journal article·2018-05

Hydrogen assisted cracking and CO2 corrosion behaviors of low-alloy steel with high strength used for armor layer of flexible pipe

Zhenguang Liu, Xiuhua Gao, Linxiu Du, Jianping Li, Xiaowei Zhou, Xiaonan Wang, Yuxin Wang, Chuan Liu, Guoxiang Xu, R.D.K. Misra

Publisher page

Abstract

Abstract In this study, hydrogen induced cracking (HIC), sulfide stress corrosion cracking (SSCC) and hydrogen embrittlement (HE) were carried out to study hydrogen assisted cracking behavior (HIC, SSCC and HE) of high strength pipeline steel used for armor layer of flexible pipe in ocean. The CO2 corrosion behavior of designed steel with high strength was studied by using immersion experiment. The experimental results demonstrate that the corrosion resistance of designed steel with tempered martensite to HIC, SSCC and HE is excellent according to specific standards, which contributes to the low concentration of dislocation and vacancies previously formed in cold rolling process. The corrosion mechanism of hydrogen induced cracking of designed steel, which involves in producing process, microstructure and cracking behavior, is proposed. The designed steel with tempered martensite shows excellent corrosion resistance to CO2 corrosion. Cr-rich compound was first formed on the coupon surface exposed to CO2-saturated brine condition and chlorine, one of the corrosion ions in solution, was rich in the inner layer of corrosion products.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Corrosion Behavior and Inhibition · Nuclear Materials and Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (94)

