Stress assisted selective ablation of ITO thin film by picosecond laser
Source abstract
Abstract
Abstract Fast selective pattering with high precession on 175 nm ITO thin film with IR ps lasers is investigated. Ablation parameters are optimized with detailed studies on the scribed depth, topography, and particle generation using AFM and SEM. A comparison of 10 and 150 ps laser revealed that the shorter pulse (10 ps) laser is more appropriate in selective and partial ablation; up to 20 nm resolution for controlled depth with multipulses having energy below the damage threshold is demonstrated. The experimental results are interpreted to involve stress assisted ablation mechanism for the 10 ps laser while thermal ablation along with intense melting occurs for 150 ps laser. The transition between these regimes is estimated to occur at approximately 30 ps.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Laser Material Processing Techniques · Laser-induced spectroscopy and plasma · Surface Roughness and Optical Measurements
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (19)
Show source-provided references
1. Thin films engineering of indium tin oxide: large area flat panel displays application10.1016/j.surfcoat.2005.08.144 ↗
2. Influence of indium tin oxide electrodes deposited at room temperature on the properties of organic light-emitting devices10.1063/1.2077835 ↗
3. Indium tin oxide and indium phosphide heterojunction nanowire array solar cells10.1063/1.4847355 ↗
4. Ultraviolet curing imprint lithography on flexible indium tin oxide substrates10.1116/1.2200375 ↗
5. Study of wet etching thin films of indium tin oxide in oxalic acid by monitoring the resistance10.1016/j.tsf.2014.07.027 ↗
6. Laser patterning with beam shaping on indium tin oxide thin films of glass/plastic substrate10.1016/j.tsf.2009.06.063 ↗
7. Rear-side picosecond laser ablation of indium tin oxide micro-grooves10.1016/j.optlaseng.2015.02.001 ↗
8. Femtosecond laser processing of indium-tin-oxide thin films10.1016/j.optlaseng.2015.01.011 ↗
9. Part 1: Wavelength dependent nanosecond laser patterning of very thin indium tin oxide films on glass substrates10.1016/j.optlaseng.2015.12.005 ↗
10. Excimer laser etching of transparent conducting oxides10.1063/1.105380 ↗
11. Laser lift-off initiated by direct induced ablation of different metal thin films with ultra-short laser pulses10.1088/0022-3727/45/31/315303 ↗
12. Ultrafast laser ablation of metal films on flexible substrates10.1007/s00339-013-7901-2 ↗
13. Ablation depth control with 40nm resolution on ITO thin films using a square, flat top beam shaped femtosecond NIR laser10.1016/j.optlaseng.2016.03.025 ↗
14. Mechanically inspired laser scribing of thin flexible glass10.1364/OL.40.004811 ↗
15. Simple technique for measurements of pulsed Gaussian-beam spot sizes10.1364/OL.7.000196 ↗
16. Laser-matter interaction in the bulk of a transparent solid: confined microexplosion and void formation10.1103/PhysRevB.73.214101 ↗
17. Part 2: Ultra-short pulse laser patterning of very thin indium tin oxide on glass substrates10.1016/j.optlaseng.2015.11.008 ↗
18. Photomechanical processes and effects in ablation10.1021/cr010436c ↗
19. Comparison of ablation mechanisms at low fluence for ultrashort and short-pulse laser exposure of very thin molybdenum films on glass10.1364/AO.55.002117 ↗