Effect of microstructure and phase constitution on mechanical properties of Ti1−xAlxN coatings
Source abstract
Abstract
Abstract Monolithic Ti Al N coatings with varying Al content in the range 0–65 at.% were deposited by cathodic arc evaporation. The variation in mechanical properties was studied by nanoindentation and scratch testing, and correlated with the phase constitution, grain size and residual stress. The hardness was found to be nearly stable up to Al content of 53% followed by a large drop at 65%. Depending on the stoichiometry, phase constitution and microstructure of the Ti 1− x Al x N coatings, the mechanical property measurements were observed to reveal distinct trends at particular Al contents-ranging from a large scatter to clustering of data around specific values. Focused Ion Beam milling and Transmission Electron Microscopy studies showed a gradual change in microstructure, from large columnar grains in TiN to finer columns at intermediate Al content and near equiaxed, ultrafine grains with a nanocomposite structure in case of Ti 0.35 Al 0.65 N. Scratch studies revealed the deformation modes to vary with Al content, with the ductile failure modes at low Al content giving way to brittle failure at the highest Al content. Toughness studies showed a gradual increase in toughness with Al%, with the maximum seen at 53% and a moderate drop seen at 65%. The toughness shows a close dependence on the mechanical properties, phase constitution and microstructure. The study outlines the role of Al content on the microstructure of PVD TiAlN coatings and highlights the advantage of a cubic, nanocomposite structure for enhancing the toughness of these coatings.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Metal and Thin Film Mechanics · MXene and MAX Phase Materials · Boron and Carbon Nanomaterials Research
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (54)
Show source-provided references
1. TiN coating of tool steels: a review10.1016/0924-0136(93)90016-Y ↗
2. Industrial applications of CrN (PVD) coatings deposited at high and low temperatures10.1016/S0257-8972(97)00393-9 ↗
3. Single layer and multilayer wear resistant coatings of (Ti,Al)N: a review10.1016/S0921-5093(02)00259-9 ↗
4. Multicomponent and multiphase hard coatings for tribological applications10.1016/S0257-8972(00)00783-0 ↗
5. Anti-oxidation properties of TiAlN film prepared by plasma-assisted chemical vapor deposition and roles of Al10.1016/S0040-6090(97)00212-5 ↗
6. The development of the PVD coating TiAlN as a commercial coating for cutting tools10.1016/0257-8972(91)90142-J ↗
7. Concepts for the design of advanced nanoscale PVD multilayer protective thin films10.1016/j.jallcom.2008.08.133 ↗
8. Characterization of multilayer nitride coatings by electron microscopy and modulus mapping10.1016/j.matchar.2013.04.003 ↗
9. Microstructural design of hard coatings10.1016/j.pmatsci.2006.02.002 ↗
10. Modern coatings in high performance cutting applications10.1016/j.ijrmhm.2005.11.005 ↗
11. Performance of PVD TiN, TiCN, and TiAlN coated cemented carbide tools in turning10.1016/S0263-4368(99)00008-6 ↗
12. Self-organized nanostructures in the TiAlN system10.1063/1.1608464 ↗
13. Decomposition pathways in age hardening of TiAlN films10.1063/1.3610451 ↗
14. Industrial applications of superhard nanocomposite coatings10.1016/j.surfcoat.2008.05.038 ↗
15. Effects of Al content on hardness, lattice parameter and microstructure of Ti1−xAlxN films10.1016/S0257-8972(99)00491-0 ↗
16. Abrasive wear resistance of Ti1−xAlxN hard coatings deposited by a vacuum arc system with lateral rotating cathodes10.1016/j.surfcoat.2008.08.019 ↗
17. Effect of the aluminium content and the bias voltage on the microstructure formation in Ti1−xAlxN protective coatings grown by cathodic arc evaporation10.1016/j.surfcoat.2010.07.057 ↗
18. Mechanical properties and machining performance of Ti1−xAlxN-coated cutting tools10.1016/j.surfcoat.2004.04.056 ↗
19. Influence of the Al distribution on the structure, elastic properties, and phase stability of supersaturated Ti1−xAlxN10.1063/1.2360778 ↗
20. Characterisation of nano-structured titanium and aluminium nitride coatings by indentation, transmission electron microscopy and electron energy loss spectroscopy10.1016/j.tsf.2011.04.113 ↗
