journal article·2010-08

Surface characterization of Pd/Ag23wt% membranes after different thermal treatments

A. Ramachandran, W.M. Tucho, A.L. Mejdell, M. Stange, H.J. Venvik, J.C. Walmsley, R. Holmestad, R. Bredesen, A. Borg

Applied Surface Science· Volume 256· Issue 20
Publisher page

Abstract

Abstract Hydrogen permeation measurements of 1.5–10 μm thick Pd/Ag23 wt% membranes before and after thermal treatments at 300 °C in air (both sides) or in the temperature range 300–450 °C in N 2 (feed side) and Ar (permeate side) were performed. Accompanying changes in surface topography and chemical composition were subsequently investigated by atomic force microscopy (AFM), X-ray photoelectron spectroscopy (XPS) and Auger electron spectroscopy (AES) depth profiling. For a 2 μm thick membrane, the surface roughness increased for all annealing temperatures applied, while a temperature of 450 °C was required for an increase in roughness of both membrane surfaces to occur for the 5 μm membrane. The thickest membrane, of 10 μm, showed changed surface roughness on one side of the membrane only and a slight decrease in hydrogen permeance after all heat treatments in N 2 /Ar. X-ray photoelectron spectroscopy investigations performed after treatment and subsequent permeation measurements revealed segregation of silver to the membrane surfaces for all annealing temperatures applied. In comparison, heat treatment at 300 °C in air resulted in significantly increased hydrogen permeance accompanied by increasing surface roughness. Upon exposure to oxygen, Pd segregates to the surface to form a 2–3 nm thick oxide layer (PdO), with more complex segregation behavior after subsequent reduction and permeance measurements in pure hydrogen. The available permeance data for the Pd/Ag23 wt% membranes after heat treatment in air at 300 °C is found to depend linearly on the inverse membrane thickness, implying bulk limited hydrogen permeation for thicknesses down to 1.5–2.0 μm.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Catalytic Processes in Materials Science · Electrocatalysts for Energy Conversion · Nanoporous metals and alloys

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (62)

