Inter-yarn friction helps to increase energy absorption in ballistic fabrics. This paper reports on the results of sol–gel treatment on aramid yarns to increase the inter-yarn friction. Two types of TiO2/ZnO hydrosols (submicro-sized and nano-sized) prepared using hydrolysis and peptization methods were used to treat aramid yarns with and without curing. SEM was used to characterize the change in morphology. FTIR and EDX analyses were applied to identify the coating substance. The inter-yarn friction was tested using Capstan method. Images from SEM showed that the surface of the yarn treated with TiO2/ZnO submicro-sized hydrosol was covered with lump-like coating whilst in the case of TiO2/ZnO nano-sized sol treatment, the coating on the fibres was more film-like. The substance in the coating was confirmed as titanium dioxide and zinc oxide by FTIR and EDX analyses. The test results for coefficient of friction revealed that the coefficient of friction between the yarns treated by submicro-sized hydrosol was 54% higher than the non-treated, and the nano-sized hydrosol was associated to a 10% increase. However, the curing process had little effect on the coefficient of friction between yarns. The study also showed that the tensile properties of the treated yarns and the weight add-on were not significantly affected.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Textile materials and evaluations · Dyeing and Modifying Textile Fibers · Fiber-reinforced polymer composites

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (41)

Show source-provided references
1. Ballistic impact into fabric and compliant composite laminates10.1016/S0263-8223(03)00029-1 ↗
2. Modeling friction effects on the ballistic impact behavior of a single-ply high-strength fabric10.1016/j.ijimpeng.2004.06.008 ↗
3. A numerical investigation of the influence of friction on energy absorption by a high-strength fabric subjected to ballistic impact10.1016/j.ijimpeng.2004.11.005 ↗
4. Modeling the effects of yarn material properties and friction on the ballistic impact of a plain-weave fabric10.1016/j.compstruct.2008.11.012 ↗
5. Ballistic impact of Twaron CT709® plain weave fabrics10.1080/15376494.2011.575532 ↗
6. Ballistic impact modeling of woven fabrics considering yarn strength, friction, projectile impact location, and fabric boundary condition effects10.1016/j.compstruct.2012.05.030 ↗
7. Influence of yarn gripping on the ballistic performance of woven fabrics from ultra-high molecular weight polyethylene fibre10.1016/j.compositesb.2014.02.022 ↗
8. Role of interfacial friction and lubrication in yarn and fabric mechanics10.1177/004051759006001201 ↗
9. Yarn pull-out as a mechanism for dissipating ballistic impact energy in Kevlar® KM-2 fabric: Part I: quasi-static characterization of yarn pull-out10.1177/004051750407401012 ↗
10. Yarn pull-out as a mechanism for dissipating ballistic impact energy in Kevlar(R) KM-2 fabric: Part II: predicting ballistic performance10.1177/004051750407401101 ↗
11. Dissipation of energy by bullet proof aramid fabric10.1023/A:1018674528993 ↗
12. Mechanics of energy absorbability in plain-woven fabrics: an analytical approach
13. Improving the impact resistance performance of Kevlar fabrics using silica based shear thickening fluid10.1016/j.msea.2011.09.021 ↗
14. Plasma modification of Kevlar fabrics for ballistic applications10.1177/0040517512450765 ↗
15. Surface modification of aramid fibers by atmospheric pressure plasma-enhanced vapor deposition10.1177/0040517513515311 ↗
16. Improvement in UV-protection property of cotton fabric and fastness of finishing performance10.4028/www.scientific.net/AMR.441.266 ↗
17. TiO2 and ZnO water sol preparation by sol–gel method and application on polyester fabric of antistatic finishing10.4028/www.scientific.net/AMR.331.270 ↗
18. Wright · 2000 · vol. 4
19. Improving the photo-stability of high performance aramid fibers by sol-gel treatment10.1007/s12221-008-0073-6 ↗
20. Applying the sol-gel method to the deposition of nanocoats on textiles to improve their abrasion resistance10.1002/app.36353 ↗
21. Dyeing and DP treatment of sol-gel pre-treated cotton fabrics10.1007/s12221-011-0226-x ↗
22. More about fibre friction and its measurements10.1080/00405160903178591 ↗
23. Adsorption–photodegradation of humic acid in water by using ZnO coupled TiO2/bamboo charcoal under visible light irradiation10.1016/j.jhazmat.2013.08.037 ↗
24. Photocatalytic activity of thin TiO2 films deposited using sol–gel and plasma enhanced chemical vapor deposition methods10.1016/j.ceramint.2012.09.046 ↗
25. Porous texture of a titanium oxide gel: evolution as a function of medium used10.1016/S0022-3093(05)80610-6 ↗
26. Syntheses of submicron TiO2 powders in vapor. Liquid and supercritical phases10.1016/0254-0584(92)90207-O ↗
27. Chemical and micro structural properties of TiO2 synthesized by sol-gel procedure10.1016/S0921-5107(96)02041-7 ↗
28. Infrared studies of the surface hydroxyl groups on titanium dioxide, and of the chemisorption of carbon monoxide and carbon dioxide10.1021/j100823a011 ↗
29. Surface modification for Nano-ZnO and its mechanism
30. Properties and distribution of the surface hydroxyl groups of TiO2
31. Chitosan/poly (vinyl alcohol) films containing ZnO nanoparticles and plasticizers10.1016/j.msec.2009.01.026 ↗
32. Robert · 2009 · 38
33. Particle size analysis of zirconia sol in process of chemical coating
34. Effect of chemical treatment of Kevlar fibers on mechanical interfacial properties of composites10.1006/jcis.2002.8479 ↗
35. The effect of chemical treatment on reinforcement/matrix interaction in Kevlar-fiber/bismaleimide composites10.1016/S0266-3538(00)00074-9 ↗
36. Modification of mechanical properties of Kevlar fibre by polymer infiltration10.1007/BF00353106 ↗
37. Influence of hydrolytic and chemical treatment on the mechanical properties of aramid and copolyaramid fibers10.1177/004051759806800807 ↗
38. Improvement of the adhesion of Kevlar fiber to bismaleimide resin by surface chemical modification10.1163/156856199X00109 ↗
39. New concepts in para-Aramid fibers10.1177/004051759206201210 ↗
40. A new approach to high modulus, high tenacity fibers10.1295/polymj.19.119 ↗
41. Deterioration of aramid, glass, and carbon fibers due to alkali, acid, and water in different temperatures