21. Superhard nanocomposite Ti1−xAlxN films prepared by magnetron sputtering10.1016/S0040-6090(00)00653-2 ↗
22. Structure, mechanical and tribological properties of sputtered Ti1−xAlxN coatings with 0.5≤x≤0.7510.1016/j.surfcoat.2004.12.008 ↗
23. Structure, hardness and thermal stability of TiAlN and nanolayered TiAlN/CrN multilayer films10.1016/j.vacuum.2004.08.020 ↗
24. Effect of mechanical properties measured at room and elevated temperatures on the wear resistance of cutting tools with TiAlN and AlCrN coatings10.1016/j.surfcoat.2005.08.132 ↗
25. In situ small-angle X-ray scattering study of nanostructure evolution during decomposition of arc evaporated TiAlN coatings10.1063/1.3078283 ↗
26. Structural and optical properties of titanium aluminum nitride films (Ti1−xAlxN)10.1116/1.1359532 ↗
27. Functional multi-layer nitride coatings for high temperature solar selective applications10.1016/j.solmat.2013.10.024 ↗
28. Optical properties and thermal stability of TiAlN/AlON tandem absorber prepared by reactive DC/RF magnetron sputtering10.1016/j.solmat.2008.06.004 ↗
29. Significance of Al on the morphological and optical properties of Ti1−xAlxN thin films10.1016/j.matchemphys.2011.07.083 ↗
30. Wear mechanisms of titanium and aluminium nitride coatings: a microtribological approach10.1016/j.surfcoat.2013.02.033 ↗
31. The role of structural properties on damage behaviour of titanium and aluminium nitride coatings: an EXAFS and TEM study10.1016/j.surfcoat.2009.10.029 ↗
32. Toughness enhancement in TiAlN-based quarternary alloys10.1016/j.tsf.2012.01.030 ↗
33. Improved technique for determining hardness and elastic modulus using load and displacement sensing indentation experiments10.1557/JMR.1992.1564 ↗
34. X-ray diffraction residual stress techniques
35. 2010
36. Klug · 1974
37. Structural effects of energy input during growth of Ti1–xAlxN (0.55≤x≤0.66) coatings by cathodic arc evaporation10.1016/j.surfcoat.2013.12.018 ↗
38. 2010
39. Indentation fracture toughness and acoustic energy release in tetrahedral amorphous carbon diamond-like thin films10.1016/j.actamat.2006.05.003 ↗
40. Relating hardness-curve shapes with deformation mechanisms in TiAlN thin films enduring indentation10.1016/j.msea.2005.06.010 ↗
41. ASTM Standard C1624-05, 2010, “Standard Test Method for Adhesion Strength and Mechanical Failure Modes of Ceramic Coatings by Quantitative Single Point Scratch Testing,” ASTM International, West Conshohocken, PA, 2010, DOI: 10.1520/C1624-05R10, http://www.astm.org/.10.1520/C1624-05R10 ↗
42. Failure mode maps in the thin film scratch adhesion test10.1016/S0301-679X(97)00012-1 ↗
43. Microstructural response of TiN monolithic and multilayer coatings during microscratch testing10.1557/jmr.2007.0292 ↗
44. Nanocomposite hard coatings: deposition issues and validation of their mechanical properties10.1002/adem.200500045 ↗
45. Structure and properties of TiN coatings10.1016/0040-6090(85)90333-5 ↗
46. Analysis of hardness of nanocrystalline coatings of aluminum-rich Ti1−xAlxN10.1007/s12034-012-0354-y ↗
47. Crystal growth and microstructure of polycrystalline Ti1−xAlxN alloy films deposited by ultra-high-vacuum dual-target magnetron sputtering10.1016/0040-6090(93)90244-J ↗
48. The effect of aluminum on the microstructure and mechanical properties of arc-evaporated Ti1−xAlxN coatings deposited on cemented carbide substrates
49. Nano-indentation hardness and elastic moduli of bulk single-crystal AlN10.1143/JJAP.41.4620 ↗
50. Nanocomposite oxide and nitride hard coatings produced by pulse magnetron sputtering10.1016/j.surfcoat.2005.02.120 ↗
51. Studies on phase dependent mechanical properties of dc magnetron sputtered TaN thin films: evaluation of super hardness in orthorhombic Ta4N phase10.1088/0022-3727/41/4/045409 ↗
52. Effect of aluminum concentration on friction and wear properties of titanium aluminum nitride films10.1016/S0257-8972(03)00936-8 ↗
53. Ab initio calculated binodal and spinodal of cubic Ti1−xAlxN10.1063/1.2177630 ↗
54. The grain refining effect of energy competition and the amorphous phase in nanocomposite materials10.1016/j.scriptamat.2013.07.023 ↗