journal article·2015-07

High-temperature crack-healing behaviour and strength recovery of (MoNb)Si2

Gaoming Zhu, Xiaohong Wang, Qiong Lu, Guangzhi Wu, Peizhong Feng

Publisher page

Abstract

Abstract (MoNb)Si2 materials were prepared using combustion synthesis and the vacuum hot-pressing technology. Cracks were introduced on the surface of polished materials using the Vickers indentation method. The crack-healing behaviour of (MoNb)Si2 materials were investigated with high-temperature oxidation in air. The results show that after annealing at 900 °C, 1200 °C and 1500 °C for 1 h, the crack-healing behaviour was observed in each case. The bending strength obviously decreased when the cracks were introduced, and the materials significantly recovered after the heat treatment. The crack-healed samples exhibited higher bending strengths than the original level after the 1200 °C treatment, e.g. 479 MPa versus 195 MPa of pure MoSi2. MoSi2 micro alloyed with niobium shows a high bending strength at room temperature and excellent crack-healing properties at high temperatures.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Intermetallics and Advanced Alloy Properties · MXene and MAX Phase Materials · Advanced ceramic materials synthesis

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (44)

Show source-provided references
1. Mechanical behaviour and oxidation resistance of structural silicides10.1179/174328006X79454 ↗
2. Molybdenum disilicide heating elements; meeting advanced ceramics requirements
3. Extrusion and selected engineering properties of Mo–Si–B intermetallics10.1016/S0966-9795(00)00080-7 ↗
4. Key developments in high temperature structural silicides10.1016/S0921-5093(98)01043-0 ↗
5. Oxidation behavior of in situ synthesized MoSi2–SiC composites at 500°C10.3724/SP.J.1037.2013.00527 ↗
6. Toughening MoSi2 with niobium metal-effects of morphology of ductile reinforcements10.1007/BF01178416 ↗
7. First-principles calculation of elastic properties of Nb and Al codoping MoSi2
8. Tailoring the microstructure of molybdenum disilicide matrix composites with Nb additions10.1016/S0955-2219(03)00221-8 ↗
9. Microalloying for ductility in molybdenum disilicide10.1016/S0921-5093(98)01060-0 ↗
10. Deformation mechanism of polycrystalline MoSi2 alloyed with 1 at.% Nb10.1016/S0921-5093(03)00307-1 ↗
11. Effects of Nb-alloying on high-temperature oxidation of MoSi210.12693/APhysPolA.125.563 ↗
12. Interfacial modification and impact properties of Nb/MoSi2 laminate composites by the addition of ZrO2, NbSi2, and SiC particles, Metall10.1007/s11661-000-0235-7 ↗
13. Microstructure and mechanical properties of MoSi2/Nb composites made by MA-pulse discharge sintering10.2320/matertrans1989.41.1268 ↗
14. Effect of alloying elements on anomalous strengthening of NbSi2-based silicides with C40 structure10.1016/S0921-5093(97)00566-2 ↗
15. Crack healing behavior of SiC whisker reinforced Si3N4 composite10.4028/www.scientific.net/MSF.750.15 ↗
16. Cracked-healing and the bending strength of Si3N4 composite ceramics with SiO2 additions
17. Preliminary study of the crack healing and strength recovery of Al2O3-matrix composites10.1111/j.1460-2695.2004.00725.x ↗
18. Crack-healing behavior of zirconium diboride composite reinforced with silicon carbide whiskers10.1016/j.scriptamat.2008.08.013 ↗
19. Crack healing of a MoSi2-based composite at high temperetures
20. Crack-healing and oxidation behavior of silicon nitride ceramics10.1016/S0955-2219(03)00645-9 ↗
21. Ghosh · 2009 · 183
22. The beneficial effect of water vapour on the oxidation at 600 and 700°C of a MoSi2-based composite10.1016/j.jeurceramsoc.2004.01.005 ↗
23. High temperature oxidation of MoSi210.1007/s10853-009-4012-8 ↗
24. Rapid solution hardening at elevated temperatures by substitutional Re alloying in MoSi210.1016/S1359-6454(99)00380-8 ↗
25. High temperature plastic anisotropy in MoSi2 single crystals10.1016/0956-7151(94)00260-O ↗
26. Multiple crack healing of a Ti2AlC ceramic10.1016/j.jeurceramsoc.2012.01.017 ↗
27. Crack healing in alumina bioceramics10.1016/j.dental.2007.06.001 ↗
28. Solid solution softening and hardening in alloyed MoSi210.1016/S0966-9795(97)00103-9 ↗
29. Study of the microstructure and oxidation of NbSi2 base alloys10.1557/PROC-364-1321 ↗
30. Oxidation properties of self-propagating high temperature synthesized niobium disilicide10.1016/j.corsci.2014.04.029 ↗
31. Crack-healing and mechanical behaviour of Al2O3/SiC composites at elevated temperature10.1111/j.1460-2695.2004.00785.x ↗
32. Microstructure of high-temperature oxidation layer of molybdenum disilicide
33. Sintering mechanisms of zirconium and hafnium carbides doped with MoSi210.1111/j.1551-2916.2009.03049.x ↗
34. Investigation of MoSi2 melt infiltrated RSiC and its oxidation behavior10.1016/j.ceramint.2011.04.138 ↗
35. Oxidation behaviour of a (Mo,W)Si2-based composite in dry and wet oxygen atmospheres in the temperature range 350–950°C10.1016/j.jeurceramsoc.2008.12.009 ↗
36. Oxidation behavior of hot-pressed MoSi2-TiC composite10.1023/A:1004851823360 ↗
37. A study on the oxidation behavior of Nb alloy (Nb-1 pct Zr-0.1 pct C) and silicide-coated Nb alloys10.1007/s11661-012-1554-1 ↗
38. Oxidation kinetics and high temperature in-situ observation of the oxidation behaviour of NbSi2 at 1023K10.1007/s11431-006-0147-x ↗
39. Oxidation-induced crack healing in Ti3AlC2 ceramics10.1016/j.scriptamat.2007.09.006 ↗
40. Crack-healing behavior of Si3N4/SiC ceramics under stress and fatigue strength at the temperature of healing (1000°C)10.1016/S0955-2219(01)00435-6 ↗
41. Crack healing behavior of silicon carbide ceramics10.1111/j.1151-2916.2000.tb01632.x ↗
42. Crack healing in silicon carbide10.1111/j.1551-2916.2004.00490.x ↗
43. Grain growth in thin films of ThO2, NpO2, and PuO210.1002/pssb.19680290245 ↗
44. Crack healing and strengthening of thermally shocked alumina10.1111/j.1151-2916.1976.tb10949.x ↗