Corrosion investigation of fire-gilded bronze involving high surface resolution spectroscopic imaging
Source abstract
Abstract
Gilded bronzes are often affected by severe corrosion, due to defects in the Au layer and Au/Cu alloygalvanic coupling, stimulated by large cathodic area of the gilded layer. Galvanic corrosion, triggered by gilding defects, leads to products growth at the Au/bronze interface, inducing blistering or break-up of the Au layer. In this context, fire-gilded bronze replicas prepared by ancient methods (use of spreadableAu–Hg paste) was specifically characterised by compiling complementary spectroscopic and imaging information before/after accelerated ageing with synthetic rain. Fire-gilded bronze samples were chemically imaged in cross-section at nanometric scale (<200 nm) using high energy and lateral resolution synchrotron radiation photoemission (HR-SRPES) of core levels and valence band after conventional characterisation of the samples by Glow Discharge optical Emission Spectroscopy (GD-OES) and conventional X-ray photoelectron spectroscopy (XPS). We have found a net surface enrichment in Zn and Snafter fire-gilding and presence of metallic Hg, Pb and Cu within the Au layer. Moreover, the composition distribution of the elements together with their oxidation has been determined. It was also revealed that metallic phases including Hg and Pb remain in the gilding after corrosion. Moreover, selective dissolution of Zn and Cu occurs in the crater due to galvanic coupling, which locally induces relative Sn species enrichment (decuprification). The feasibility advantages and disadvantages of chemical imaging using HR-SRPES to study artworks have been investigated on representative replicas.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Electron and X-Ray Spectroscopy Techniques · Ion-surface interactions and analysis · Corrosion Behavior and Inhibition
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (62)
Show source-provided references
1. Gilding for matter decoration and sublimation. A brief hisotry of the artisanal technical know-how
2. The surface enrichment of carat gold alloys—depletion gilding
3. Gilding of metals in the old world
4. The practice and characterization of historic fire gilding techniques10.1007/s11837-997-0015-6 ↗
5. Atmospheric corrosion of fire-gilded bronze: corrosion and corrosion protection during accelerated ageing tests10.1016/j.corsci.2015.08.013 ↗
6. The gilding of Lorenzo Ghiberti's “Doors of Paradise"10.1007/BF03214652 ↗
7. Analyses of the patinas of a gilded horse of St Mark's Basilica in Venice: corrosion mechanisms and conservation problems
8. The condition of the “Door of Paradise” by L. Ghiberti. Tests and proposals for cleaning
9. On the conservation of the Baptistery doors in Florence10.1179/sic.1979.013 ↗
10. The Gate of Paradise: Physical optimization of the laser cleaning approach10.1179/sic.2001.46.4.269 ↗
11. The gilded bronze Paradise Doors by Ghiberti in the florence baptistery: scientific investigation and problems of restoration
12. Effectiveness of some inhibitors on the atmospheric corrosion of gold plated bronzes
13. Behaviour of a galvanic cell simulating the atmospheric corrosion conditions of gold plated bronzes10.1016/0010-938X(77)90007-5 ↗
14. Laser cleaning methodology for the preservation of the Porta del Paradiso by Lorenzo Ghiberti10.1016/S1296-2074(02)01138-X ↗
15. Laser and chemical cleaning tests for the conservation of the Porta del Paradiso by Lorenzo Ghiberti10.1016/S1296-2074(02)01190-1 ↗
16. Setup of galvanic sensors for the monitoring of gilded bronzes10.3390/s140407066 ↗
17. The monument of Marcus Aurelius: research and conservation
18. Gli studi per la protezione del Marco Aurelio
19. The atmospheric corrosion of quaternary bronzes: the leaching action of acid rain10.1016/j.corsci.2008.10.008 ↗
20. Surface spectroscopic studies on patinas of ancient metal objects10.1179/sic.1984.29.4.172 ↗
21. Surface and interface microchemistry of archaeological objects studied with x-ray photoemission spectroscopy and scanning Auger microscopy10.1016/0368-2048(95)02429-8 ↗
22. X-ray photoelectron spectroscopy and scanning Auger microscopy studies of bronzes from the collections of the Vatican Museums10.1016/S0042-207X(99)00124-4 ↗
23. Effect of dopants on the electronic structure of SnO2 thin film10.1016/S0925-4005(00)00347-6 ↗
