journal article·2015-10

Effects of combined plasma chromizing and shot peening on the fatigue properties of a Ti6Al4V alloy

Shouming Yu, Daoxin Liu, Xiaohua Zhang, Dongxing Du

Publisher page

Abstract

Abstract A plasma chromizing treatment was conducted on Ti6Al4V samples by employing the recently developed double glow plasma surface alloying technology. The Cr-alloyed layer consisted of four sub-layers, namely the Cr deposition, Cr 2 Ti, CrTi 4 , and Cr-Ti solid-solution layers. The local hardness and moduli were determined via nanoindentation. In addition, the fatigue properties of the samples were evaluated by using a rotating-bending fatigue machine under a given load. The results showed that the hardness or elastic moduli of the adjacent sub-layers differed significantly and the fatigue properties of the Ti6Al4V alloy deteriorated with the plasma chromizing treatment. This deterioration stemmed mainly from cracks initiated at the interfaces between the sub-layers and the microstructural changes of the substrate; these changes were induced by the high temperature used in the plasma chromizing process. However, the fatigue life of the plasma-chromized samples was increased by a shot peening post-treatment. The fatigue life of the samples resulting from this combination of treatments was slightly higher than that of the single-shot-peened Ti6Al4V substrate. In fact, the sample retaining only the Cr-Ti solid-solution layer (that is, the first three sub-layers were removed), when shot-peened, exhibited the highest fatigue life among all the tested samples; this was attributed to that sample having the highest residual compressive stress, the significant work hardening, and the good hardness to toughness balance.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Metal and Thin Film Mechanics · Surface Treatment and Residual Stress · Metal Alloys Wear and Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (24)

Show source-provided references
1. Dry sliding wear mechanisms of the Ti6Al4V alloy10.1016/S0043-1648(96)07454-6 ↗
2. Tribological properties of titanium alloys10.1016/0043-1648(91)90249-T ↗
3. Tribological behavior of plasma Mo-N surface modified Ti-6Al-4V alloy10.1016/S0257-8972(03)00855-7 ↗
4. Double glow plasma surface alloying and plasma nitriding10.1016/j.surfcoat.2006.07.187 ↗
5. Recent developments in improving tribological performance of TC4 titanium alloy via double glow plasma surface alloying in China: a literature review
6. Tribology behavior of double-glow discharge Mo layers on titanium alloy in aviation kerosene environment10.1016/S1003-6326(11)61415-5 ↗
7. Friction and wear behaviors of Mo-N modified Ti6Al4V alloy in Hanks’ solution10.1016/j.surfcoat.2012.05.046 ↗
8. Microstructure and sliding wear behavior of pure titanium surface modified by double-glow plasma surface alloying with Nb10.1016/j.matdes.2013.05.061 ↗
9. Characteristics and wear performance of borided Ti6Al4V alloy prepared by double glow plasma surface alloying10.1016/j.surfcoat.2013.02.053 ↗
10. Evaluation of surface-modified Ti-6Al-4V alloy by combination of plasma-carburizing and deep-rolling10.1016/j.msea.2007.11.079 ↗
11. Bloyce · 1994 · 835
12. Effect of ceramic conversion surface treatment on fatigue properties of Ti6Al4V alloy10.1016/j.ijfatigue.2006.11.016 ↗
13. Effects of combined plasma-caburizing and shot-peening on fatigue and wear properties of Ti-6Al-4V alloy10.1016/j.surfcoat.2008.11.013 ↗
14. Plasma chromizing and wear resistance of Ti6Al4V alloy and AISI420 stainless steel
15. Assessments on friction and wear behaviors of P110 steel and chromizing coating sliding against two counterparts under dry and wet conditions10.1016/j.apsusc.2012.01.128 ↗
16. Cyclic oxidation behavior of plasma surface chromising coating on titanium alloy Ti-6Al-4V10.1016/j.apsusc.2012.08.102 ↗
17. GB/T 2965, Titanium and titanium alloy bars, 2007.
18. GB/T 4337, Metallic materials – fatigue testing – rotating bar bending method, 2008.
19. Measurement of hardness and elastic modulus by instrumented indentation: advances in understanding and refinements to methodology10.1557/jmr.2004.19.1.3 ↗
20. Effects of surface treatments on the fatigue strength of AISI 4340 aeronautical steel10.1016/S0142-1123(01)00015-9 ↗
21. Fatigue behaviour of 2011-T6 aluminium alloy coated with PVD WC/C, PA-CVD DLC and PE-CVD SiOx coatings10.1016/j.surfcoat.2009.03.040 ↗
22. Effect of film elastic modulus on fatigue behaviour of DLC-coated wrought magnesium alloy AZ6110.1016/j.proeng.2011.04.179 ↗
23. Evaluating the effects of plasma diffusion processing and duplex diffusion/PVD-coating on the fatigue performance of Ti-6Al-4V alloy10.1016/j.ijfatigue.2011.04.004 ↗
24. An evaluation of shot peening, residual stress and stress relaxation on the fatigue life of AISI 4340 steel10.1016/S0142-1123(01)00205-5 ↗