journal article·2019-07

Effect of pH of the sulfuric acid bath on cavitation erosion behavior in natural seawater of electroless nickel plating coating

Il-Cho Park, Seong-Jong Kim

Publisher page

Abstract

Abstract Electroless nickel plating (ENP) was performed to prevent the cavitation erosion damage of gray cast iron in the marine environment. The effect of the changes in the pH of a plating bath on the ENP coating characteristics, corrosion resistance and the cavitation erosion damage behavior in natural seawater were examined. The results showed that the pH of the plating bath had a significant effect on the plating rate, crystallinity, composition, and microhardness of the ENP coating. The corrosion resistance of ENP coating was greatly affected by the plating rate and the microstructure of the substrate. The cavitation erosion damage behavior depended on the crystallinity of the ENP coating. Once the substrate is exposed by the cavitation erosion of ENP coating, it is accompanied by galvanic corrosion, which accelerates the damage. Furthermore, the cavitation erosion damage mechanism of ENP coating was investigated.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Electrodeposition and Electroless Coatings · Corrosion Behavior and Inhibition · Metal and Thin Film Mechanics

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (41)

Show source-provided references
1. Tribological study of gray cast iron with automotive brake linings: the effect of rotor microstructure10.1016/S0301-679X(02)00260-8 ↗
2. A methodology for the fatigue design of notched castings in gray cast iron10.1016/j.engfracmech.2006.04.018 ↗
3. Analysis of cavitation erosion resistance of cast iron and nonferrous metals based on database and comparison with carbon steel data10.1016/j.wear.2010.04.031 ↗
4. Cavitation corrosion of nodular cast iron (NCI) in seawater: Microstructural effects10.1016/S1044-5803(02)00185-7 ↗
5. Ultrasonic cavitation erosion of nodular cast iron with ferrite–pearlite microstructure10.1016/j.ultsonch.2014.11.001 ↗
6. Tribology of electroless nickel coatings–a review10.1016/j.matdes.2010.11.013 ↗
7. Electroless nickel, alloy, composite and nano coatings–a critical review10.1016/j.jallcom.2013.03.107 ↗
8. Cavitation erosion behavior of electroless nickel-plating on AISI 1045 steel10.1016/j.wear.2005.02.099 ↗
9. The cavitation erosion behavior of electroless Ni–P–SiC composite coating10.1016/j.wear.2006.03.054 ↗
10. Electroless nickel plating from acid bath10.1016/S0257-8972(99)00423-5 ↗
11. Dynamic behavior of electroless nickel plating reaction on magnesium alloys10.1007/s11998-011-9336-z ↗
12. Electroless nickel-phosphorus plating on silicon carbide particles for metal matrix composites10.1016/j.ceramint.2014.08.027 ↗
13. On the mechanism of electroless Ni-P plating10.1149/1.2055125 ↗
14. Influence of pH values on electroless Ni-P-SiC plating on AZ91D magnesium alloy10.1016/S1003-6326(10)60560-2 ↗
15. Effects of preparation technology on the structure and amorphous forming region for electroless Ni-P alloys10.1016/S0924-0136(01)01021-4 ↗
16. Electroless deposition of ternary Ni-P alloy coatings containing tungsten or nano-scattered alumina composite on steel10.1007/s10800-007-9451-9 ↗
17. Effect of bath pH and stabilizer on electroless nickel plating of magnesium alloys10.1016/j.surfcoat.2013.04.011 ↗
18. Microstructure evolution and hardening mechanisms of Ni-P electrodeposits10.1016/j.surfcoat.2010.08.115 ↗
19. Improved microhardness and wear resistance of the as-deposited electroless Ni-P coating10.1016/j.surfcoat.2008.06.180 ↗
20. Modified Scherrer equation to estimate more accurately nano-crystallite size using XRD10.4236/wjnse.2012.23020 ↗
21. Mallory · 1990 · 57
22. Structure and mechanical properties of Ni–P electrodeposited coatings10.1016/j.apsusc.2008.10.013 ↗
23. Grain size effects in nanocrystalline materials10.1557/JMR.1992.2114 ↗
24. The relationship between hardness and abrasive wear resistance of electrodeposited nanocrystalline Ni-P coatings10.1016/S1359-6462(02)00633-4 ↗
25. Nanomechanics of Hall-Petch relationship in nanocrystalline materials10.1016/j.pmatsci.2009.03.008 ↗
26. Role of phosphorus in the electrochemical behavior of electroless Ni-P alloys in 3.5 wt.% NaCl solutions10.1016/S0257-8972(05)80023-4 ↗
27. Effect of grain size on corrosion behavior of electrodeposited bulk nanocrystalline Ni10.1016/S1003-6326(09)60101-1 ↗
28. The observation of the nucleation and growth of electrolessly plated nickel deposited from different bath pH by TEM and QCM method10.1016/j.electacta.2006.05.021 ↗
29. Denny · 2011 · 168
30. Characterization of corrosion products formed on steels in the first months of atmospheric exposure10.1590/S1516-14392003000300015 ↗
31. The effects of stabilizers on the bath stability of electroless Ni deposition and the deposit10.1016/j.apsusc.2004.02.003 ↗
32. Effect of organic additives on the corrosion resistance properties of electroless nickel deposits10.1016/j.tsf.2007.10.008 ↗
33. Effect of thiourea and lead acetate on the deposition of electroless nickel10.1016/S0254-0584(01)00516-8 ↗
34. Preventing hydrogen embrittlement in stainless steel by means of compressive stress induced by cavitation peening
35. Comparison between cavitation peening and shot peening for extending the fatigue life of a duralumin plate with a hole10.1016/j.jmatprotec.2015.08.012 ↗
36. Cavitation and electrochemical characteristics in seawater by water cavitation peening of 5083-O Al alloy for ships10.1142/S0218625X17500767 ↗
37. The effects of triple junctions and grain boundaries on hardness and Young's modulus in nanostructured Ni-P10.1016/S1359-6462(02)00511-0 ↗
38. Triple line disclination effects on the mechanical behaviour of materials10.1016/0956-716X(90)90091-T ↗
39. On the role of intercrystalline defects in polycrystal plasticity10.1016/S1359-6462(98)00173-0 ↗
40. Triple-line corrosion in high purity nickel10.1016/0921-5093(89)90300-6 ↗
41. Erb · 1996 · 93