Microstructure refinement for superior ductility of Al–Si alloy by electron beam melting
Source abstract
Abstract
Abstract Refining the microstructure to improve the ductility of an Al‒Si alloy is challenging. In this paper, we report for the first time a novel microstructure refinement approach for AlSi10Mg (wt%) alloys using electron beam melting (EBM) technology, without the addition of any modification elements. The synergetic effect of superheating, fast cooling, and preheating contributes to a refined Si phase with a fine granular structure (0.5–2 μm) within bimodal Al grains (40 μm grains and 0.5–2 μm sub-grains). The results provide good evidence for the proposed refinement mechanism. A maximum ductility of approximately 32.7 % with a tensile strength of approximately 136 MPa was achieved for the as-built AlSi10Mg EBM alloy. After solution heat treatment and T6-like aging, nano-Si precipitates formed which strengthened the alloys. The pathway developed in this study for refining the Al–Si alloy microstructure to improve the tensile ductility will provide a feasible and fast manufacturing method for improving the microstructure and mechanical properties of other low-melting temperature alloys in the near future using EBM technology.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Aluminum Alloy Microstructure Properties · Additive Manufacturing Materials and Processes · High-Temperature Coating Behaviors
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (75)
Show source-provided references
1. A.S.M. International · 1991
2. Kearney · 1990
3. Eutectic nucleation in Al-Si alloys10.1016/j.actamat.2004.05.043 ↗
4. Effect of trace La addition on the microstructures and mechanical properties of A356 (Al–7Si–0.35Mg) aluminum alloys10.1016/j.jallcom.2009.07.183 ↗
5. The aluminum–silicon eutectic reaction: mechanisms and crystallography10.1016/S1471-5317(02)00003-2 ↗
6. Nucleation mechanism of the eutectic phases in aluminum–silicon hypoeutectic alloys10.1016/j.actamat.2004.05.045 ↗
7. Pacz · 1921
8. The microstructure and mechanical properties of unidirectionally solidified Al−Si alloys10.1007/BF02385422 ↗
9. Mondolfo · 1976
10. A selective laser melting and solution heat treatment refined Al-12Si alloy with a controllable ultrafine eutectic microstructure and 25% tensile ductility10.1016/j.actamat.2015.05.017 ↗
11. Superheat-dependent microstructure of molten Al–Si alloys of different compositions studied by small angle neutron scattering10.1016/j.jallcom.2012.09.086 ↗
12. Structure of molten Al and eutectic Al–Si alloy studied by neutron diffraction10.1016/j.jnoncrysol.2012.10.027 ↗
13. The influence of process parameters on vertical surface roughness of the AlSi10Mg parts fabricated by selective laser melting10.1016/j.jmatprotec.2018.10.015 ↗
14. Fine-structured aluminium products with controllable texture by selective laser melting of pre-alloyed AlSi10Mg powder10.1016/j.actamat.2012.11.052 ↗
15. Reducing porosity in AlSi10Mg parts processed by selective laser melting
16. 3D printing of high-strength aluminium alloys10.1038/nature23894 ↗
17. The effect of texture on the anisotropy of thermophysical properties of additively manufactured AlSi10Mg
18. Role of hierarchical microstructure of additively manufactured AlSi10Mg on dynamic loading behavior
19. Factors that affect the properties of additively-manufactured AlSi10Mg: porosity versus microstructure
20. Quality control of AlSi10Mg produced by SLM: metallography versus CT scans for critical defect size assessment
21. Compressive creep of AlSi10Mg parts produced by selective laser melting additive manufacturing technology
22. On microstructure and early stage corrosion performance of heat treated direct metal laser sintered AlSi10Mg
23. Nondestructive ultrasonic evaluation of additively manufactured AlSi10Mg samples
24. High-temperature mechanical properties of AlSi10Mg specimens fabricated by additive manufacturing using selective laser melting technologies (AM-SLM)
25. Split Hopkinson pressure bar tests for investigating dynamic properties of additively manufactured AlSi10Mg alloy by selective laser melting
26. Columnar to equiaxed transition during direct metal laser sintering of AlSi10Mg alloy: effect of building direction
27. On the effect of shot-peening on fatigue resistance of AlSi10Mg specimens fabricated by additive manufacturing using selective laser melting (AM-SLM)
28. Strengthening mechanisms in direct metal laser sintered AlSi10Mg: comparison between virgin and recycled powders
29. Thermal post-processing of AlSi10Mg parts produced by Selective Laser Melting using recycled powder
30. Continuous wave vs pulsed wave laser emission in selective laser melting of AlSi10Mg parts with industrial optimized process parameters: Microstructure and mechanical behaviour
31. Process dependent porosity and the influence of shot peening on porosity morphology regarding selective laser melted AlSi10Mg parts
32. Abrasive fluidized bed (AFB) finishing of AlSi10Mg substrates manufactured by Direct Metal Laser Sintering (DMLS)
