The effect of incorporated self-lubricated BN(h) particles on the tribological properties of Ni–P/BN(h) composite coatings
Source abstract
Abstract
Abstract Ni–P/BN(h) composite coatings are prepared by means of the conventional electroless plating from the bath containing up to 10.0 g/l of hexagonal boron nitride particles with size 0.5 μm. The Ni–P coating is also prepared as a comparison. Cationic surfactant cetyltrimethylammonium bromide (CTAB) is used to stabilize the electrolyte, and the optimum CTAB concentration resulting in a nonagglomerated dispersion of particles is obtained using a dispersion stability analyzer. Morphology of the coatings and the effect of incorporated particles on coating structure and composition are investigated via scanning electron microscopy, field emission electron probe micro-analyzer and X-ray diffraction analysis. Hardness, roughness, friction coefficient and wear resistance of the coatings are also evaluated using Vickers microhardness tester, atomic force microscopy and ball-on disk machine. The presence of CTAB in the depositing bath has a positive effect on the surface roughness and performance of Ni–P/BN(h) composite coatings. The friction and wear tests results show that incorporation of 14.5 vol% BN(h) particles into the Ni–P coating lowers the coating friction coefficient by about 75% and the wear resistance of the Ni–P composites is approximately 10 times higher than Ni–P coating.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Electrodeposition and Electroless Coatings · Metal and Thin Film Mechanics · Corrosion Behavior and Inhibition
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (35)
Show source-provided references
1. Electroless Ni–P plating on AZ91D magnesium alloy from a sulfate solution10.1016/j.jallcom.2004.07.083 ↗
2. Cavitation erosion behavior of electroless nickel-plating on AISI 1045 steel10.1016/j.wear.2005.02.099 ↗
3. The tribological characteristics of electroless NiP coatings10.1016/S0043-1648(01)00539-7 ↗
4. Tribology of electroless nickel coatings – A review10.1016/j.matdes.2010.11.013 ↗
5. The effect of microstructure on the corrosion behaviour of electroless Ni-P alloys in acidic media10.1016/0257-8972(95)02446-8 ↗
6. Properties of hard Ni–P–Al2O3 and Ni–P–SiC coatings on Al-based casting alloys10.1080/10426910902809784 ↗
7. Dry sliding wear and friction behavior of Ni–P–ZrO2-Al2O3 composite electroless coatings on aluminum10.1081/AMP-120016088 ↗
8. Wear behavior of Ni–P and Ni–P–Al2O3 electroless coatings10.1016/j.wear.2006.10.013 ↗
9. Electroless ternary Ni–W–P alloys containing micron size Al2O3 particles10.1016/j.surfcoat.2010.07.047 ↗
10. Wear behavior of electroless Ni–P–B4C composite coatings10.1016/j.wear.2005.01.020 ↗
11. Synthesis and tribological behavior of electroless Ni–P–WC nanocomposite coatings10.1016/j.surfcoat.2007.01.035 ↗
12. Effect of wear conditions on tribological properties of electrolessly-deposited Ni-P-Gr-SiC hybrid composite coating10.1016/S1003-6326(11)61504-5 ↗
13. Preparation and properties of electroless Ni–P–SiO2 composite coatings10.1016/j.apsusc.2009.03.039 ↗
14. A study on friction and wear properties of PTFE coatings under vacuum conditions10.1016/j.wear.2010.04.014 ↗
15. Investigation in electroless Ni–P–Cg(graphite)–SiC composite coating10.1016/j.surfcoat.2005.11.140 ↗
16. Synthesis and tribological behaviour of electroless Ni–P-WS2 composite coatings10.1016/j.apsusc.2012.09.051 ↗
17. Tribological characteristics of electroless Ni–P–MoS2 composite coatings at elevated temperatures10.1016/j.apsusc.2012.10.055 ↗
18. The effect of carbon nanotubes on the corrosion and tribological behavior of electroless Ni–P–CNT composite coating10.1016/j.apsusc.2011.10.067 ↗
19. Deposition of Ni–P–BN(h) composite autocatalytic coatings10.1016/S0257-8972(98)00595-7 ↗
20. Influence of the heat treatment on the tribological behavior of a Ni–P–BN(h) autocatalytic composite coating10.1016/S0257-8972(99)00438-7 ↗
21. High temperature wear of an electroless Ni–P–BN (h) composite coating10.1016/S0257-8972(02)00663-1 ↗
22. Wear mechanism of Ni–P–BN(h) composite autocatalytic coatings10.1016/j.surfcoat.2005.08.061 ↗
23. Boron nitride (BN) and BN composites for high-temperature applications10.1016/j.jeurceramsoc.2007.09.005 ↗
24. Effect of surfactants on codeposition of PTFE particles with electroless Ni-P coating10.1016/S0254-0584(01)00513-2 ↗
25. Effect of surfactants addition on the suspension of PTFE particles in electroless plating solutions10.1080/00202967.1995.11871048 ↗
26. The effect of SiC particles added in electroless Ni–P plating solution on the properties of composite coatings10.1016/j.surfcoat.2007.10.015 ↗
27. Dispersion stability and particle characterization by sedimentation kinetics in a centrifugal field10.1081/DIS-120015373 ↗
28. Electroless Ni-P composite coating10.1023/A:1025572410205 ↗
29. Influence of particle size on the microstructure, hardness and corrosion resistance of electroless Ni–P–Al2O3 composite coatings10.1016/j.surfcoat.2005.03.007 ↗
30. Improved microhardness and wear resistance of the as-deposited electroless Ni–P coating10.1016/j.surfcoat.2008.06.180 ↗
31. Hardness evolution of electroless nickel–phosphorus deposits with thermal processing10.1016/S0257-8972(03)00209-3 ↗
32. The effect of heat treatment on the structure and abrasive wear resistance of autocatalytic NiP and NiP–SiC coatings10.1016/S0257-8972(01)01492-X ↗
33. Autocatalytic nickel coatings on aluminium with improved abrasive wear resistance10.1016/S0257-8972(00)00864-1 ↗
34. Budevski · 1996
35. Preparation and investigation of nanostructured SiC –nickel layers by electrodeposition10.1016/S0167-2738(02)00586-6 ↗