journal article·2017-05

Influence of Si wafer thinning processes on (sub)surface defects

Fumihiro Inoue, Anne Jourdain, Lan Peng, Alain Phommahaxay, Joeri De Vos, Kenneth June Rebibis, Andy Miller, Erik Sleeckx, Eric Beyne, Akira Uedono

Publisher page

Abstract

Abstract Wafer-to-wafer three-dimensional (3D) integration with minimal Si thickness can produce interacting multiple devices with significantly scaled vertical interconnections. Realizing such a thin 3D structure, however, depends critically on the surface and subsurface of the remaining backside Si after the thinning processes. The Si (sub)surface after mechanical grinding has already been characterized fruitfully for a range of few dozen of μm. Here, we expand the characterization of Si (sub)surface to 5 μm thickness after thinning process on dielectric bonded wafers. The subsurface defects and damage layer were investigated after grinding, chemical mechanical polishing (CMP), wet etching and plasma dry etching. The (sub)surface defects were characterized using transmission microscopy, atomic force microscopy, and positron annihilation spectroscopy. Although grinding provides the fastest removal rate of Si, the surface roughness was not compatible with subsequent processing. Furthermore, mechanical damage such as dislocations and amorphous Si cannot be reduced regardless of Si thickness and thin wafer handling systems. The CMP after grinding showed excellent performance to remove this grinding damage, even though the removal amount is 1 μm. For the case of Si thinning towards 5 μm using grinding and CMP, the (sub)surface is atomic scale of roughness without vacancy. For the case of grinding + dry etch, vacancy defects were detected in subsurface around 0.5–2 μm. The finished surface after wet etch remains in the nm scale in the strain region. By inserting a CMP step in between grinding and dry etch it is possible to significantly reduce not only the roughness, but also the remaining vacancies at the subsurface. The surface of grinding + CMP + dry etching gives an equivalent mono vacancy result as to that of grinding + CMP. This combination of thinning processes allows development of extremely thin 3D integration devices with minimal roughness and vacancy surface.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: 3D IC and TSV technologies · Semiconductor materials and devices · Silicon Nanostructures and Photoluminescence

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (25)

Show source-provided references
1. A wafer–scale 3–D circuit integration technology10.1109/TED.2006.882043 ↗
2. Thinned wafer multi-stack 3DI technology10.1016/j.mee.2009.07.006 ↗
3. Characterization of extreme Si thinning process for wafer-to-wafer stacking
4. Cu retardation performance of extrinsic gettering layers in thinned wafers evaluated by transient capacitance measurement10.1149/1.3597317 ↗
5. Grinding of silicon wafers: a review from historical perspectives10.1016/j.ijmachtools.2008.05.009 ↗
6. Effect of ultraprecision grinding on the microstructural change in silicon monocrystals10.1016/S0924-0136(98)00090-9 ↗
7. Grinding force and power modeling based on chip thickness analysis10.1007/s00170-006-0473-y ↗
8. Fine grinding of silicon wafers: machine configurations for spindle angle adjustments10.1016/j.ijmachtools.2004.06.013 ↗
9. Edge chipping of silicon wafers in diamond grinding10.1016/j.ijmachtools.2012.08.002 ↗
10. A process model of wafer thinning by diamond grinding10.1016/j.jmatprotec.2007.11.243 ↗
11. A study of the total thickness variation in the grinding of ultra-precision substrates10.1016/S0924-0136(01)01039-1 ↗
12. Process induced sub-surface damage in mechanically ground silicon wafers
13. Characterization methods for ultrathin wafer and die quality: a review10.1109/TCPMT.2014.2363570 ↗
14. Experimental investigation of surface/subsurface damage formation and material removal mechanisms in SiC grinding10.1016/j.ijmachtools.2007.10.013 ↗
15. Impact of back-grinding-induced damage on si wafer thinning for three-dimensional integration10.7567/JJAP.53.05GE04 ↗
16. Vacancy-type defects induced by grinding of Si wafers studied by monoenergetic positron beams10.1063/1.4896829 ↗
17. Behavior of copper contamination on backside damage for ultra-thin silicon three dimensional stacking structure10.1016/j.mee.2016.10.010 ↗
18. Feasibility of surface activated bonding for ultra-fine pitch interconnection – a new concept of bump-less direct bonding for system level packaging
19. Atomic diffusion bonding of wafers with thin nanocrystalline metal films10.1116/1.3437515 ↗
20. Permanent wafer bonding in the low temperature by using various plasma enhanced chemical vapour deposition dielectrics
21. Edge trimming for surface activated dielectric bonded wafers10.1016/j.mee.2016.10.014 ↗
22. Krause-Rehberg · 1999 · vol. 127
23. A raman study of etching silicon in aqueous tetramethylammonium hydroxide10.1149/1.1838911 ↗
24. Si etching in high-density SF6 plasmas for microfabrication: surface roughness formation10.1016/S0167-9317(04)00117-0 ↗
25. What is the Young’s modulus of silicon?10.1109/JMEMS.2009.2039697 ↗