Abstract

Abstract A new corrosion inhibitor, cerium malate, was synthesized. Its inhibiting behaviour on coupled Al2Cu-Al2CuMg-Al, Al2CuMg-Al and Al2Cu-Al was studied. Cerium malate is effective in corrosion inhibition of the three coupled systems. The inhibition mechanism of cerium malate on pitting corrosion of Al2CuMg and Al2Cu phases in AA 2024-T3 was analyzed by scanning vibrating electrode technique (SVET), atomic force microscopy (AFM) and scanning kelvin probe force microscopy (SKPFM). The results indicate that cerium malate has good inhibiting effect on AA 2024-T3.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Aluminum Alloy Microstructure Properties · Corrosion Behavior and Inhibition · Aluminum Alloys Composites Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (51)

Show source-provided references
1. Corrosion protection of untreated AA2024-T3 in chloride solution by a chromate conversion coating monitored with Raman spectroscopy10.1149/1.1838630 ↗
2. Local dissolution phenomena associated with S phase (Al2CuMg) particles in aluminum alloy 2024-T310.1149/1.1837874 ↗
3. Davis · 1999
4. SVET study of galvanic corrosion of Al/Mg2Si couple in aqueous solutions at different pH10.1149/2.0671706jes ↗
5. Localized corrosion mechanism of 2×××-series Al alloy containing S(Al2CuMg) and θ′(Al2Cu) precipitates in 4.0% NaCl solution at pH 6.110.1016/j.matchemphys.2004.11.034 ↗
6. Study of localized corrosion in AA2024 aluminium alloy using electron tomography10.1016/j.corsci.2012.02.001 ↗
7. Simulating the galvanic coupling between S-Al2CuMg phase particles and the matrix of 2024 aerospace aluminium alloy10.1016/j.corsci.2012.07.020 ↗
8. Corrosion of AA2024-T3 Part I: localized corrosion of isolated IM particles10.1016/j.corsci.2010.09.009 ↗
9. A compilation of corrosion potentials reported for intermetallic phases in aluminum alloys10.1149/1.2048447 ↗
10. First-principles surface interaction studies of aluminum-copper and aluminum-copper-magnesium secondary phases in aluminum alloys10.1016/j.apsusc.2017.12.256 ↗
11. Corrosion protection of AA 2024-T3 by bis-[3-(triethoxysilyl)propyl]tetrasulfide in neutral sodium chloride solution. Part 1: corrosion of AA 2024-T310.1016/S0010-938X(03)00060-X ↗
12. A study on pitting corrosion of aluminum alloy 2024-T3 by scanning microreference electrode technique10.1016/S0921-5093(02)00445-8 ↗
13. Corrosion of AA2024-T3 Part II: co-operative corrosion10.1016/j.corsci.2010.09.030 ↗
14. Corrosion of AA2024-T3 Part III: propagation10.1016/j.corsci.2010.09.035 ↗
15. Revie · 1985
16. High effective organic corrosion inhibitors for 2024 aluminium alloy10.1016/j.electacta.2007.05.058 ↗
17. Mechanism of corrosion inhibition of AA2024 by rare-earth compounds10.1021/jp0560664 ↗
18. Synergistic effect between 8-hydroxyquinoline and benzotriazole for the corrosion protection of 2024 aluminium alloy: a local electrochemical impedance approach10.1016/j.corsci.2015.09.002 ↗
19. LDHs/graphene film on aluminum alloys for active protection10.1016/j.apsusc.2017.10.126 ↗
20. Protection of 2024-T3 aluminium alloy by corrosion resistant phytic acid conversion coating10.1016/j.apsusc.2013.04.156 ↗
21. Corrosion inhibition of aluminum alloy 2024-T3 by aqueous vanadium species10.1149/1.2907772 ↗
22. Corrosion inhibition of aluminum alloy 2024-T3 by sodium molybdate10.1149/2.044403jes ↗
23. On the importance of irreversibility of corrosion inhibitors for active coating protection of AA2024-T310.1016/j.corsci.2018.05.037 ↗
