journal article·2017-02

Effect of surface treatment on the corrosion properties of magnesium-based fibre metal laminate

X. Zhang, Y. Zhang, Q.Y. Ma, Y. Dai, F.P. Hu, G.B. Wei, T.C. Xu, Q.W. Zeng, S.Z. Wang, W.D. Xie

Publisher page

Abstract

Abstract The surface roughness, weight of phosphating film and wettability of magnesium alloy substrates after abrasion and phosphating treatment were investigated in this work. The interfacial bonding and corrosion properties of a magnesium-based fibre metal laminate (MgFML) were analysed. The results showed that the wettability of the magnesium alloy was greatly influenced by the surface roughness, and the rough surface possessed a larger surface energy and better wettability. The surface energy and wettability of the magnesium alloy were significantly improved by the phosphating treatment. After phosphating for 5 min, a phosphating film with a double-layer structure was formed on the magnesium substrate, and the weight of the phosphating film and the surface energy reached their maximum values. The surface energies of the phosphated substrate after abrasion with #120 and #3000 grit abrasive papers were 84.31 mJ/m 2 and 83.65 mJ/m 2 , respectively. The wettability of the phosphated magnesium was significantly better than the abraded magnesium. The phosphated AZ31B sheet had a better corrosion resistance than the abraded AZ31B sheet within short times. The corrosion resistance of the magnesium alloy was greatly increased by being composited with glass fibre/epoxy prepregs.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Material Properties and Applications · Mechanical Behavior of Composites · Aluminum Alloys Composites Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (38)

Show source-provided references
1. The prediction of tensile failure in titanium-based thermoplastic fibre–metal laminates10.1016/j.compscitech.2005.11.031 ↗
2. Long term behaviour of Glare10.1023/A:1025589812963 ↗
3. Fatigue and damage tolerance issues of Glare in aircraft structures10.1016/j.ijfatigue.2006.02.015 ↗
4. A review on the development and properties of continuous fiber/epoxy/aluminum hybrid composites for aircraft structures10.1590/S1516-14392006000300002 ↗
5. A review: Fibre metal laminates background, bonding types and applied test methods10.1016/j.matdes.2011.03.011 ↗
6. Corrosion protection of Mg/Al alloys by thermal sprayed aluminium coatings10.1016/j.apsusc.2009.03.022 ↗
7. The fracture properties of a fibre-metal laminate based on magnesium alloy10.1016/j.compositesb.2005.06.002 ↗
8. Applicability of AZ31B-H24 magnesium in fibre metal laminates −An experimental impact research10.1016/j.compositesa.2012.04.008 ↗
9. Impact characterization of thermoformable fibre metal laminates of 2024-T3 aluminium and AZ31B-H24 magnesium based on self-reinforced polypropylene10.1016/j.compositesa.2014.02.011 ↗
10. The applicability of magnesium based Fibre Metal Laminates in aerospace structures10.1016/j.compscitech.2008.06.017 ↗
11. Hygrothermal effects evaluation using the iosipescu shear test for Glare laminates10.1590/S1678-58782008000300006 ↗
12. Effect of the interface stiffness and skin-core adhesion efficiency on the interfacial stress distribution of sandwich structures10.1016/j.compositesa.2006.06.006 ↗
13. Strategies for the replacement of chromic acid anodising for the structural bonding of aluminium alloys10.1016/j.ijadhadh.2005.07.001 ↗
14. Interfacial fracture toughness of polyester-based fiber-metal laminates with primary contact and secondary adhesive bonding10.1023/B:JMSC.0000021464.13845.79 ↗
15. Interfacial fracture of the fibre-metal laminates based on fibre reinforced thermoplastics10.1016/j.matdes.2014.03.058 ↗
16. A simple surface treatment and characterization of AA 6061 aluminum alloy surface for adhesive bonding applications10.1016/j.apsusc.2012.08.091 ↗
17. Improving the wettability of 2024 aluminium alloyby means of cold plasma10.1016/S0169-4332(03)00359-3 ↗
18. Effect of surface treatments on the durability of green polyurethane adhesive bonded aluminium alloy10.1016/j.ijadhadh.2014.07.007 ↗
19. Principles and practices of adhesive bonded structural joints and repairs10.1016/S0143-7496(98)00026-8 ↗
20. Effect of surface morphology on crack growth at a sol–gel reinforced epoxy/aluminum interface10.1080/00218460600713725 ↗
21. Effects of cure cycles on void content and mechanical properties of composite laminates10.1016/j.compstruct.2005.02.001 ↗
22. Effects of surface pre-treatment and void content on GLARE laminate process characteristics10.1016/j.jmatprotec.2010.01.017 ↗
23. Interface analysis of fiber metal laminates10.1080/15685543.2014.854527 ↗
24. Effect of Zn content on the chemical conversion treatments of AZ91D magnesium alloy10.1016/j.apsusc.2012.07.130 ↗
25. Effect of microstructure on the zinc phosphate conversion coatings on magnesium alloy AZ9110.1016/j.apsusc.2012.09.119 ↗
26. Influence of phytic acid concentration on coating properties obtained by MAO treatment on magnesium alloys10.1016/j.apsusc.2009.04.145 ↗
27. W.N. Shen Preparation and characterization of the micro-arc oxidation composite coatings on magnesium alloys10.1016/j.jma.2014.11.006 ↗
28. Research of growth mechanism of ceramic coatings fabricated by micro-arc oxidation on magnesium alloys at high current mode10.1016/j.jma.2015.07.003 ↗
29. Effect of electrodeposition modes on surface characteristics and corrosion properties of fluorine-doped hydroxyapatite coatings on Mg–Zn–Ca alloy10.1016/j.apsusc.2010.12.073 ↗
30. Corrosion behaviors and effects of corrosion products of plasma electrolytic oxidation coated AZ31 magnesium alloy under the salt spray corrosion test10.1016/j.apsusc.2016.04.011 ↗
31. Preparation and characterization of mesoporous 45S5 bioactive glass-ceramic coatings on magnesium alloy for corrosion protection10.1016/j.jallcom.2013.05.103 ↗
32. Influence of chloride ion concentration on immersion corrosion behaviour of plasma sprayed alumina coatings on AZ31 B magnesium alloy10.1016/j.jma.2014.11.001 ↗
33. Crack self-healing of phytic acid conversion coating on AZ31 magnesium alloy by heat treatment and the corrosion resistance10.1016/j.apsusc.2014.06.104 ↗
34. Effect of cerium additive on aluminum-based chemical conversion coating on AZ91D magnesium alloy10.1016/j.apsusc.2013.05.012 ↗
35. Research on surface treatment of magnesium alloy and its wettability with epoxy resin10.1080/02670836.2015.1104020 ↗
36. A Wilhelmy technique for the rapidassessment of solid wetting dynamics10.1021/la00020a057 ↗
37. Surface free energy evaluation of well-ordered Langmuir-Blodgett surfaces comparison of different approaches10.1016/j.colsurfa.2005.10.025 ↗
38. Failure analysis of bonded T-peel joints: efficient modelling by standard finite elements with experimental validation10.1016/j.ijadhadh.2009.10.004 ↗