Solder wetting behavior enhancement via laser-textured surface microcosmic topography
Source abstract
Abstract
Abstract In order to reduce or even replace the use of Sn-Pb solder in electronics industry, the laser-textured surface microstructures were used to enhance the wetting behavior of lead free solder during soldering. According to wetting theory and Sn-Ag-Cu lead free solder performance, we calculated and designed four microcosmic structures with the similar shape and different sizes to control the wetting behavior of lead free solder. The micro-structured surfaces with different dimensions were processed on copper plates by fiber femtosecond laser, and the effect of microstructures on wetting behavior was verified experimentally. The results showed that the wetting angle of Sn-Ag-Cu solder on the copper plate with microstructures decreased effectively compared with that on the smooth copper plate. The wetting angles had a sound fit with the theoretical values calculated by wetting model. The novel method provided a feasible route for adjusting the wetting behavior of solders and optimizing solders system.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Adhesion, Friction, and Surface Interactions · Surface Roughness and Optical Measurements · Fluid Dynamics and Thin Films
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (39)
Show source-provided references
1. Spalling of Cu6Sn5 spheroids in the soldering reaction of eutectic SnPb on Cr/Cu/Au thin films10.1063/1.363728 ↗
2. Magnetic nanoparticle-based solder composites for electronic packing application10.1016/j.pmatsci.2014.08.001 ↗
3. Diode laser soldering using a lead-free filler material for electronic packaging structures10.1016/j.apsusc.2005.07.095 ↗
4. Lead free solders in microelectronics10.1016/S0927-796X(00)00010-3 ↗
5. Solidification of Sn-Pb alloy: experiments on the influence of the initial concentration10.1016/j.ijthermalsci.2015.01.007 ↗
6. Effect of volume in interfacial reaction between eutectic Sn–Pb solder and Cu metallization in microelectronic packaging10.1016/j.mseb.2003.09.003 ↗
7. Effect of stress and strain state on heterogeneous coarsening in Sn–Pb solder10.1016/j.actamat.2005.08.042 ↗
8. Pb-free solder-alloy based on Sn–Zn–Bi with the addition of germanium10.1016/j.jallcom.2010.03.094 ↗
9. Effect of indium on the mechanical properties of ternary Sn-In-Ag solders10.1007/s11661-003-0337-0 ↗
10. A microstructure study of the thermal fatigue failure of 60Sn-Pb solder joints10.1007/BF02652148 ↗
11. Lead (PB)-free solders for electronic packaging10.1007/BF02651362 ↗
12. Fatigue crack growth behavior in Sn–Pb eutectic solder/copper joint under mode I loading10.1016/j.mechmat.2005.02.002 ↗
13. Electromigration in Sn–Ag solder thin films under high current density10.1016/j.tsf.2014.06.030 ↗
14. A quantitative evaluation of time-independent and time-dependent deformations of lead-free and lead-containing solder alloys10.1007/s11664-006-0195-9 ↗
15. Creep deformation characteristics of tin and tin-based electronic solder alloys10.1007/s11661-005-0142-z ↗
16. Oxidation kinetics of thin copper films and wetting behaviour of copper and Organic Solderability Preservatives (OSP) with lead-free solder10.1016/j.apsusc.2011.02.048 ↗
17. Microstructures and properties of new Sn–Ag–Cu lead-free solder reinforced with Ni-coated graphene nanosheets10.1016/j.jallcom.2015.09.178 ↗
18. Contact angle of 63Sn–37Pb and Pb-free solder on Cu plating10.1016/S0169-4332(03)00342-8 ↗
19. Wetting characteristics of Cu–xZn layers for Sn–3.0Ag–0.5Cu solders10.1016/j.jallcom.2013.03.083 ↗
20. Wettability in reactive Sn-base alloy/Ni-base metallic glass systems10.1016/j.apsusc.2013.03.110 ↗
21. Wetting and interface phenomena in the molten Sn/CuFeNiCoCr high-entropy alloy system10.1016/j.apsusc.2015.08.090 ↗
22. Brazing of Si3N4 ceramic to copper10.1016/S0924-0136(97)00427-5 ↗
23. The effect of Ga content on the wetting reaction and interfacial morphology formed between Sn–8.55Zn–0.5Ag–0.1Al–xGa solders and Cu10.1016/j.scriptamat.2005.09.033 ↗
24. Spontaneous patterned superhydrophilic hybrid surfaces10.1016/j.matlet.2014.04.162 ↗
25. Superhydrophilic textured-surfaces on stainless steel substrates10.1016/j.tsf.2009.09.059 ↗
26. Hydrophilic control of laser micro-square-convexes SiC surfaces10.1016/j.matlet.2013.07.097 ↗
27. Purity of the sacred lotus, or escape from contamination in biological surfaces10.1007/s004250050096 ↗
28. A practical superhydrophilic self cleaning and antireflective surface for outdoor photovoltaic applications10.1016/j.solmat.2011.10.011 ↗
29. Anisotropic wetting characteristics versus roughness on machined surfaces of hydrophilic and hydrophobic materials10.1016/j.apsusc.2014.12.071 ↗
30. Influence of surface morphology and roughness on water wetting properties of low temperature nitrided austenitic stainless steels10.1016/j.matchar.2014.07.006 ↗
31. Prediction of roughness after ball burnishing of thermally coated surfaces10.1016/j.jmatprotec.2014.11.008 ↗
32. The effect of initial surface roughness on water droplet erosion behavior10.1016/j.wear.2015.08.019 ↗
33. Progressive evolution of silicon surface microstructures via femtosecond laser irradiation in ambient air10.1016/j.apsusc.2014.06.105 ↗
34. Femtosecond laser fabrication of highly hydrophobic stainless steel surface with hierarchical structures fabricated by combining ordered microstructures and LIPSS
35. Multifunctional surfaces produced by femtosecond laser pulses10.1063/1.4905616 ↗
36. Mechanism of surface modification using machine hammer peening technology10.1016/j.cirp.2012.03.139 ↗
37. How Wenzel and Cassie were wrong10.1021/la062634a ↗
38. Buoyant force and sinking conditions of a hydrophobic thin rod floating on water10.1103/PhysRevE.76.066103 ↗
39. Multiple equilibrium droplet shapes and design criterion for rough hydrophobic surfaces10.1021/la0268348 ↗