journal article·2019-06

The influence of copper on the stress corrosion cracking of 304 stainless steel

Xuehan Wang, Zhile Yang, Zheng Wang, Qiaoying Shi, Bin Xu, Chengshuang Zhou, Lin Zhang

Publisher page

Abstract

Abstract Water leakage occurred in hot-water pipes made of 304 stainless steel of an antiburning boiler after usage for 8 months. The detection revealed that the 304 austenitic stainless steel in a combustion chamber cracked on the side of the hot water outflow. This study analyzed the cause of cracking of the 304 austenitic stainless-steel hot water pipe by using microstructural, intergranular corrosion, and corrosion product analyses. Results showed that the 304 stainless steel, which met the material requirements, fractured via a mixed cracking that included transgranular and intergranular cracking (mainly transgranular). Moreover, a large amount of single copper accumulated on the crack surface, which indicated that the crack was induced by stress corrosion involving copper ions and mechanical stress. High temperature was another factor that induced cracking because the passive film of 304 stainless steel weakened in hot water. The copper ions came from the inferior brass valves when immersed in hot water with oxygen exposure. Basing on the above results, this type of cracking can be prevented by using 2205 duplex stainless steel (DSS) instead of 304 stainless steel. The stress corrosion behaviors of 304 stainless steel and 2205 DSS in aqueous solution with a certain concentration of copper chloride were analyzed using four-point bending test. Results showed that 2205 DSS did not crack, whereas 304 austenitic stainless failed in the test.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Corrosion Behavior and Inhibition · Concrete Corrosion and Durability

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (31)

Show source-provided references
1. Nonequilibrium grain boundary segregation of sulfur and its effect on intergranular corrosion for 304 stainless steel10.1016/S1006-706X(11)60079-4 ↗
2. Failure analysis of the 304 stainless steel tube in a gas analyzer10.1016/j.engfailanal.2011.10.004 ↗
3. Corrosion behaviour of 316L stainless steel and anti-corrosion materials in a high acidified chloride solution10.1016/j.apsusc.2014.09.205 ↗
4. Characterization of corrosion scale formed on stainless steel delivery pipe for reclaimed water treatment10.1016/j.watres.2015.11.021 ↗
5. Development of stress corrosion cracking resistant welds of 321 stainless steel by simple surface engineering10.1016/j.apsusc.2017.07.223 ↗
6. A study on the corrosion of stainless steel floor drains in an indoor swimming pool10.1016/j.engfailanal.2017.02.014 ↗
7. Sulphide stress cracking behaviour of the dissimilar metal welded joint of X60 pipeline steel and Inconel 625 alloy10.1016/j.corsci.2016.04.044 ↗
8. The effect of δ-ferrite on fatigue cracks in 304L steels10.1016/S0142-1123(00)00043-8 ↗
9. Crystallography of intergranular corrosion in sensitized austenitic stainless steel10.1016/j.matchar.2018.07.014 ↗
10. A hydrogen embrittlement mechanism for sensitized types 304, 316 and 310 austenitic stainless steels in boiling saturated magnesium chloride solutions10.1016/j.corsci.2009.07.016 ↗
11. Improved resistance to hydrogen environment embrittlement of warm-deformed 304 austenitic stainless steel in high-pressure hydrogen atmosphere10.1016/j.corsci.2018.12.015 ↗
12. Martensite caused by passive film-induced stress during stress corrosion cracking in type 304 stainless steel10.1016/S0921-5093(03)00269-7 ↗
13. Failure analysis of the wall tubes of a water-tube boiler10.1016/j.engfailanal.2017.05.032 ↗
14. Experimental study on temperature, heat flux, strain and stress distribution of boiler water walls10.1016/j.applthermaleng.2016.11.039 ↗
15. Effect of free Cr content on corrosion behavior of 3Cr steels in a CO2 environment10.1016/j.apsusc.2017.06.320 ↗
16. Characterization and corrosion behavior of F6NM stainless steel treated in high temperature water10.1016/j.apsusc.2017.11.089 ↗
17. Passivation behaviour of 304 stainless steel in an ionic liquid with a fluorinated anion10.1016/j.apsusc.2015.08.189 ↗
18. Structure and corrosion properties of Cr coating deposited on aerospace bearing steel10.1016/j.apsusc.2017.06.099 ↗
19. Repassivation behavior of 316L stainless steel in borate buffer solution: kinetics analysis of anodic dissolution and film formation10.1016/j.apsusc.2015.09.018 ↗
20. Effect of dissolved oxygen and temperature on fatigue crack growth rate behaviour of SA312 type 304L(N) material in water environment10.1016/j.ijfatigue.2016.10.022 ↗
21. The effect of temperature on the passive film properties and pitting behaviour of a Fe-Cr-Ni alloy10.1016/0010-938X(96)00176-X ↗
22. The oxidation behaviour of 304 stainless steel in oxygenated high temperature water10.1016/j.corsci.2010.09.001 ↗
23. Finite element calculation of crack propagation in type 304 stainless steel in diluted sulphuric acid solutions10.1016/j.corsci.2006.06.025 ↗
24. Predicting crack growth rate vs. temperature behaviour of type 304 stainless steel in dilute sulphuric acid solutions10.1016/S0010-938X(01)00151-2 ↗
25. Effects of flow, brass location, tube materials and temperature on corrosion of brass plumbing devices10.1016/j.corsci.2011.01.060 ↗
26. Initial oxidation of brass induced by humidified air10.1016/j.apsusc.2011.09.080 ↗
27. Surface characterization of copper, zinc and brass in contact with tap water inhibited with phosphate ions10.1016/j.apsusc.2011.07.002 ↗
28. Effect of “475 °C embrittlement” on duplex stainless steels localized corrosion resistance10.1016/j.corsci.2004.06.012 ↗
29. Influence of sensitization on passive films in AISI 2205 duplex stainless steel10.1016/j.jallcom.2015.10.246 ↗
30. Electronic properties and corrosion resistance of passive films on austenitic and duplex stainless steels10.1016/j.electacta.2018.04.058 ↗
31. Corrosion resistance of super duplex stainless steels in chloride ion containing environments: investigations by means of a new microelectrochemical method: I. Precipitation-free states10.1016/S0010-938X(00)00087-1 ↗