24. Organic substances at metal surfaces: archaeological evidence and the elder Pliny's account
25. Characterization of artificially produced copper and bronze patina by XPS10.1002/1096-9918(200008)30:1<135::AID-SIA720>3.0.CO;2-V ↗
26. Characterisation by XPS of the corrosion patina formed on bronze surfaces10.1016/S1296-2074(02)01179-2 ↗
27. Multianalytical in situ investigation of the initial atmospheric corrosion of bronze10.1016/S0010-938X(01)00083-X ↗
28. Characterization of the patina formed on a low tin bronze exposed to aqueous hydrogen sulfide10.1002/sia.5520 ↗
29. X-ray photoemission investigation of the corrosion film formed on a polished Cu–13Sn alloy in aerated NaCl solution10.1016/S0169-4332(01)00023-X ↗
30. Characterisation of anodic layers on Cu–10Sn bronze (RDE) in aerated NaCl solution10.1016/j.corsci.2008.06.003 ↗
31. Possibility of bacteria-induced corrosion of ancient bronze mirrors found in ground10.2320/matertrans.44.268 ↗
32. Production of reference “ancient” Cu-based alloys and their accelerated degradation methods10.1007/s00339-006-3545-9 ↗
33. Production of reference alloys for the conservation of archaeological silver-based artifacts10.1007/s00339-010-5677-1 ↗
34. Dynamic secondary ion mass spectrometry and X-ray photoelectron spectroscopy on artistic bronze and copper artificial patinas10.1016/j.apsusc.2009.02.020 ↗
35. The characterization of a new pale blue corrosion product found on copper alloy artifacts10.1179/sic.2002.47.4.217 ↗
36. XPS characterization of (copper-based) coloured stains formed on limestone surfaces of outdoor Roman monuments10.1186/1752-153X-6-S2-S10 ↗
37. The films on bronze surface formed by AMT composite regent through XPS and AES methods
38. Surface characterisation of corrosion inhibitors on bronzes for artistic casting10.1533/9781845693015.335 ↗
39. Combined PIXE and XPS analysis on republican and imperial Roman coins10.1016/S0168-583X(99)00965-9 ↗
40. Combined use of XPS and SEM+EDS for the study of surface microchemical structure of archaeological bronze Roman mirrors10.1002/sia.1789 ↗
41. A multitechnique study of archeological bronzes10.1002/sia.2647 ↗
42. A multitechnique study of archaeological bronzes: Part II10.1002/sia.3642 ↗
43. Unusual surface degradation products grown on archaeological bronze artefacts10.1007/s00339-013-7771-7 ↗
44. An investigation on the patina of ancient bronze coins10.1080/10420150.2014.910209 ↗
45. Ancient mercury-based plating methods: combined use of surface analytical techniques for the study of manufacturing process and degradation phenomena10.1021/ar300232e ↗
46. Colorando Auro: Contribution to the understanding of a medieval recipe to colour gilded silver plates10.1007/s00339-012-7532-z ↗
47. Effectiveness of corrosion inhibitor films for the conservation of bronzes and gilded bronzes10.1016/j.corsci.2012.03.003 ↗
48. Cellini · 1927
49. Interferometer-controlled soft X-ray scanning photoemission microscope at SOLEIL10.1088/1742-6596/425/13/132013 ↗
50. ANTARES, a scanning photoemission microscopy beamline at SOLEIL10.1088/1742-6596/425/19/192023 ↗
51. Cross-interaction between Au and Cu in Au/Sn/Cu ternary diffusion couples10.1007/BF02692458 ↗
52. Diffusion-related behaviour of gold in thin film systems10.1007/BF03216542 ↗
53. Identification of ancient gilding technology and Late Bronze Age metallurgy by EDXRF, Micro-EDXRF, SEM-EDS and metallographic techniques10.1007/s00604-009-0284-6 ↗
54. Corrosion chemistry of gilded silver and copper
55. Characterization of surface oxide films on titanium and adhesion of osteoblast10.1016/S0142-9612(03)00366-1 ↗
56. An XPS and AES study of the free corrosion of Cu-, Ni- and Zn-based alloys in synthetic sweat10.1016/S0010-938X(98)00141-3 ↗
57. ASM International · 1992
58. A global approach to the authentication of ancient bronzes based on the characterization of the alloy–patina–environment system10.1016/j.culher.2005.11.001 ↗
59. Mechanism of dissolution of a Cu–13Sn alloy in low aggressive conditions10.1016/S0010-938X(02)00207-X ↗
60. X-ray photoemission study of soldered lead materials relevance to the surface and interface chemical composition of Roman lead pipes “fistulae"10.1016/S0042-207X(97)00149-8 ↗
61. Study of the effect of acetic acid vapor on copper corrosion at 40 and 80% relative humidity10.1149/1.1404968 ↗
62. Composition and electrochemical properties of natural patinas of outdoor bronze monuments10.1016/j.electacta.2006.12.053 ↗