Effect of polishing process on corrosion behavior of 308L stainless steel in high temperature water

Cheng Ma, En-Hou Han, Qunjia Peng, Wei Ke

Publisher page

Abstract

Abstract Effect of change in surface composition and roughness by different polishing processes on corrosion of 308L stainless steel in high temperature water was investigated. The investigation was conducted by comparing the corrosion behavior of electropolished specimens with that of the 40 nm-colloidal silica slurry polished specimens. The result revealed that the electropolished specimens had a higher corrosion rate than the colloidal silica slurry polished specimens, which was attributed to formation of an amount of chromium hydroxide and higher roughness of the electropolished surface. Moreover, the ferrite in 308L stainless steel was found to have a higher resistance to corrosion than the austenite matrix.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · High-Temperature Coating Behaviors · Metal and Thin Film Mechanics

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (50)

Show source-provided references
1. Stress corrosion cracking of a low alloy steel to stainless steel transition weld in PWR primary waters at 292 degrees C10.1016/S0010-938X(99)00131-6 ↗
2. T. Lucas, R.G. Ballinger, H. Hänninen, T. Saukkonen, Effect of thermal aging on SCC, material properties and fracture toughness of stainless steel weld metals, in: 15th International Conference on Environmental Degradation of Materials in Nuclear Power Systems and Water Reactors, 2011, pp. 883–900.10.1007/978-3-319-48760-1_54 ↗
3. Environmentally assisted crack growth in 308L stainless steel weld metal in simulated primary water10.1016/j.corsci.2016.12.011 ↗
4. Corrosion behavior of 304 stainless steel in high temperature hydrogenated water10.1016/S0010-938X(02)00004-5 ↗
5. The mechanism of high temperature aqueous corrosion of stainless steels10.1016/0010-938X(91)90125-9 ↗
6. The effects of electropolishing (Ep) process parameters on corrosion resistance of 316L stainless steel10.1016/S0924-0136(03)00785-4 ↗
7. Influence of oxide films on primary water stress corrosion cracking initiation of alloy 60010.1016/j.jnucmat.2005.10.002 ↗
8. Sensitivity of stress corrosion cracking of stainless steel to surface machining and grinding procedure10.1016/j.corsci.2011.06.020 ↗
9. Microstructure and mechanical property of the fusion boundary region in an alloy 182-low alloy steel dissimilar weld joint10.1007/s10853-010-4581-6 ↗
10. Residual strain measurement and grain boundary characterization in the heat-affected zone of a weld joint between alloy 690TT and alloy 5210.1016/j.jnucmat.2009.12.016 ↗
11. Influence of dissolved oxygen on oxide films of alloy 690TT with different surface status in simulated primary water10.1016/j.corsci.2011.07.012 ↗
12. Short-time oxidation of alloy 690 in high-temperature and high-pressure steam and water10.1016/S1005-0302(12)60098-X ↗
13. Effect of electropolishing on corrosion of nuclear Grade 316L stainless steel in deaerated high temperature water10.1016/j.corsci.2016.09.002 ↗
14. Electropolishing effects on corrosion behavior of 304 stainless steel in high temperature hydrogenated water10.1016/j.corsci.2008.06.032 ↗
15. Effect of surface preparation on the corrosion of austenitic stainless steel 304L in high temperature steam and simulated PWR primary water10.1016/j.corsci.2011.12.007 ↗
16. Effect of surface state on the oxidation behavior of welded 308L in simulated nominal primary water of PWR10.1016/j.apsusc.2015.02.066 ↗
17. Microstructural changes in AISI 304L stainless steel due to surface machining: effect on its susceptibility to chloride stress corrosion cracking10.1016/j.jnucmat.2010.05.028 ↗
18. Effect of surface finishing on the oxidation behaviour of a ferritic stainless steel10.1016/j.apsusc.2017.03.280 ↗
19. Effect of surface preparation on intergranular stress corrosion cracking of alloy 600 in hydrogenated steam10.5006/1.3279916 ↗
20. Effect of electropolishing on corrosion of alloy 600 in high temperature water10.1016/j.corsci.2015.05.026 ↗
21. Chemical mechanical polishing of steel substrate using colloidal silica-based slurries10.1016/j.apsusc.2015.01.016 ↗
