour of laser surface alloyed MMC of SiC and Si3N4 on Al alloy AA606110.1016/S0257-8972(00)00729-5 ↗
9. Cavitation erosion resistance of a-C:H coatings produced by PECVD on stainless steel and NiTi substrates10.1016/j.surfcoat.2010.04.003 ↗
10. The effect of plasma spray parameters on the cavitation erosion of Al2O3–13% TiO2 coatings10.1016/j.surfcoat.2010.08.044 ↗
11. Synthesis and erosion behaviors of nanoscale coatings prepared by wire arc spraying
12. Electroplating of mild steel by aluminium in a first generation ionic liquid: a green alternative to commercial Al-plating in organic solvents10.1016/j.surfcoat.2006.01.065 ↗
13. Laser cladding of Al(2)O(3)–ZrO(2) eutectic on steel
14. Erosion testing of laser-cladding layers by abrasive water jetting10.1016/j.jmatprotec.2004.12.006 ↗
15. Study of anodic oxidation of aluminum in mixed acid using a pulsed current10.1016/S0257-8972(99)00646-5 ↗
16. Formation of antithermal shock composite membrane on aluminum alloy through anodic oxidation
17. Architecture of multilayer nanocomposite coatings with super-hard diamond-like carbon layers for wear protection at high contact loads10.1016/S0043-1648(96)07425-X ↗
18. Diamond-like carbon coating for aluminum 390 alloy automotive applications10.1016/S0257-8972(97)00061-3 ↗
19. Production of hard and heat-resistant coatings on aluminium using a plasma micro-discharge10.1016/S0257-8972(99)00421-1 ↗
20. Effect of microarc discharge surface treatment on the tensile properties of Al–Cu–Mg alloy10.1016/S0167-577X(02)00605-5 ↗
21. Microstructure and corrosion resistance of modified 2024 Al alloy using surface mechanical attrition treatment combined with microarc oxidation process10.1016/j.corsci.2010.09.061 ↗
22. An improved technique for determining hardness and elastic modulus using load and displacement sensing indentation experiments10.1557/JMR.1992.1564 ↗
23. Preliminary experience with a new compact disk apparatus for cavitation erosion studies10.1016/j.wear.2006.12.064 ↗
24. Cavitation prevention with roughened surface10.1061/(ASCE)0733-9429(2001)127:10(878) ↗
25. Franc · 2004 · 267
26. A study of cavitation bubble collapse pressures and erosion. Part 1: a method for measurement of collapse pressures10.1016/0043-1648(89)90037-9 ↗
27. A study of pressures and erosion produced by collapsing cavitation10.1016/0043-1648(95)07144-X ↗
28. Damages on steel surface at the incubation stage of the vibration cavitation erosion in water10.1016/j.wear.2007.12.011 ↗
29. Investigation into cavitation erosion pits10.1115/1.3075863 ↗
30. Growth mechanism and corrosion behavior of ceramic coatings on aluminum produced by autocontrol AC pulse PEO10.1016/j.surfcoat.2008.03.031 ↗
31. Spheroidal particles produced by cavitation erosion
32. Mechanisms of formation of spheroids produced by cavitation erosion
33. Effect of Al(OH)3 on the hydrogen generation of aluminum–water system10.1016/j.jpowsour.2012.06.077 ↗
34. Corrosion behavior of pressure vessel steel exposed to residual bubbles after cavitation bubble collapse10.5006/1.3548733 ↗
35. Corrosion, erosion and erosion–corrosion performance of plasma electrolytic oxidation (PEO) deposited Al2O3 coatings10.1016/j.surfcoat.2004.09.038 ↗
36. On the collapse of cavities10.1007/s001930200128 ↗
37. Investigation concerning the cavitation resistance of TiN coatings deposited on austenitic stainless steel at various temperatures10.1016/j.wear.2007.08.020 ↗