Show source-provided references
1. Comparative study on the stress corrosion cracking of X70 pipeline steel in simulated shallow and deep sea environments
2. Long-term under-deposit pitting corrosion of carbon steel pipes
3. Modeling localized corrosion of pipeline steels in oilfield produced water environments
4. Effect of exposure angle on the corrosion behavior of X70 steel under supercritical CO2 and gaseous CO2 environments
5. Effect of sulfide films formed on X65 steel surface on hydrogen permeation in H2S environments
6. Hydrogen-induced cracking and healing behaviour of X70 steel
7. The dual role of shot peening in hydrogen-assisted cracking of PSB1080 high strength steel
8. Sulfide stress corrosion study of a super martensitic stainless steel in H2S sour environments: Metallic sulfides formation and hydrogen embrittlement
9. Effect of microstructure and crystallography on sulfide stress cracking in API-5CT-C110 casing steel
10. Effect of the cathodic current density on the sub-surface concentration of hydrogen in X80 pipeline steels under cathodic protection
11. Hydrogen embrittlement of high strength pipeline steels
12. Investigation of hydrogen assisted cracking in acicular ferrite using site-specific micro-fracture tests
13. The effect of nanosized (Ti, Mo)C precipitates on hydrogen embrittlement of tempered lath martensitic steel
14. Identification of the hydrogen diffusion parameters in bearing steel by Evolutionary Algorithm
15. Composition optimization of high-strength steels for sulfide stress cracking resistance improvement
16. The influence of hydrogen on the mechanical and fracture properties of some martensitic advanced high strength steels studied using the linearly increasing stress test
17. Hydrogen embrittlement phenomena and mechanisms
18. Hydrogen embrittlement of steels turning of the research direction
19. Effect of free Cr content on corrosion behavior of 3Cr steels in a CO2 environment
20. Effect of impurity on the corrosion behavior of X65 steel in water-saturated supercritical CO2 system
21. CO2 corrosion resistance of carbon steel in relation with microstructure changes
22. Effect of Cr content on the corrosion performance of low-Cr alloy steel in a CO2 environment
23. Effect of temperature on the 3Cr low-alloyed steel initial corrosion behavior in CO2 solution
24. Effect of pressure on corrosion behavior of X60, X65, X70, and X80 carbon steels in water-unsaturated supercritical CO2 environments
25. The influence of pH on localized corrosion behavior of X65 carbon steel in CO2-saturated brines
26. Effect of impurities on the corrosion behavior of CO2 transmission pipeline steel in supercritical CO2-water environments
27. NACE TM 0283-2003, Evaluation of Pipeline and Pressure Vessel Steels for Resistance to Hydrogen-Induced Cracking, NACE International, Houston, Texas, United States.
28. NACE TM 0177-2005, Laboratory Testing of Metals for Resistance to Sulfide Stress Cracking and Stress Corrosion Cracking in H2S Environments, NACE International, Houston, Texas, United States.
29. ASTM F519-97, Standard Test Method for Mechanical Hydrogen Embrittlement Evaluation of Plating Processes and Service Environments, ASTM, West Conshohocken, Pennsylvania, United States.
30. Investigation of the effect of electrolytic hydrogen charging of X70 steel: I. The effect of microstructure on hydrogen-induced cold cracking and blistering
31. The effect of pre-strain on hydrogen embrittlement in 310S stainless steel
32. On the theory of CO2 corrosion reactions-Investigating their interrelationship with the corrosion products and API-X100 steel microstructure
33. Effect of grain size and dislocation density on the susceptibility to high-pressure hydrogen environment embrittlement of high-strength low-alloy steels
34. Recent developments in the study of hydrogen embrittlement, hydrogen effect on dislocation nucleation
35. Effects of annealing cooling rates on mechanical properties, microstructure and texture in continuous annealed IF steel
36. Evolution of the microstructure and texture of X70 pipeline steel during cold-rolling and annealing treatments
37. Effect of substructure on mechanical properties and fracture behavior of lath martensite in 0.1C–1.1Si-1.7Mn steel
38. The role of silicon in carbon partitioning processes in martensite/austenite microstructures
39. A comparative study of hydrogen induced cracking behavior in API 5L X60 and X70 pipeline steels
40. Color tint-etching for multiphase steels
41. Blister formation on 13Cr2MoNbVB ferritic-martensitic steel exposed to hydrogen plasma
42. Crack and blister initiation and growth in purified iron due to hydrogen loading
43. Effects of grain size and deformation temperature on hydrogen-enhanced vacancy formation in Ni alloys
44. Characterization of hydrogen induced cracking in TRIP-assisted steels
45. An extensive study of hydrogen-induced cracking susceptibility in an API X60 sour service pipeline steel
46. Effect of deformation and charging conditions on crack and blister formation during electrochemical hydrogen charging
47. A mechanistic theory of hydrogen embrittlement of steels
48. A new model for hydrogen-assisted cracking (hydrogen “embrittlement”)
49. Environmentally assisted cracking: overview of evidence for an adsorption-induced localised-slip process
50. The mechanism of hydrogen embrittlement in intercritically annealed medium Mn TRIP steel
51. Hydrogen embrittlement of austenitic stainless steels revealed by deformation microstructures and strain-induced creation of vacancies
52. Influence of cold deformation and annealing on hydrogen embrittlement of cold hardening bainitic steel for high strength bolts
53. Trap effect of vacancy on hydrogen diffusivity in bcc-Fe
54. Current issues in recrystallization: a review
55. Microstructure and deformation behavior of metastable duplex stainless steel at high rolling reductions
56. On the formation of vacancies in a-ferrite of a heavily cold-drawn pearlitic steel wire
57. Defects in carbon-rich ferrite of cold-drawn pearlitic steel wires
58. Dynamic recovery and dynamic recrystallization competition on a Nb- and N-bearing austenitic stainless steel biomaterial: influence of strain rate and temperature
59. Recrystallization behavior of a high-manganese steel: experiments and simulations
60. D.A. Porter, K.E. Easterling, Phases Transformation in Metal and Alloys, second ed. London, UK, 1993.
61. H.K.D.H. Bhadeshia, S.R. Honeycombe, Steels Microstructure and Properties, third ed. Oxford, UK, 2006.
62. Investigation of the effect of electrolytic hydrogen charging of X70 steel: II. Microstructural and crystallographic analyses of the formation of hydrogen induced cracks and blisters
63. Mechanisms of hydrogen trapping in austenitic, duplex, and super martensitic stainless steels
64. The mechanism of failure by hydrogen induced cracking in an acidic environment for API 5L X70 pipeline steel
65. A focus on different factors affecting hydrogen induced cracking in oil and natural gas pipeline steel
66. Investigating the effect of as-quenched vacancies in the final microstructure of 1.2080 tool steel during the deep cryogenic heat treatment
67. Effect of diffusion coefficient variation on interrelation between hydrogen diffusion and induced internal stress in hydrogen storage alloys
68. Hydrogen chemical potentials and diffusion coefficients in hydrogen diffusion membranes
69. G.L. Turconi, G. Echaniz, G. Cumino, E. Anelli, L. Scoppio, T. Perez, C. Morales, Improvement of Resistance to SSC Initiation and Propagation of High Strength OCTG through Microstructure and Precipitation Control, Corrosion/2001, NACE, Houston, TX, Paper No. 01077.
70. Effect of quenching and tempering process on sulfide stress cracking susceptibility in API-5CT-C110 casing steel
71. Strengthening mechanisms of precipitates in S30432 heatresistant steel during short-term aging
72. Grain boundary effect on diffusion of hydrogen in pure aluminum
73. Hydrogen-induced crack growth rate in steel plates exposed to sour environments
74. Hydrogen electrode reaction and hydrogen embrittlement of mild steel in hydrogen sulfide solutions
75. Anodized porous titanium coated with Ni-CeO2 deposits for enhancing surface toughness and wear resistance
76. Partial oxidation of TiN coating by hydrothermal treatment and ozone treatment to improve its osteoconductivity
77. Evaluation of the micro-arc oxidation treatment effect on the protective performance of a Mg-rich epoxy coating on AZ91D magnesium alloy
78. Preparation and high temperature performance of Co-10Mn and Co-40Mn alloy coatings for solid oxide fuel cell metal interconnects
79. Corrosion behaviour of low-alloy martensite steel exposed to vapour-saturated CO2 and CO2-saturated brine conditions
80. Corrosion behavior of low-alloy steel with martensite/ferrite microstructure at vapor-saturated CO2 and CO2-saturated brine conditions
81. Corrosion behavior of low-alloy steel used for pipeline at vapor-saturated CO2 and CO2-saturated brine conditions
82. Corrosion behavior of low-alloy pipeline steel with 1% Cr under CO2 condition
83. Corrosion behavior of low alloy pipeline steel in saline solution saturated with supercritical carbon dioxide
84. Comparison of corrosion behavior of low-alloy pipeline steel exposed to H2S/CO2-saturated brine and vapor-saturated H2S/CO2 environments
85. Comparison of corrosion behaviors of low-alloy steel exposed to vapor-saturated H2S/CO2 and H2S/CO2-saturated brine environments
86. Corrosion behaviour of low-alloy steel with titanium addition exposed to seawater environment
87. Corrosion behaviour of low-alloy pipeline steel exposed to H2S/CO2-saturated saline solution
88. Corrosion behaviour of steels for CO2 injection
89. Reactions of pipeline steel in carbon dioxide solution
90. The growth mechanism of CO2 corrosion product films
91. Reliability of pipe steels with different amounts of C and Cr during onshore carbon dioxide injection
92. Corrosion of Cr bearing low alloy pipeline steel in CO2 environment at static and flowing conditions
93. Corrosion of low alloy steel and stainless steel in supercritical CO2/H2O/H2S systems
94. Effects of chloride content on CO2 corrosion of carbon steel in simulated oil and gas well environments