33. The effect of atmosphere on the structure and properties of a selective laser melted Al-12Si alloy10.1016/j.msea.2014.01.012 ↗
34. Selective laser melting of nano-TiB2 decorated AlSi10Mg alloy with high fracture strength and ductility10.1016/j.actamat.2017.02.062 ↗
35. High power selective laser melting (HP SLM) of aluminum parts10.1016/j.phpro.2011.03.035 ↗
36. Selective laser melting of aluminium components, J. Mater
37. van Lancker · 1967
38. Build direction dependence of microstructure and high-temperature tensile property of Co-Cr-Mo alloy fabricated by electron beam melting10.1016/j.actamat.2013.10.017 ↗
39. Phase and grain size inhomogeneity and their influences on creep behavior of Co-Cr-Mo alloy additive manufactured by electron beam melting10.1016/j.actamat.2014.11.012 ↗
40. Advanced metal powder based manufacturing of complex components by electron beam melting10.1179/106678509X12475882446133 ↗
41. Effects of post-processing on cyclic fatigue response of a titanium alloy additively manufactured by electron beam melting10.1016/j.msea.2016.10.059 ↗
42. Preparation of weak-textured commercially pure titanium by electron beam melting
43. Cellular lattices of biomedical Co-Cr-Mo-alloy fabricated by electron beam melting with the aid of shape optimization
44. Investigations of and precipitates in the nickel-based superalloy 718 produced by electron beam melting10.1016/j.msea.2007.07.012 ↗
45. Microstructures of Rene 142 nickel-based superalloy fabricated by electron beam melting10.1016/j.actamat.2013.04.002 ↗
46. CoCrFeNiTi-based high-entropy alloy with superior tensile strength and corrosion resistance achieved by a combination of additive manufacturing using selective electron beam melting and solution treatment10.1016/j.matlet.2016.11.026 ↗
47. Novel precipitate-microstructural architecture developed in the fabrication of solid copper components by additive manufacturing using electron beam melting10.1016/j.actamat.2011.03.033 ↗
48. Open-cellular copper structures fabricated by additive manufacturing using electron beam melting10.1016/j.msea.2011.03.053 ↗
49. Molten pool behavior and effect of fluid flow on solidification conditions in selective electron beam melting (SEBM) of a biomedical Co-Cr-Mo alloy
50. Effect of heat treatment on AlSi10Mg alloy fabricated by selective laser melting: microstructure evolution, mechanical properties and fracture mechanism10.1016/j.msea.2016.03.088 ↗
51. Microstructure and strength of selectively laser melted AlSi10Mg10.1016/j.actamat.2016.07.012 ↗
52. Multiple precipitation pathways in an Al-7Si-0.6Mg alloy fabricated by selective laser melting10.1016/j.scriptamat.2018.09.045 ↗
53. Quantification and characterisation of porosity in selectively laser melted Al-Si10-Mg using X-ray computed tomography10.1016/j.matchar.2015.12.001 ↗
54. Nanostructural hierarchy increases the strength of aluminium alloys10.1038/ncomms1062 ↗
55. Properties and selection: nonferrous alloys and Special-purpose materials
56. Effects of electromagnetic stirring and superheat on the microstructural characteristics of Al–Si–Fe alloy10.1016/j.msea.2006.05.076 ↗
57. Grain refinement of Al–Si alloy (A356) by melt thermal treatment10.1016/S0924-0136(02)01007-5 ↗
58. Additive manufacturing of metals10.1016/j.actamat.2016.07.019 ↗
59. Effect of build geometry on the β-grain structure and texture in additive manufacture of Ti6Al4V by selective electron beam melting10.1016/j.matchar.2013.07.012 ↗
60. The nucleation crystallography and wettability of Mg grains on active Al2Y inoculants in an Mg-10 wt% y Alloy10.1016/j.jallcom.2013.10.042 ↗
61. Microstructure, defects and mechanical behavior of beta-type titanium porous structures manufactured by electron beam melting and selective laser melting10.1016/j.actamat.2016.04.029 ↗
62. Standard Specification for Aluminum-Alloy Die Castings, West Conshohocken, PA, 2014. https://doi.org/10.1520/B0085-B0085M-14.
63. Oxides, porosity and fatigue performance of AlSi10Mg parts produced by selective laser melting10.1016/j.ijfatigue.2016.06.002 ↗
64. Fatigue performance enhancement of selectively laser melted aluminium alloy by heat treatment
65. Jürgen Hirsch Birgit Skrotzki · 2008
66. Warmuzek · 2004
67. Microstructures and mechanical properties of A356 (AlSi7Mg0.3) aluminum alloy fabricated by selective laser melting10.1016/j.matdes.2015.10.065 ↗
68. High tensile ductility in a nanostructured metal10.1038/nature01133 ↗
69. Microstructural evolution and hardening parameters10.1016/S0921-5093(01)01191-1 ↗
70. Totten · 2003
71. Microstructure and flow stress of polycrystals and single crystals10.1016/S1359-6454(97)00365-0 ↗
72. Microstructure and strengthening mechanisms in an Al-Mg-Si alloy processed by equal channel angular pressing (ECAP)10.1007/s00170-017-1310-1 ↗
73. Mechanical behavior and strengthening mechanisms in ultrafine grain precipitation-strengthened aluminum alloy10.1016/j.actamat.2013.09.042 ↗
74. Hardening by annealing and softening by deformation in nanostructured metals10.1126/science.1124268 ↗
75. Nanostructured high-strength molybdenum alloys with unprecedented tensile ductility10.1038/nmat3544 ↗