22. Impact of localized deformation on IASCC in austenitic stainless steels10.1016/j.jnucmat.2010.10.087 ↗
23. Low temperature thermal aging of austenitic stainless steel welds: kinetics and effects on mechanical properties10.1016/j.msea.2011.11.055 ↗
24. Influence of long-term low-temperature aging on the microhardness and corrosion properties of duplex stainless steel10.1016/j.corsci.2012.10.038 ↗
25. Low temperature embrittlement of duplex stainless steel: correlation between mechanical and electrochemical behavior10.1016/j.msea.2010.02.069 ↗
26. Microstructure characterization of the fusion zone of an alloy 600–82 weld joint10.1016/j.jmst.2015.08.013 ↗
27. High temperature oxidation behavior of Aisi 304L stainless steel—effect of surface working operations10.1016/j.apsusc.2012.10.018 ↗
28. Microstructural characteristics of the oxide scale formed on 304 stainless steel in oxygenated high temperature water10.1016/j.corsci.2010.07.015 ↗
29. Influence of dissolved oxygen concentration on the oxide film formed on 304 stainless steel in high temperature water10.1016/j.corsci.2012.06.007 ↗
30. Chemical composition and electronic structure of the oxide films formed on 316L stainless steel and nickel based alloys in high temperature aqueous environments10.1016/S0010-938X(00)00012-3 ↗
31. Mass transport effects during electropolishing of iron in phosphoric-sulfuric acid10.1016/0013-4686(92)87086-F ↗
32. Voltammetric and impedance studies of the electropolishing of type 316 stainless steel in a choline chloride based ionic liquid10.1016/j.electacta.2005.12.030 ↗
33. Electrochemical micromachining, polishing and surface structuring of metals: fundamental aspects and new developments10.1016/S0013-4686(03)00368-2 ↗
34. An electrochemical treatment to improve corrosion and contact resistance of stainless steel bipolar plates used in polymer electrolyte fuel cells10.1016/j.jpowsour.2013.07.041 ↗
35. Electrochemistry and surface chemistry of stainless steels in alkaline media simulating concrete pore solutions10.1016/j.electacta.2008.06.007 ↗
36. XPS and STM study of the growth and structure of passive films in high temperature water on a nickel-base alloy10.1016/j.electacta.2004.04.032 ↗
37. Effects of temperature on the protective property, structure and composition of the oxide film on alloy 62510.1016/j.corsci.2009.06.043 ↗
38. XPS study of Ni-base alloys oxide films formed in primary conditions of pressurized water reactor
39. Measurement methods for surface oxides on Sus 316L in simulated light water reactor coolant environments using synchrotron XRD and XRF10.1016/j.jnucmat.2012.10.049 ↗
40. Microstructural characterization of SCC crack tip and oxide film for Sus 316 stainless steel in simulated PWR primary water at 320°C10.1080/18811248.2005.9726383 ↗
41. The corrosion of alloy 690 in high-temperature aqueous media – thermodynamic considerations10.1016/S0022-3115(01)00468-8 ↗
42. The mechanism of high temperature aqueous corrosion of steel10.1016/0010-938X(89)90120-0 ↗
43. Nanoscale characterisation of grain boundary oxidation in cold-worked stainless steels10.1016/j.corsci.2012.06.030 ↗
44. Multi-scale characterization of stress corrosion cracking of cold-worked stainless steels and the influence of Cr content10.1016/j.actamat.2009.07.040 ↗
45. Stress corrosion cracking in the heat affected zone of a stainless steel 308L–316L weld joint in primary water10.1016/j.corsci.2016.02.030 ↗
46. Role of Δ-ferrite in stress corrosion cracking retardation near fusion boundary of 316NG welds10.1016/j.jnucmat.2012.02.006 ↗
47. D.J. Edwards, L.E. Thomas, K. Asano, S. Ooki, S.M. Bruemmer, Microstructure, microchemistry and stress corrosion crack characteristics in a BWR 316L SS core shroud weld, in: 15th International Conference on Environmental Degradation of Materials in Nuclear Power Systems and Water Reactors, 2007, in the CD–ROM.
48. Microstructural characteristics of the oxide films formed on alloy 690 TT in pure and primary water at 325 °C10.1016/j.corsci.2013.06.023 ↗
49. Early stage oxidation initiation at different grain boundaries of FCC Fe–Cr binary alloy: a computational chemistry study10.1007/s11085-013-9366-2 ↗
50. Oxidation behavior of grain boundary engineered alloy 690 in supercritical water environment10.1016/j.jnucmat.2011.12.022 ↗