Evolution of micro-arc oxidation behaviors of the hot-dipping aluminum coatings on Q235 steel substrate
Source abstract
Abstract
Micro-arc oxidation (MAO) is not applicable to prepare ceramic coatings on the surface of steel directly. In this work, hybrid method of MAO and hot-dipping aluminum (HDA) were employed to fabricate com- posite ceramic coatings on the surface of Q235 steel. The evolution of MAO coatings, such as growth rate, thickness of the total coatings, ingrown and outgrown coatings, cross section and surface morphologies and phase composition of the ceramic coatings were studied. The results indicate that both the current density and the processing time can affect the total thickness, the growth rate and the ratio of ingrown and outgrown thickness of the ceramic coatings. The total thickness, outgrown thickness and growth rate have maximum values with the processing time prolonged. The time when the maximum value appears decreases and the ingrown dominant turns to outgrown dominant little by little with the current density increasing. The composite coatings obtained by this hybrid method consists of three layers from inside to outside, i.e. Fe-Al alloy layer next to the substrate, aluminum layer between the Fe-Al layer and the ceramic coatings which is as the top exterior layer. Metallurgical bonding was observed between every of the two layers. There are many micro-pores and micro-cracks, which act as discharge channels and result of quick and non-uniform cooling of melted sections in the MAO coatings. The phase composition of the ceramic coatings is mainly composed of amorphous phase and crystal Al2O3 oxides. The crystal Al2O3 phase includes -Al2O3, -Al2O3 and -Al2O3. Compared with the others, the -Al2O3 content is the least. The MAO process can be divided into three periods, namely the common anodic oxidation stage, the stable MAO stage and the ceramic coatings destroyed stage. The exterior loose part of the ceramic coatings was destroyed badly in the last period which should be avoided during the MAO process. © 2010 Elsevier B.V. All rights reserved.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: High-Temperature Coating Behaviors · Magnesium Alloys: Properties and Applications · Corrosion Behavior and Inhibition
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (19)
Show source-provided references
1. Real-time imaging of coating growth during plasma electrolytic oxidation of titanium10.1016/j.electacta.2007.08.074 ↗
2. Characterisation of discharge events during plasma electrolytic oxidation10.1016/j.surfcoat.2009.05.004 ↗
3. Current status and progress of study on micro-arc oxidation technology
4. Investigation of plasma electrolytic oxidation processes of magnesium alloy MA2-1 under pulse polarization modes10.1016/j.surfcoat.2004.09.036 ↗
5. Growth process and wear resistance for ceramic coatings formed on Al–Cu–Mg alloy by micro-arc oxidation10.1016/j.apsusc.2005.12.156 ↗
6. Plasma electrolytic oxidation of arc-sprayed aluminum coatings10.1007/s11666-007-9104-x ↗
7. Characterization and wear- and corrosion-resistance of microarc oxidation ceramic coatings on aluminum alloy10.1016/j.jallcom.2004.05.084 ↗
8. Microstructures and phase composition of ceramic coatings on steel fabricated by hot dipping and micro-arc oxidation
9. Deposition of duplex Al2O3/aluminum coatings on steel using a combined technique of arc spraying and plasma electrolytic oxidation10.1016/j.apsusc.2005.04.036 ↗
10. Structure and mechanical properties of ceramic coatings fabricated by plasma electrolytic oxidation on aluminized steel10.1016/j.apsusc.2007.04.007 ↗
11. Wear resistance of micro-arc oxidized ceramic layers on aluminum alloy
12. Evolution of aluminum layer transformed into ceramic coatings on steel substrate
13. Size change of Ly12 aluminum alloy in process of microarc oxidation
14. Process characteristics and parameters of anodic oxidation by spark discharge (ANOF)10.1002/crat.2170190721 ↗
15. Anodic processes in plasma electrolytic oxidation of aluminium in alkaline solutions10.1016/j.electacta.2003.11.027 ↗
16. Application fields of ANOF layers and composites10.1002/crat.2170211224 ↗
17. Structure and properties of ANOF layers10.1002/crat.2170190117 ↗
18. Mechanism of anodic spark deposition
19. The properties and the processes of the micro-arc oxidation ceramic coatings on aluminum alloys