journal article·2015-08

Low-temperature preparation of high-n TiO2 thin film on glass by pulsed laser deposition

Akihiro Ishii, Yoko Nakamura, Itaru Oikawa, Atsunori Kamegawa, Hitoshi Takamura

Publisher page

Abstract

Abstract Single-phase rutile-type TiO2 thin films with a high refractive index (n) and a low extinction coefficient (k) prepared on glass are expected to improve the performance of anti-reflection coatings. In this study, TiO2 thin films were prepared by the pulsed laser deposition (PLD) method at temperatures ranging from room temperature to 600 °C under an oxygen partial pressure of 1–9 Pa or a 10−5 Pa vacuum, and their crystal structure, microstructure and optical properties were investigated. A single-phase rutile-type TiO2 thin film was successfully prepared on a glass substrate by depositing at room temperature in a vacuum followed by post-annealing at 450 °C in air. A nanocrystalline oxygen-deficient phase in the as-deposited films plays an important role in the formation of the single rutile phase during post-annealing. The single-phase rutile-type TiO2 thin films showed excellent optical properties, with n = 3.14 and k
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: TiO2 Photocatalysis and Solar Cells · Advanced Photocatalysis Techniques · ZnO doping and properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (33)

Show source-provided references
1. Tri-layer antireflection coatings (SiO2/SiO2–TiO2/TiO2) for silicon solar cells using a sol–gel technique10.1016/j.solmat.2006.04.001 ↗
2. Influence of substrate and annealing temperatures on optical properties of RF-sputtered TiO2 thin films10.1016/j.optmat.2009.07.011 ↗
3. Low temperature preparation of high refractive index and mechanically resistant sol–gel TiO2 films for multilayer antireflective coating applications10.1023/A:1011232807842 ↗
4. The surface science of titanium dioxide10.1016/S0167-5729(02)00100-0 ↗
5. Review of the anatase to rutile phase transformation10.1007/s10853-010-5113-0 ↗
6. Structural evolution and optical properties of TiO2 thin films prepared by thermal oxidation of sputtered Ti films10.1063/1.1309039 ↗
7. Structural properties of TiO2 films grown by pulsed laser deposition
8. Epitaxial growth of titanium oxide thin films on c-cut and α-cut sapphire substrates10.1016/j.susc.2007.09.019 ↗
9. Structure and energetics of stoichiometric TiO2 anatase surfaces10.1103/PhysRevB.63.155409 ↗
10. dc reactive magnetron sputtering of titanium-structural and optical characterization of TiO2 films10.1063/1.351264 ↗
11. Resistive switching mechanism of TiO2 thin films grown by atomic-layer deposition10.1063/1.2001146 ↗
12. Status of pulsed laser deposition: challenges and opportunities10.1179/174329406X98502 ↗
13. High rate thick film growth10.1146/annurev.ms.07.080177.001323 ↗
14. Growth and characteristics of laser deposited anatase and rutile TiO2 films on Si substrates10.1016/j.tsf.2008.08.179 ↗
15. Boulbar · Appl. Surf. Sci. · 2011 · 257 · 538010.1016/j.apsusc.2010.10.149 ↗
16. Rutile-type TiO2 thin film for high-k gate insulator10.1016/S0040-6090(02)01105-7 ↗
17. Fabrication of TiO2-based transparent conducting oxide films on glass by pulsed laser deposition10.1143/JJAP.46.L86 ↗
18. Atomic layer chemical vapor deposition of TiO2: low temperature epitaxy of rutile and anatase10.1149/1.1393901 ↗
19. TiO2 thin films prepared by PLD for photocatalytic applications10.1016/S0169-4332(02)00347-1 ↗
20. Pulsed laser deposition of anatase and rutile TiO2 thin films10.1016/j.surfcoat.2007.03.004 ↗
21. Influence of laser energy density on the plasma expansion dynamics and dil stoichiometry during laser ablation of BiSrCaCuO10.1063/1.362357 ↗
22. XPS characterization of TiO2 layers deposited on quartz plates
23. XPS study of cobalt doped TiO2 films prepared by pulsed laser deposition10.1002/sia.5397 ↗
24. Nonstoichiometry in TiO2−y studied by ion beam methods and photoelectron spectroscopy10.1155/2012/826873 ↗
25. Refractive index of thin films of SiO2, ZrO2, and HfO2 as a function of the films’ mass density10.1364/AO.44.003006 ↗
26. Room-temperature deposition of amorphous titanium dioxide thin film with high refractive index by a filtered cathodic vacuum arc technique10.1364/AO.43.001281 ↗
27. Effect of O2 in O2/Ar gas mixture on morphological and optical properties of TiO2 thin film deposited by DC cylindrical magnetron sputtering10.1007/s10894-013-9598-9 ↗
28. Optical constants of TiO1.7 thin films deposited by electron beam gun10.1016/j.jallcom.2007.09.034 ↗
29. Monitoring electronic structure changes of TiO2(110) via sign reversal of adsorbate vibrational bands10.1039/b926602j ↗
30. Structural and optical properties of titanium oxide thin films deposited on unheated substrate at different total pressures by reactive dc magnetron sputtering with a substrate bias
31. Thermal expansion of anatase and rutile between 300 and 575K using synchrotron powder X-ray diffraction10.1154/1.2790965 ↗
32. Residual stresses and Raman shift relation in anatase TiO2 thin film10.1016/j.tsf.2009.02.141 ↗
33. Oxygen diffusion in yttria-stabilized zirconia subjected to uniaxial stress10.1016/j.ssi.2010.01.023 ↗