Effects of microstructure and mechanical properties on cavitation erosion resistance of NiCrWMoCuCBFe coatings
Source abstract
Abstract
Abstract NiCrWMoCuCBFe coatings were prepared by high velocity oxy-fuel (HVOF) spraying technology with the microstructures and mechanical properties characterized in detail. Besides, an ultrasonic vibratory apparatus was employed to investigate the cavitation erosion resistance of the coating in deionized water and its cavitation erosion mechanism was revealed. The results show that there were some inherent defects existed on the coating surface but its microhardness was more than triple that of 316 L stainless steel. In the initial stage of cavitation erosion, these inherent defects of coating surfaces were damaged at first, leading the incubation period of the coating was shorter than 10 min. With the prolongation of cavitation erosion time, many cracks interpenetrated and finally led to the exfoliation of coatings. When the cavitation erosion time extended to 10 h, the erosion rate of the coating was almost stable and reached maximum about 1.32 ± 0.08 μm/h, which was less than that of 316 L stainless steel (2.62 ± 0.18 μm/h). That is, the inherent defects influenced the cavitation erosion resistance in the incubation period of the coating but the mechanical properties played a dominant role in the long-term cavitation erosion of the coating.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced materials and composites · High-Temperature Coating Behaviors · Erosion and Abrasive Machining
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (41)
Show source-provided references
1. Cavitation erosion risk indicators for a thin gap within a diesel fuel pump10.1016/j.wear.2019.203024 ↗
2. Cavitation erosion in hydraulic turbine components and mitigation by coatings: current status and future needs10.1007/s11665-011-0051-9 ↗
3. Large Eddy Simulation of Diesel injector including cavitation effects and correlation to erosion damage10.1016/j.fuel.2016.02.037 ↗
4. Visualization and measurements of shock waves in cavitating flow10.1016/j.expthermflusci.2020.110215 ↗
5. Analysis of the effect of impact of near-wall acoustic bubble collapse micro-jet on Al 106010.1016/j.ultsonch.2016.12.030 ↗
6. Cavitation erosion by single laser-produced bubbles10.1017/S0022112098008738 ↗
7. A ring area formed around the erosion pit on 1Cr18Ni9Ti stainless steel surface in incipient cavitation erosion10.1016/j.wear.2008.08.002 ↗
8. Theoretical estimation of the temperature and pressure within collapsing acoustical bubbles10.1016/j.ultsonch.2013.05.008 ↗
9. Quo VadisThermal Spraying?10.1361/105996301770349510 ↗
10. Deposition and cavitation erosion behavior of multimodal WC-10Co4Cr coatings sprayed by HVOF10.1016/j.surfcoat.2020.125757 ↗
11. Cavitation erosion of several oxy-fuel sprayed coatings tested in deionized water and artificial seawater10.1016/j.wear.2013.12.026 ↗
12. Effect of flow velocity on cavitation erosion behavior of HVOF sprayed WC-10Ni and WC-20Cr3C2–7Ni coatings10.1016/j.ijrmhm.2020.105330 ↗
13. Cavitation erosion resistance in NaCl medium of HVOF sprayed WC-based cermet coatings at various flow velocities: a comparative study on the effect of Ni and CoCr binder phases10.1016/j.ijrmhm.2020.105407 ↗
14. Performance analysis of cavitation erosion resistance and corrosion behavior of HVOF-sprayed WC-10Co-4Cr, WC-12Co, and Cr3C2-NiCr coatings10.1007/s11666-020-00994-y ↗
15. Evaluation of cavitation/corrosion synergy of the Cr3C2-25NiCr coating deposited by HVOF process10.1016/j.ultsonch.2020.105271 ↗
16. Erosion wear performance of WC-10Co4Cr and Cr3C2-25NiCr coatings sprayed with high-velocity thermal spray processes10.1016/j.surfcoat.2019.04.067 ↗
17. Microstructure and cavitation erosion behavior of HVOF sprayed ceramic-metal composite coatings for application in hydro-turbines10.1016/j.renene.2020.08.099 ↗
18. Cavitation erosion mechanisms in stainless steels and in composite metal–ceramic HVOF coatings10.1016/j.wear.2016.07.015 ↗
19. In-situ SEM observations of ultrasonic cavitation erosion behavior of HVOF-sprayed coatings10.1016/j.ultsonch.2019.104760 ↗
20. Microwave-assisted post-processing of detonation gun-sprayed coatings for better slurry and cavitation erosion resistance10.1007/s11666-019-00914-9 ↗
21. Increased lifetime for biomass and waste to energy power plant boilers with HVOF coatings: high temperature corrosion testing under chlorine-containing molten salt10.1007/s11666-013-9928-5 ↗
22. Effects of Mo on the evolution of microstructures and mechanical properties in Co-Al-W base superalloys10.1016/j.msea.2018.11.087 ↗
23. Influence of Mo and W on high temperature hardness of M7C3 carbide in high chromium white cast iron10.2320/matertrans.F-M2014801 ↗
24. Effect of carbon content on microstructure, hardness and wear resistance of CoCrFeMnNiCx high-entropy alloys10.1016/j.jallcom.2020.156533 ↗
25. The interaction mechanism of cavitation erosion and corrosion on HVOF sprayed NiCrWMoCuCBFe coating in artificial seawater10.1016/j.apsusc.2020.146499 ↗
26. Measurement of hardness and elastic modulus by instrumented indentation: advances in understanding and refinements to methodology10.1557/jmr.2004.19.1.3 ↗
27. An improved technique for determining hardness and elastic modulus using load and displacement sensing indentation experiments10.1557/JMR.1992.1564 ↗
28. ASTM. International, Standard Test Method for Cavitation Erosion Using Vibratory Apparatus, in: ASTM G32-16, 2016.
29. On the recent development in production technology of alloy powders10.2320/matertrans1989.31.363 ↗
30. Study on stainless steel 316L coatings sprayed by a novel high pressure HVOF10.1016/j.surfcoat.2013.11.018 ↗
31. Effect of annealing treatment on microstructures, mechanical properties and cavitation erosion performance of high velocity oxy-fuel sprayed NiCoCrAlYTa coating10.1016/j.jmst.2020.03.030 ↗
32. Residual stress in HVOF thermally sprayed WC-10Co-4Cr coating in landing gear application10.1007/s11666-019-00894-w ↗
33. Inhomogeneous dislocation distributions and the formation of dislocation cell structure
34. Fundamentals of cell and subgrain structures in historical perspective10.1016/0956-716X(92)90455-N ↗
35. Correlation between cavitation erosion resistance and cyclic mechanical properties of different metallic materials10.1088/1742-6596/843/1/012037 ↗
36. Towards numerical prediction of cavitation erosion, Interface
37. Application of spherical nanoindentation to determine the pressure of cavitation impacts from pitting tests10.1557/jmr.2011.259 ↗
38. The coupling effect of immersion corrosion and cavitation erosion of NiCoCrAlYTa coatings in artificial seawater10.1016/j.corsci.2020.108635 ↗
39. Tribology of FeVCrC coatings deposited by HVOF and HVAF thermal spray processes10.1016/j.wear.2017.10.014 ↗
40. Cavitation erosion behavior of Hastelloy C-276 nickel-based alloy10.1016/j.jallcom.2014.08.248 ↗
41. Cavitation erosion behavior of 316L stainless steel10.1007/s11249-019-1225-0 ↗