journal article·2013-01

Significant effect of substrate temperature on the phase structure, optical and electrical properties of RF sputtered CIGS films

Zhou Yu, Yong Yan, Shasha Li, Yanxia Zhang, Chuanpeng Yan, Lian Liu, Yong Zhang, Yong Zhao

Publisher page

Abstract

Abstract This work studied the effect of substrate temperature on the phase structure, optical and electrical properties of the one-step radio frequency sputtered Cu(In,Ga)Se 2 (CIGS) thin films. X-ray diffraction (XRD) analysis revealed that all the deposited CIGS films are chalcopyrite phase with polycrystalline structure. The films deposited beyond the substrate temperature of 350 °C show (1 1 2) prefer orientation. Raman spectra reveal that the 150 °C deposited CIGS film coexists with Cu 2− x Se phase and the 500 °C deposited film contains ordered defect compound (ODC) phase. With the increase of substrate temperature, energy band gap of the CIGS film increase from 0.99 to 1.27 eV. Films deposited at higher temperature exhibit larger electrical conductivity. Conductivity of the CIGS films is dominated by “variable range hopping” mechanism. The disorder in our CIGS the films is associated with the formation of intrinsic defects such as V Se and In Cu for their low formation energy.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Chalcogenide Semiconductor Thin Films · Copper-based nanomaterials and applications · Quantum Dots Synthesis And Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (32)

Show source-provided references
1. Jackson · Prog. Photovolt. · 2011 · 19 · 89410.1002/pip.1078 ↗
2. Repins · Prog. Photovoltaics Res. Appl. · 2008 · 16 · 23510.1002/pip.822 ↗
3. Jackson · Prog. Photovoltaics Res. Appl. · 2007 · 15 · 50710.1002/pip.757 ↗
4. Dimmler · Thin Solid Films · 2007 · 515 · 597310.1016/j.tsf.2006.12.150 ↗
5. Kaelin · Sol. Energy · 2004 · 77 · 74910.1016/j.solener.2004.08.015 ↗
6. Chiba · 2010 · 164
7. Chen · Sol. Energy Mater. Sol. Cells · 2009 · 93 · 135110.1016/j.solmat.2009.02.014 ↗
8. Shi · Prog. Photovoltaics · 2011 · 19 · 16010.1002/pip.1001 ↗
9. Yu · Appl. Surf. Sci. · 2012 · 261 · 35310.1016/j.apsusc.2012.08.013 ↗
10. Yu · Appl. Surf. Sci. · 2012 · 258 · 852710.1016/j.apsusc.2012.05.034 ↗
11. Müller · Thin Solid Films · 2006 · 496 · 36410.1016/j.tsf.2005.09.077 ↗
12. Yu · Appl. Surf. Sci. · 2012 · 258 · 522210.1016/j.apsusc.2012.01.152 ↗
13. Rampino · Prog. Photovoltaics Res. Appl. · 2011
14. Tanino · Phys. Rev. B · 1992 · 45 · 1332310.1103/PhysRevB.45.13323 ↗
15. Ishii · J. Solid State Chem. · 1993 · 105 · 50410.1006/jssc.1993.1242 ↗
16. Rincón · Appl. Phys. Lett. · 1998 · 73 · 44110.1063/1.121893 ↗
17. Nomura · Jpn. J. Appl. Phys. · 1997 · 36 · L107510.1143/JJAP.36.L1075 ↗
18. Witte · Thin Solid Films · 2008 · 517 · 86710.1016/j.tsf.2008.07.011 ↗
19. Kohara · Jpn. J. Appl. Phys. · 1995 · 34 · L114110.1143/JJAP.34.L1141 ↗
20. Çolakoğlu · J. Non-Cryst. Solids · 2008 · 354 · 363010.1016/j.jnoncrysol.2008.03.014 ↗
21. Swanepoel · J. Phys. E Sci. Instrum. · 1983 · 16 · 121410.1088/0022-3735/16/12/023 ↗
22. Alonso · Phys. Rev. B · 2001 · 63 · 07520310.1103/PhysRevB.63.075203 ↗
23. Nasr · Thin Solid Films · 2006 · 515 · 175810.1016/j.tsf.2006.06.030 ↗
24. Parlak · Thin Solid Films · 1998 · 322 · 33410.1016/S0040-6090(97)00929-2 ↗
25. Abaab · Sol. Energy Mater. Sol. Cells · 1999 · 59 · 29910.1016/S0927-0248(99)00043-4 ↗
26. Zhang · Sol. Energy Mater. Sol. Cells · 2009 · 93 · 11410.1016/j.solmat.2008.09.002 ↗
27. Negami · Appl. Phys. Lett. · 1995 · 67 · 82510.1063/1.115456 ↗
28. Schmitt · Phys. Rev. B · 2000 · 61 · 1605210.1103/PhysRevB.61.16052 ↗
29. Amara · Catal. Today · 2006 · 113 · 25110.1016/j.cattod.2005.11.074 ↗
30. Gandotra · Phys. Status Solidi A · 1986 · 98 · 59510.1002/pssa.2210980233 ↗
31. Mott · Phil. Mag. · 1969 · 19 · 83510.1080/14786436908216338 ↗
32. Mesa · Thin Solid Films · 2010 · 518 · 176410.1016/j.tsf.2009.09.028 ↗