High-temperature oxidation of advanced FeCrNi alloy in steam environments
Source abstract
Abstract
Abstract Alloys of iron-chromium-nickel are being explored as alternative cladding materials to improve safety margins under severe accident conditions. Our research focuses on non-destructively investigating the oxidation behavior of the FeCrNi alloy “Alloy 33” using synchrotron-based methods. The evolution and structure of oxide layer formed in steam environments were characterized using X-ray diffraction, hard X-ray photoelectron spectroscopy, X-ray fluorescence methods and scanning electron microscopy. Our results demonstrate that a compact and continuous oxide scale was formed consisting of two layers, chromium oxide and spinel phase (FeCr2O4) oxides, wherein the concentration of the FeCr2O4 phase decreased from the surface to the bulk-oxide interface.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Nuclear Materials and Properties · High-Temperature Coating Behaviors · Fusion materials and technologies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (41)
Show source-provided references
1. Advanced oxidation-resistant iron-based alloys for LWR fuel cladding10.1016/j.jnucmat.2013.06.041 ↗
2. Sample environment for in situ synchrotron corrosion studies of materials in extreme environments10.1063/1.4964101 ↗
3. Protection of zirconium by alumina- and chromia-forming iron alloys under high-temperature steam exposure10.1016/j.jnucmat.2013.03.006 ↗
4. High temperature oxidation of fuel cladding candidate materials in steam-hydrogen environments10.1016/j.jnucmat.2013.05.047 ↗
5. Oxidation of fuel cladding candidate materials in steam environments at high temperature and pressure10.1016/j.jnucmat.2012.05.007 ↗
6. Oxidation behavior of austenitic stainless steels as fuel cladding candidate materials for SCWR in superheated steam10.1016/j.nucengdes.2014.08.020 ↗
7. Scaling of austenitic stainless steels and nickel-based alloys in high-temperature steam at 973K10.5006/1.3585251 ↗
8. Progress in corrosion resistant materials for supercritical water reactors10.1016/j.corsci.2009.07.007 ↗
9. Lattice and grain boundary diffusion of chromium in superalloy Incoloy-80010.1016/0022-3115(94)90306-9 ↗
10. The effect of grain boundary engineering on the oxidation behavior of INCOLOY alloy 800H in supercritical water10.1016/j.jnucmat.2005.09.023 ↗
11. Analyses of oxide films grown on AISI 304L stainless steel and Incoloy 800HT exposed to supercritical water environment10.1016/j.jnucmat.2011.05.007 ↗
12. Short-time oxidation of alloy 690 in high-temperature and high-pressure steam and water10.1016/S1005-0302(12)60098-X ↗
13. Temperature effect in the corrosion resistance of Ni-Fe-Cr alloy in chloride medium10.1016/j.corsci.2008.06.030 ↗
14. Effects of solution temperature on localized corrosion of high nickel content stainless steels and nickel in chromated LiBr solution10.1016/j.corsci.2005.11.010 ↗
15. Pitting corrosion studies of super austenitic stainless steels in natural sea water using dynamic electrochemical impedance spectroscopy10.1007/s10800-006-9231-y ↗
16. Passivation and corrosion of the metallic high performance materials alloy 33 and MC-alloy in different environments10.1016/S0010-938X(02)00101-4 ↗
17. Galvanic studies of copper coupled to alloy 33 and titanium in lithium bromide solutions10.5006/1.3280797 ↗
18. Case reviews on the effect of microstructure on the corrosion behavior of austenitic alloys for processing and storage of nuclear waste10.1007/s11661-005-0201-5 ↗
19. Alloy selection for accident tolerant fuel cladding in commercial light water reactors
20. Corrosion behavior of an alumina forming austenitic steel exposed to supercritical carbon dioxide10.1016/j.corsci.2013.12.023 ↗
21. Effect of shot-peening on the oxidation of alloy 800H exposed to supercritical water and cyclic oxidation10.1016/j.corsci.2008.04.008 ↗
22. Corrosion behavior of alloy 800H (Fe-21Cr-32Ni) in supercritical water10.1016/j.corsci.2010.10.021 ↗
23. Birkholz · 2006
24. Hammersley · 1997
25. Elemental X-ray imaging using the Maia detector array: the benefits and challenges of large solid-angle10.1016/j.nima.2009.11.035 ↗
26. Khanna · 2002
27. Batchelor · 2011
28. Kinetics of high temperature oxidation and chromia volatilization for a binary Ni-Cr alloy10.1007/s11085-005-6562-8 ↗
29. Oxidation of FeCrAl alloy: influence of temperature and atmosphere on scale growth rate and mechanism10.1016/S0257-8972(00)00989-0 ↗
30. Calculations of parabolic rate constants for metal oxidation10.1007/BF00603388 ↗
31. Role of chlorides in hot corrosion of a cast Fe-Cr-Ni alloy. Part I: experimental studies10.1016/j.corsci.2004.04.013 ↗
32. Influence of the dissolved oxygen content on corrosion of the ferritic-martensitic steel P92 in supercritical water10.1016/j.corsci.2011.11.013 ↗
33. Continuous and cyclic oxidation of T91 ferritic steel under steam10.1016/S0010-938X(03)00173-2 ↗
34. Microstructural evaluation of oxide layers formed on Fe-22Cr-6Al metallic foam by pre-oxidization10.1016/j.apsusc.2013.12.144 ↗
35. 1.17 Oxidation in steam and steam/hydrogen environments10.1016/B978-044452787-5.00022-6 ↗
36. XPS and STM study of the growth and structure of passive films in high temperature water on a nickel-base alloy10.1016/j.electacta.2004.04.032 ↗
37. An oxidation study of Ni-Cr-Fe alloys in carbon dioxide at 800–1000°C10.1007/BF00550055 ↗
38. The oxidation of alloys10.1088/0034-4885/39/5/001 ↗
39. Corrosion behavior of Alloy 690 in aerated supercritical water10.1016/j.corsci.2012.10.001 ↗
40. Effects of exposure temperature and time on corrosion behavior of a ferritic-martensitic steel P92 in aerated supercritical water10.1016/j.corsci.2014.10.022 ↗
41. Steam oxidation of Fe-32% Ni-23% Cr alloys with manganese and carbon10.1149/1.2129781 ↗