Influence of stripping and cooling atmospheres on surface properties and corrosion of zinc galvanizing coatings
Source abstract
Abstract
In this work the influence of stripping/cooling atmospheres used after withdrawal of steel sheet from Zn or Zn-alloy melt on surface properties of Zn (Z) and Zn-Al-Mg (ZM) hot-dip galvanizing coatings has been studied. The aim was to understand how the atmosphere (composed by nitrogen (N2) or air) affects adhesion strength to model adhesive and corrosive behaviour of the galvanized substrates. It was shown that the surface chemical composition and Volta potential of the galvanizing coatings prepared under the air or nitrogen atmosphere are strongly influenced by the atmosphere. The surface chemistry Z and ZM surfaces prepared under N2 contained a higher content of metal atoms and a richer hydroxide density than the specimens prepared under air atmosphere as assessed by X-ray photoelectron spectroscopy (XPS). The induced differences on the microstructure of the galvanized coatings played a key role on the local corrosion induced defects as observed by means of in situ Atomic force microscopy (AFM). Peel force tests performed on the substrates coated by model adhesive films indicate a higher adhesive strength to the surfaces prepared under nitrogen atmosphere. The obtained results have been discussed in terms of the microstructure and surface chemical composition of the galvanizing coatings.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Corrosion Behavior and Inhibition · Concrete Corrosion and Durability · Hydrogen embrittlement and corrosion behaviors in metals
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (41)
Show source-provided references
1. Shreir · 1994
2. The delamination of polymeric coatings from electrogalvanised steel—a mechanistic approach: part 1: delamination from a defect with intact zinc layer10.1016/S0010-938X(00)00047-0 ↗
3. Characterization of hot-dip galvanized (HDG) steel treated with bis-1,2-(triethoxysilyl)ethane and γ-aminopropyltriethoxysilane10.1163/15685610152542342 ↗
4. Formation and stability of organophosphonic acid monolayers on ZnAl alloy coatings10.1016/j.surfcoat.2010.04.027 ↗
5. Hot-dip coatings, ASTM Handbook Corrosion, Vol. 13, 1999.
6. P. Biele, Determination of the active Al and Fe contents in the zinc bath and their influence on alloys-layer formation in the hot galvanizing process, in: Galvatech’95 (1995) 769–776.
7. Study of zinc coatings on steel substrate attained by two different techniques10.1016/S0257-8972(99)00358-8 ↗
8. Schuhmacher · Surf. Coat. Technol. · 2003 · 163–164 · 70310.1016/S0257-8972(02)00660-6 ↗
9. T. Tsujimura, A. Komatsu, A. Andoh, in: Proc. Galvatech June 2001, Belgium: Stahleisen, 2001, pp. 145–152.
10. Corrosion resistance of zinc—magnesium coated steel10.1016/j.corsci.2007.03.032 ↗
11. The metallurgy of zinc-coated steel10.1016/S0079-6425(98)00006-1 ↗
12. Hartshorn · 1986
13. Acid-base characterization of aluminum oxide surfaces with XPS10.1021/jp037877f ↗
14. Surface chemistry of galvanized steel sheets relevant to adhesion performance10.1016/0300-9440(95)00610-9 ↗
15. Interfacial layer development in hot-dip galvanneal coating in interstitial free (IF) steel10.1007/BF02652311 ↗
16. C.E. Jordan, A.R. Marder, Alloy layer growth during hot-dip initial reaction of the Fe–Al layer during the first stages galvanizing at 450°C, in: Galvatech ’95 (1995) 319–325.
17. J. Davene, L. Dondin, J.K. Kem, S.I. Kin, Dynamic air knife: DAK, in: Galvatech ’95 (1989) 205–213.
18. Nanoscopic view on the initial stages of corrosion of hot-dip galvanized Zn-Mg-Al coatings10.1016/j.corsci.2014.02.027 ↗
19. SKP and FT-IR microscopy study of the paint corrosion de-adhesion from the surface of galvanized steel10.1016/j.porgcoat.2011.10.009 ↗
20. Characterization of AA2024-T3 by scanning Kelvin probe force microscopy10.1149/1.1838633 ↗
21. Calibration of the scanning Kelvin probe force microscope under controlled environmental conditions10.1016/j.electacta.2012.01.054 ↗
22. Evolution of the surface chemistry of hot-dip galvanized Zn-Mg-Al and Zn coatings on steel during short term exposure to sodium chloride containing environments10.1016/j.corsci.2014.11.033 ↗
23. Critical assessment and thermodynamic modeling of Mg-Zn, Mg-Sn, Sn-Zn and Mg-Sn-Zn systems10.1016/j.calphad.2011.10.007 ↗
24. Solidification structure of the coating layer on hot-Dip Zn-11% Al-3% Mg-0.2% Si-coated steel sheet10.2320/matertrans.MRA2008009 ↗
25. M. Vlot, M. Zuijderwijk, M. Toose, L. Elliott, R. Bleeker, T. Maalman in, Proceedings Galvatech 2007, ISIJ, 510–515.
26. Corrosion behaviour of Zn-Al-Mg coated steel sheet in sodium chloride-containing environment10.1016/j.corsci.2009.06.019 ↗
27. Probing the atmospheric corrosion of metals: zinc10.1134/S003317320605002X ↗
28. Volta potential of oxidized aluminum studied by scanning Kelvin probe force microscopy10.1021/jp1011044 ↗
29. Scanning Kelvin probe study of (Oxyhydr) oxide surface of aluminum alloy10.1021/jp205585u ↗
30. The physical meaning of electrode potentials at metal surfaces and polymer/metal interfaces: consequences for delamination10.1149/1.2926589 ↗
31. Corrosion mechanism of model zinc–magnesium alloys in atmospheric conditions10.1016/j.corsci.2008.06.008 ↗
32. 1986 · 33
33. Self-localization of polyacrylic acid molecules on polar ZnO(0001)-Zn surfaces10.1039/c1cp20913b ↗
34. Interface chemistry and molecular interactions of phosphonic acid self-assembled monolayers on oxyhydroxide-covered aluminum in humid environments10.1021/la200445x ↗
35. R. Hausbrand, M. Rohwerder, M. Stratmann, C. Schwerdt, B. Schuhmacher, G. Grundmeier, in: Proc. Galvatech June, 2001, pp. 161–167.
36. Corrosion mechanisms of Zn(Mg,Al) coated steel: 2: The effect of Mg and Al alloying on the formation and properties of corrosion products in different electrolytes10.1016/j.corsci.2014.07.042 ↗
37. The influence of magnesium and hydrogen introduction in sputtered zinc oxide thin films10.1016/j.tsf.2005.07.066 ↗
38. Delamination resistant zinc alloys: simple concept and results on the system zinc–magnesium10.1002/srin.200300212 ↗
39. Corrosion of zinc–magnesium coatings: mechanism of paint delamination10.1016/j.corsci.2009.05.042 ↗
40. In situ monitoring of the microstructural corrosion mechanisms of zinc–magnesium–aluminium alloys using time lapse microscopy10.1016/j.corsci.2011.02.043 ↗
41. Understanding corrosion via corrosion product characterization: II. Role of alloying elements in improving the corrosion resistance of Zn-Al-Mg coatings on steel10.1016/j.corsci.2011.03.016 ↗