24. Corrosion inhibition with rare earth metal salts10.1016/0925-8388(92)90359-H ↗
25. Electrochemical study of modified non-functional bis-silane layers on Al alloy 2024-T310.1016/j.corsci.2008.01.018 ↗
26. The characteristics of corrosion inhibiting films formed in the presence of rare earth cations
27. Corrosion inhibition of pure aluminium and alloys AA2024-T3 and AA7075-T6 by cerium(III) and cerium(IV) salts10.1149/2.0431603jes ↗
28. Development of cerium-rich layers on anodic films formed on pure aluminium and AA7075-T6 alloy10.1149/2.0091501jes ↗
29. Characterization of 2024-T3 aluminum alloy after rare earth desmutting10.1149/2.0201606jes ↗
30. Electrochemical techniques for practical evaluation of corrosion inhibitor effectiveness. Performance of cerium nitrate as corrosion inhibitor for AA2024-T3 alloy10.1016/j.corsci.2010.06.012 ↗
31. Cerium tartrate as a pigment in epoxy coatings for corrosion protection of AA 2024-T310.1016/j.porgcoat.2017.01.002 ↗
32. The characterisation and performance of Ce(dbp)3-inhibited epoxy coatings10.1016/j.porgcoat.2010.10.009 ↗
33. Cerium cinnamate as an environmentally benign inhibitor pigment for epoxy coatings on AA 2024-T310.1016/j.porgcoat.2014.01.003 ↗
34. Synergistic corrosion inhibition effect of metal cations and mixtures of organic compounds: a review10.1016/j.jece.2016.12.001 ↗
35. Comparison of the synergistic effects of inhibitor mixtures tailored for enhanced corrosion protection of bare and coated AA2024-T310.1016/j.surfcoat.2015.10.075 ↗
36. The use of macroscopic modelling of intermetallic phases in aluminium alloys in the study of ferricyanide accelerated chromate conversion coatings10.1016/S0010-938X(01)00181-0 ↗
37. Cerium tartrate as a corrosion inhibitor for AA 2024-T310.1016/j.corsci.2015.03.010 ↗
38. Wiberg · 2001
39. Study of corrosion inhibition of coupled Al2Cu-Al and Al3Fe-Al by cerium cinnamate using scanning vibrating electrode technique and scanning ion-selective electrode technique10.1016/j.corsci.2015.05.019 ↗
40. Simulating corrosion of Al2CuMg phase by measuring ionic currents, chloride concentration and pH10.1016/j.corsci.2014.07.021 ↗
41. Combination of AFM, SKPFM, and SIMS to study the corrosion behavior of S-phase particles in AA2024-T35110.1149/1.2833315 ↗
42. The anodic dissolution of magnesium in chloride and sulphate solutions10.1016/S0010-938X(97)00090-5 ↗
43. Stable pit formation on AA2024-T3 in a NaCl environment10.1016/j.corsci.2009.08.043 ↗
44. Investigation of the de-alloying behaviour of θ-phase (Al2Cu) in AA2024-T351 aluminium alloy10.1016/j.corsci.2016.03.003 ↗
45. Effects of pH and chloride concentration on pitting corrosion of AA6061 aluminum alloy10.1016/j.corsci.2008.03.006 ↗
46. Unveiling the effect of the electrodes area on the corrosion mechanism of a graphite -AA2024-T3 galvanic couple by localized electrochemistry10.1016/j.electacta.2018.04.187 ↗
47. Statistical study of the corrosion behavior of Al2CuMg intermetallics in AA2024-T351 by SKPFM10.1149/1.2799089 ↗
48. The investigation of cerium as a cathodic inhibitor for aluminum-copper alloys10.1149/1.2049985 ↗
49. The effect of post-treatment time and temperature on cerium-based conversion coatings on Al 2024-T310.1016/j.corsci.2009.09.023 ↗
50. Electrochemical characteristics of intermetallic phases in aluminum alloys: an experimental survey and discussion10.1149/1.1869984 ↗
51. Localized corrosion of 2024–T351 aluminium alloy in chloride media10.1016/S0010-938X(98)00116-4 ↗