Abstract The etching process of an ultra-wide bandgap β-Ga2O3 semiconductor is challenging, owing to its high chemical robustness and bond strength. We demonstrated the photoelectrochemical (PEC) etching of β-Ga2O3 using phosphoric acid as electrical potential and temperature were varied, both of which were proportional to the etching rate. Once initiated at defect sites, the etch pit anisotropically proceeded along the [0 0 1] direction with an activation energy of 46.3 kJ/mol, which is much lower than previously reported values. The PEC etching rate was as high as 0.7 μm/min in the [0 0 1] direction at a bias of 20 V and temperature of 160 °C. The new facet exposed by PEC etching in phosphoric acid was found to be (−2 0 1), which is assumed to be stable because the Ga-terminated (−2 0 1) surface is converted into an O-terminated one after the removal of the Ga on the surface. The optoelectronic performance, including the responsivity and response/decay characteristics, was greatly improved, indicating the effective removal of defects by PEC etching. Our findings are expected to play an important role in the fabrication of an ultra-wide bandgap β-Ga2O3 semiconductor devices, thus paving the way for improved optoelectronic device performance.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Ga2O3 and related materials · ZnO doping and properties · Advanced Photocatalysis Techniques
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (41)
Show source-provided references
1. Observation of nanometer-sized crystalline grooves in as-grown β-Ga2O3 single crystals10.7567/JJAP.55.030303 ↗
2. Exfoliated β-Ga2O3 nano-belt field-effect transistors for air-stable high power and high temperature electronics10.1039/C6CP01987K ↗
3. Demonstration of mechanically exfoliated β-Ga2O3/GaN p-n heterojunction10.1063/1.5088516 ↗
4. Revelation of dislocations in β-Ga2O3 substrates grown by edge-defined film-fed growth10.1002/pssa.201900630 ↗
5. Radiation damage effects in Ga2O3 materials and devices10.1039/C8TC04193H ↗
6. Scaling-up of bulk β-Ga2O3 single crystals by the czochralski method
7. Large-size β-Ga2O3 single crystals and wafers10.1016/j.jcrysgro.2004.06.027 ↗
8. High-quality β-Ga2O3 single crystals grown by edge-defined film-fed growth10.7567/JJAP.55.1202A2 ↗
9. A review of β-Ga2O3 single crystal defects, their effects on device performance and their formation mechanism10.1088/1674-4926/40/1/011804 ↗
10. Relationship between crystal defects and leakage current in β-Ga2O3 Schottky barrier diodes10.7567/JJAP.55.1202BB ↗
11. Near unity ideality factor for sidewall Schottky contacts on un-intentionally doped β-Ga2O3
12. Improvement of dry etch-induced surface roughness of single crystalline β-Ga2O3 using post-wet chemical treatments10.1016/j.apsusc.2019.144673 ↗
13. Tuning the thickness of exfoliated quasi-two-dimensional β-Ga2O3 flakes by plasma etching10.1063/1.4979028 ↗
14. Inductively-coupled-plasma reactive ion etching of single-crystal β-Ga2O310.7567/JJAP.56.030304 ↗
15. Chlorine-based dry etching of β-Ga2O310.1088/0268-1242/31/6/065006 ↗
16. A preliminary study of SF6 based inductively coupled plasma etching techniques for beta gallium trioxide thin film10.1016/j.mssp.2015.05.065 ↗
17. Inductively coupled plasma etch damage in (-201) Ga2O3 Schottky diodes10.1063/1.4979592 ↗
18. Annealing of dry etch damage in metallized and bare (-201) Ga2O310.1116/1.4986300 ↗
19. Defects at the surface of β-Ga2O3 produced by Ar plasma exposure10.1063/1.5109025 ↗
20. Crystal growth, defects, and mechanical and spectral properties of a novel mixed laser crystal Nd:GdYNbO410.1007/s00339-016-0672-9 ↗
21. Wet Etching of β-Ga2O3 substrates10.1143/JJAP.48.040208 ↗
22. Dry and wet etching for β-Ga2O3 Schottky barrier diodes with mesa termination10.7567/1347-4065/ab4f90 ↗
23. Anisotropic etching of β-Ga2O3 using hot phosphoric acid
24. Origins of etch pits in β-Ga2O3 (010) single crystals10.7567/JJAP.55.1202BG ↗
25. Crystal defects observed by the etch-pit method and their effects on Schottky-barrier-diode characteristics on (-201) β-Ga2O310.7567/JJAP.56.091101 ↗
26. Characterization of crystalline defects in β-Ga2O3 single crystals grown by edge-defined film-fed growth and halide vapor-phase epitaxy using synchrotron X-ray topography10.7567/1347-4065/ab0dba ↗
27. Wet chemical etching behavior of β-Ga2O3 single crystal10.1002/pssc.200779223 ↗
28. Nanoscale groove textured β-Ga2O3 by room temperature inverse metal-assisted chemical etching and photodiodes with enhanced responsivity10.1063/1.5053219 ↗
29. High aspect ratio β-Ga2O3 Fin arrays with low-interface charge density by inverse metal-assisted chemical etching10.1021/acsnano.9b01709 ↗
30. Tuning the threshold voltage of exfoliated β-Ga2O3 flake-based field-effect transistors by photo-enhanced H3PO4 Wet Etching
31. Excellent potential of photo-electrochemical etching for fabricating high-aspect-ratio deep trenches in gallium nitride10.7567/APEX.11.091001 ↗
32. Porous formation in p-type gallium nitride films via 50 Hz operated alternating current-assisted photo-electrochemical etching in methanol-sulfuric acid solution10.1149/2.0591810jes ↗
33. Structural, morphological, optical, and gas sensing characteristics of ultraviolet-assisted photoelectrochemical etching derived AlInGaN nano-spikes10.1016/j.jmrt.2019.03.011 ↗
34. Porous quaternary Al0.1In0.1Ga0.8N film formation via photoelectrochemical etching in HF:C2H5OH Electrolyte10.1111/jace.14241 ↗
35. Quasi-two-dimensional β-Ga2O3 solar-blind photodetectors with ultrahigh responsivity10.1039/C6TC02467J ↗
36. β-Ga2O3 single crystal as a photoelectrode for water splitting10.7567/JJAP.52.111102 ↗
37. Characterization of defects in β-Ga2O3 single crystals10.7567/JJAP.54.051103 ↗
38. Selective electrochemical etching of epitaxial aluminum nitride thin film10.1016/j.apsusc.2020.145279 ↗
39. Doping selective lateral electrochemical etching of GaN for chemical lift-off10.1063/1.3153116 ↗
40. A comparative study of wet etching and contacts on (-201) and (010) oriented β-Ga2O310.1016/j.jallcom.2017.09.336 ↗
41. Simultaneously improved sensitivity and response speed of β-Ga2O3 solar-blind photodetector via localized tuning of oxygen deficiency10.1063/1.5088665 ↗