Ta2O5 films were deposited by conventional electron beam evaporation method and then annealed in air at different temperature from 873 to 1273 K. It was found that the film structure changed from amorphous phase to hexagonal phase when annealed at 1073 K, then transformed to orthorhombic phase after annealed at 1273 K. The transmittance was improved after annealed at 873 K, and it decreased as the annealing temperature increased further. The total integrated scattering (TIS) tests and AFM results showed that both scattering and root mean square (RMS) roughness of films increased with the annealing temperature increasing. X-ray photoelectron spectroscopy (XPS) analysis showed that the film obtained better stoichiometry and the O/Ta ratio increased to 2.50 after annealing. It was found that the laser-induced damage threshold (LIDT) increased to the maximum when annealed at 873 K, while it decreased when the annealing temperature increased further. Detailed damaged models dominated by different parameters during annealing were discussed. (C) 2008 Elsevier B. V. All rights reserved.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Semiconductor materials and devices · Metal and Thin Film Mechanics · High-Temperature Coating Behaviors
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (26)
Show source-provided references
1. Gas pressures influence on the optical and mechanical properties of Ta2O5 films produced by reactive low voltage ion plating (RLVIP)10.1016/S0040-6090(99)00153-4 ↗
2. Stability and effect of annealing on the optical properties of plasma-deposited Ta2O5 and Nb2O5 films10.1016/j.tsf.2006.05.047 ↗
3. Laser conditioning of optical thin films
4. Effect of thermal annealing on the optical properties and residual stress of TiO2 films produced by ion-assisted deposition10.1364/AO.44.002996 ↗
5. Titania, silicon dioxide, and tantalum pentoxide waveguides and optical resonant filters prepared with radio-frequency magnetron sputtering and annealing10.1364/AO.44.000378 ↗
6. Influence of SiO2 additional layers on the laser induced damage threshold of Ta2O5 films10.1016/j.optlastec.2007.08.008 ↗
7. Laser-induced damage threshold in n-on-1 regime of Ta2O5 films at 532, 800, and 1064 nm
8. Strong photo-induced refractive index changes in RF-sputtered tantalum oxide planar waveguides
9. Sub-micron period grating structures in Ta2O5 thin oxide films patterned using UV laser post-exposure chemically assisted selective etching10.1016/j.tsf.2003.11.175 ↗
10. Employing oxygen-plasma posttreatment to improve the laser-induced damage threshold of ZrO2 films prepared by the electron-beam evaporation method10.1364/OL.29.002870 ↗
11. Laser conditioning of high-reflective and anti-reflective coatings at 1064nm
12. Investigation of damage threshold to TiO2 coatings at different laser wavelength and pulse duration10.1016/j.tsf.2007.06.058 ↗
13. Effects of annealing on laser-induced damage threshold of TiO2/SiO2 high reflectors10.1016/j.apsusc.2007.05.005 ↗
14. Annealing effects on structure and laser-induced damage threshold of Ta2O5/SiO2 dielectric mirrors10.1016/S0169-4332(03)00153-3 ↗
15. Microstructure and laser-induced damage threshold of ZrO2 coatings dependence on annealing temperature10.1016/j.apsusc.2004.05.267 ↗
16. Measurements of light scattering from glass substrates by total integrated scattering10.1364/AO.44.006163 ↗
17. ISO 11254-1:2000: lasers and laser-related equipment-determination of laser-induced damage threshold of optical surfaces. Part 1. 1-on-1 test.
18. Crystallization effects in oxygen annealed Ta2O5 thin films on Si10.1016/S0040-6090(00)01569-8 ↗
19. Effects of heating in air and chlorine atmosphere on the crystalline structure of pure Ta2O5 or mixed with carbon10.1023/A:1004469622713 ↗
20. Born · 1970
21. Optical properties and microstructure of plasma deposited Ta2O5 and Nb2O5 films10.1116/1.1851544 ↗
22. Influence of oxidation temperature on the microstructure and electrical properties of Ta2O5 on Si10.1016/S0026-2692(02)00120-9 ↗
23. Recent progress on laser-induced modifications and intrinsic bulk damage of wide-gap optical materials10.1117/12.7977089 ↗
24. Roles of absorbing defects and structural defects in multilayer under single-shot and multi-shot laser radiation10.1016/j.apsusc.2003.12.006 ↗
25. Electronic structure of oxygen vacancy in Ta2O510.1063/1.370831 ↗
26. Effects of oxygen content on the optical properties of tantalum oxide films deposited by ion-beam sputtering10.1364/AO.24.000490 ↗