Abstract

Abstract The crystallographic properties of tantalum films deposited as a bioactive coating on Co–Cr–Mo and Ti–Al–Nb alloys have been investigated. The desired tough and ductile alpha phase of tantalum has been obtained by DC magnetron sputtering on Co–Cr–Mo and Ti–Al–Nb substrates. The thickness of the tantalum layer was between 20 and 600 nm. The crystallographic structure of tantalum thin film was dependent on the sputtering parameters such as DC power, bias voltage and gas impurities. Oxygen is an important factor for the stabilization of the tantalum alpha phase on Co–Cr–Mo substrate. The crystallographic structure and texture of tantalum thin films was found to be additionally dependent on the substrate composition. For Ti–Al–Nb substrate, oxygen content was not an important factor for the stabilization of the alpha phase. The observed shift of X-ray diffraction peaks to lower 2(θ) is an indication of stress evolving during the sputtering process and was dependent on bias voltage and oxygen content of the carrier gas.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Metal and Thin Film Mechanics · Titanium Alloys Microstructure and Properties · Bone Tissue Engineering Materials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (35)

Show source-provided references
1. In vivo and in vitro evaluation of vitreous coating on cobalt base alloys for the prosthetic devices10.1016/S0022-3093(02)01035-9 ↗
2. Electrochemical corrosion and metal ion release from Co–Cr–Mo prosthesis with titanium plasma spray coating10.1016/j.biomaterials.2005.01.004 ↗
3. In vitro biocorrosion of Co–Cr–Mo implant alloy by macrophage cells10.1016/j.orthres.2004.04.005 ↗
4. Corrosion fatigue of biomedical metallic alloys: mechanisms and mitigation10.1016/j.actbio.2011.09.012 ↗
5. particular Co–Cr–Mo alloy implant metals activate the inflammasome danger signaling pathway in human macrophages: a novel mechanism for implant debris reactivity10.1002/jor.20826 ↗
6. Soluble ions more than particulate cobalt-alloy implant debris induce monocyte costimulatory molecule expression and release of proinflammatory cytokines critical to metal-induced lymphocyte reactivity10.1002/jbm.a.32627 ↗
7. Investigation of the binding of Cr(III) complexes to bovine and human serum proteins: a proteomic approach10.1002/jbm.a.32700 ↗
8. Does ion release differ between hip resurfacing and metal-on-metal THA?10.1007/s11999-007-0106-2 ↗
9. Do ion levels in hip resurfacing differ from metal-on-metal THA at midterm?10.1007/s11999-010-1424-3 ↗
10. Wear properties of Ti and Ti–6Al–7Nb castings for dental prostheses10.1016/S0142-9612(02)00533-1 ↗
11. Studies on polishing of Ti and Ag–Pd–Cu–Au alloy with five dental abrasives10.1046/j.1365-2842.2001.00737.x ↗
12. Comparative evaluation of metal ions release from titanium and Ti–6Al–7Nb into bio-fluids
13. Biocompatibilty of corrosion-resistant zeolite coatings for titanium alloy biomedical implants10.1016/j.actbio.2009.04.019 ↗
14. Aluminum ions enhance neuronal damage mediated by NMDA-activated glutamate receptors10.1134/S1990747809040096 ↗
15. Empirical data confirm autism symptoms related to aluminum and acetaminophen exposure10.3390/e14112227 ↗
16. Fatigue and wear evaluation of Ti–Al–Nb alloys for biomedical applications10.1016/j.msec.2007.04.003 ↗
17. The corrosion behavior of Ti–6Al–4V, Ti–6Al–7Nb and Ti–13Nb–13Zr in protein solutions10.1016/S0142-9612(98)00217-8 ↗
18. Direct laser processing of a tantalum coating on titanium for bone replacement structure10.1016/j.actbio.2009.11.021 ↗
19. Bonding of alkali- and heat-treated tantalum implants to bone10.1002/(SICI)1097-4636(2000)53:1<28::AID-JBM4>3.0.CO;2-F ↗
20. Erosion–corrosion of stainless steels, titanium, tantalum and zirconium10.1016/j.wear.2004.09.023 ↗
21. Mechanism of bonelike apatite formation on bioactive tantalum metal in a simulated body fluid10.1016/S0142-9612(01)00188-0 ↗
22. Novel bioactive materials with different mechanical properties10.1016/S0142-9612(03)00044-9 ↗
23. Biologic performance of tantalum10.1016/0267-6605(94)90113-9 ↗
24. Tantalum films for protective coating of steel10.1016/j.tsf.2004.04.041 ↗
25. Optimization of the sputtering process for the depositing composite thin films
26. Macro-effect of resputtering due to negative ion bombardment of growing thin films10.1557/JMR.1993.1928 ↗
27. Tantalum thin film deposited by ion assisted magnetron sputtering10.1016/j.tsf.2007.10.127 ↗
28. Phase formation and microstructure changes in tantalum thin films induced by bias sputtering10.1063/1.354946 ↗
29. The relationship between deposition conditions, the beta to alpha phase transformation, and stress relaxation in tantalum thin films10.1063/1.352059 ↗
30. In situ phase evolution study in magnetron sputtered tantalum thin films
31. Residual stress gradient analysis by the GIXRD method on CVD tantalum thin films10.1016/j.surfcoat.2004.12.018 ↗
32. Growth of nano crystalline near α phase tantalum films at room temperature using cylindrical magnetron cathode10.1016/j.surfcoat.2007.12.019 ↗
33. Sputter deposition of bcc tantalum films with TaN underlayers for protection of steel10.1016/j.tsf.2004.10.020 ↗
34. Preparation and properties of tantalum thin films10.1016/0040-6090(72)90365-3 ↗
35. Structure and electrical properties of Ta films sputtered in Ar–O210.1016/0040-6090(72)90273-8 ↗