Show source-provided references
1. Carbon dioxide zero-emission hydrogen system based on nuclear power10.1016/j.pnucene.2005.05.051 ↗
2. Carbon dioxide zero-emission hydrogen carrier system for fuel cell vehicle10.1205/cherd.04321 ↗
3. Carbon recycle nuclear hydrogen carrier system for transportation field10.1016/j.pnucene.2007.11.024 ↗
4. Biomass to hydrogen via fast pyrolysis and catalytic steam reforming of the pyrolysis oil or its fractions10.1021/ie960396g ↗
5. Catalytic steam reforming of bio-oils for the production of hydrogen: effects of catalyst composition10.1016/S0926-860X(00)00440-3 ↗
6. Gasification technologies: the path to clean, affordable energy in the 21st century10.1016/S0378-3820(01)00138-2 ↗
7. The purification of hydrogen: a review of the technology emphasizing the current status of palladium membrane diffusion10.1595/003214083X274157169 ↗
8. Pressure-composition and electrical resistance-composition isotherms of palladium-deutrium system10.1016/S0360-3199(97)00149-3 ↗
9. Hydrogen permeable palladium–silver alloy membrane supported on porous ceramics10.1016/S0376-7388(00)83041-0 ↗
10. Pd-Ag alloy films prepared by metallorganic chemical vapor deposition process10.1016/S0040-6090(00)01345-6 ↗
11. Hydrogen permeability of 2.5μm palladium–silver membranes deposited on ceramic supports10.1016/j.memsci.2008.08.020 ↗
12. Preparation of palladium–silver alloy membranes for hydrogen separation by the spray pyrolysis method10.1016/0376-7388(93)80004-H ↗
13. Characterizations of Pd–Ag membrane prepared by sequential electroless deposition10.1016/j.surfcoat.2004.07.089 ↗
14. R. Bredesen, H. Klette, Method of Manufacturing Thin Metal Membranes, US Patent No. 6086729A (2000).
15. Experimental investigation of a microchannel membrane configuration with a 1.4μm Pd/Ag23wt.% membrane—effects of flow and pressure10.1016/j.memsci.2008.11.028 ↗
16. Thin Pd-23%Ag/stainless steel composite membranes: long-term stability, life-time estimation and post-process characterisation10.1016/j.memsci.2008.10.053 ↗
17. Performance and application of thin Pd-alloy hydrogen separation membranes in different configurations10.1016/j.jtice.2008.12.013 ↗
18. Model of hydrogen permeation behavior in palladium membranes10.1016/S0376-7388(98)00256-7 ↗
19. Modelling and simulation of hydrogen permeation through supported Pd-alloy membranes with a multicomponent approach10.1016/j.ces.2008.01.009 ↗
20. Lewis · 1967
21. Diffusion of Hydrogen through Palladium10.1063/1.1701003 ↗
22. Methanol as an energy source and/or energy carrier in membrane processes10.1080/15422110601166049 ↗
23. Developing a heating procedure to optimise hydrogen permeance through Pd–Ag membranes of thickness less than 2.2μm10.1016/S0376-7388(01)00562-2 ↗
24. H2/N2 gaseous mixture separation in dense Pd/α-Al2O3 hollow fiber membranes: experimental and simulation studies10.1016/j.seppur.2006.04.007 ↗
25. High pressure performance of thin Pd–23%Ag/stainless steel composite membranes in water gas shift gas mixtures; influence of dilution, mass transfer and surface effects on the hydrogen flux10.1016/j.memsci.2007.08.056 ↗
26. Methanol-induced hydrogen permeation through a palladium membrane10.1016/S0039-6028(99)00892-4 ↗
27. The effect of CO and O2 on hydrogen permeation through a palladium membrane10.1016/S0169-4332(99)00357-8 ↗
28. Alcohol dehydrogenation over Pd versus PdAg membranes10.1016/S0926-860X(01)00591-9 ↗
29. Surface reaction of hydrogen on a palladium alloy membrane under co-existence of H2O, CO, CO2 or CH410.1016/j.ijhydene.2007.04.030 ↗
30. Studies of self-supported 1.6μm Pd/23wt.%Ag membranes during and after hydrogen production in a catalytic membrane reactor10.1016/j.cattod.2006.01.041 ↗
31. Effects of co-existing hydrocarbons on hydrogen permeation through a palladium membrane10.1016/S0376-7388(99)00357-9 ↗
32. The effect of carbon monoxide and steam on the hydrogen permeability of a Pd/stainless steel membrane10.1016/S0376-7388(99)00223-9 ↗
33. Influence of steam and carbon dioxide on the hydrogen flux through thin Pd/Ag and Pd membranes10.1016/j.memsci.2005.12.002 ↗
34. H2 for PEM-FC: effect of CO in the purification by means of Pd-based membranes10.1016/j.desal.2006.03.310 ↗
35. A novel model equation for the permeation of hydrogen in mixture with carbon monoxide through Pd–Ag membranes10.1016/j.seppur.2007.10.010 ↗
36. Effects of CO and CO2 on hydrogen permeation through a ∼3μm Pd/Ag 23wt.% membrane employed in a microchannel membrane reactor configuration10.1016/j.seppur.2009.04.025 ↗
37. Effect of hydrogen-sulfide on the hydrogen permeance of palladium–copper alloys at elevated temperatures10.1016/j.memsci.2004.04.033 ↗
38. Pd and Pd-Cu membranes: inhibition of H2 permeation by H2S10.1016/j.memsci.2004.11.031 ↗
39. Hydrogen permeance and surface states of Pd–Ag/ceramic composite membranes10.1002/aic.10892 ↗
40. Hydrogen permeation through surface modified Pd and PdAg membranes10.1016/S0376-7388(01)00414-8 ↗
41. Hydrogen permeation of thin, free-standing Pd/Ag23% membranes before and after heat treatment in air10.1016/j.memsci.2007.09.024 ↗
42. Changes in hydrogen permeability and surface state of Pd–Ag/ceramic composite membranes after thermal treatment10.1016/j.memsci.2004.12.006 ↗
43. The effect of air exposure on palladium-copper composite membranes10.1016/j.apsusc.2004.06.023 ↗
44. Surface segregation of Pd–Ag membranes upon hydrogen permeation10.1016/0039-6028(93)91484-7 ↗
45. Reversed surface segregation in palladium–silver alloys due to hydrogen adsorption10.1016/j.susc.2008.07.016 ↗
46. Microstructural studies of self-supported (1.5–10μm) Pd/23wt%Ag membranes tested for hydrogen separation10.1007/s10853-009-3671-9 ↗
47. Effects of thermal activation on hydrogen permeation properties of thin, self-supported Pd/Ag membranes10.1016/j.seppur.2009.06.015 ↗
48. Hydrogen purification with palladium and palladium alloys on porous stainless steel membranes10.1504/IJOGCT.2008.016734 ↗
49. Many-electron singularity in X-ray photoemission and X-ray line spectra from metals10.1088/0022-3719/3/2/010 ↗
50. Porter · 1991
51. Spontaneous ordering of oxide nanostructures10.1126/science.287.5461.2235 ↗
52. de Boer · 1988
53. STM study of the (111) and (100) surfaces of PdAg10.1016/S0039-6028(98)00673-6 ↗
54. Use of matrix corrections in the calculation of surface composition of AgPd alloys in Auger electron spectroscopy10.1002/sia.740230606 ↗
55. Hultgren · 1973
56. Segregation at the PdAg(111) surface: electronic structure calculations10.1103/PhysRevB.71.045411 ↗
57. The chemical potential in surface segregation calculations: AgPd alloys10.1016/j.susc.2005.12.023 ↗
58. Hydrogen desorption versus electronic structure studied on Ag-covered Pd with photoemission and a hydrogen-sensitive metal-oxide semiconductor structure10.1103/PhysRevB.30.3055 ↗
59. A comparative study of the behaviour of the PdAg(111) and Pd(111) surfaces towards the interaction with hydrogen and carbon monoxide10.1016/0039-6028(86)90814-9 ↗
60. Mulder · 1997
61. Insights into the relation between crystal structure and deuterium desorption characteristics of Pd–Au–D-alloys10.1016/j.actamat.2008.08.045 ↗
62. Inelastic neutron scattering study of the ordered Pd–Ag–H hydrides10.1088/0953-8984/5/38/004 ↗