journal article·2022-04

A facile hydrophilic modification strategy initiated by flame treatment of silicone coatings for marine antifouling application

Xingyang Xu, Rongrong Chen, Gaohui Sun, Jing Yu, Qi Liu, Jingyuan Liu, Cunguo Lin, Peili Liu, Jun Wang

Publisher page

Abstract

Highlight • Flame treatment showed the potential of modificating PDMS by oxidize the surface. • Sulfobetaine silane modifiction initiated by flame increased antifouling property. • PVA layer cured by boric acid enhance antifouling property of flame-treated PDMS. Non-toxic poly(dimethylsiloxane) (PDMS) elastomer antifouling coatings are used to protect marine equipment from biofouling; however, the coatings cannot resist all fouling organisms. Hydrophilic modification is an effective way to enhance antifouling performances in PDMS but most modification methods are complex and inconvenient. In this work, flame treatment was used to replace other complex surface activation techniques, such as plasmas. The sulfobetaine silane and polyvinyl alcohol (PVA) modifications were developed for flame treatment. The sulfobetaine silane-modified flame-treated PDMS reduced diatom adhesion by 99.0% compared to untreated PDMS. The PVA modification involves a two-step spray process and is simpler than sulfobetaine silane modification. This strategy coats PVA on flame-treated PDMS through the crosslinking effect of boric acid on PVA, which reduced diatom adhesion by 86.6% in the lab and gave better antifouling performances in field tests compare to bare PDMS.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Marine Biology and Environmental Chemistry · Microplastics and Plastic Pollution · Polymer Surface Interaction Studies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (43)

Show source-provided references
1. Impact of diatomaceous biofilms on the frictional drag of fouling-release coatings10.1080/08927014.2015.1108407 ↗
2. Microbiologically influenced corrosion: Looking to the future
3. Biofouling protection for marine environmental sensors10.5194/os-6-503-2010 ↗
4. Evaluation of heavy metals background in the adriatic sea sediments of abruzzo region, Italy10.1016/j.scitotenv.2019.05.350 ↗
5. Organotin contamination in commercial and wild oysters from china: Increasing occurrence of triphenyltin10.1016/j.scitotenv.2018.09.310 ↗
6. Toxic effects of tributyltin and its metabolites on harbour seal (phoca vitulina) immune cells in vitro10.1016/j.aquatox.2008.09.005 ↗
7. Preliminary study of cellular metal accumulation in two antarctic marine microalgae - implications for mixture interactivity and dietary risk10.1016/j.envpol.2019.06.003 ↗
8. Recent developments and applications of protective silicone coatings: A review of pdms functional materials10.1016/j.porgcoat.2017.05.012 ↗
9. Designing biomimetic antifouling surfaces10.1098/rsta.2010.0195 ↗
10. Combinatorial materials research applied to the development of new surface coatings ix: An investigation of novel antifouling/fouling-release coatings containing quaternary ammonium salt groups10.1080/08927010801894660 ↗
11. Self-repairing silicone coatings for marine anti-biofouling10.1039/C7TA05241C ↗
12. Amphiphilic surface active triblock copolymers with mixed hydrophobic and hydrophilic side chains for tuned marine fouling-release properties10.1021/la100032n ↗
13. Zwitterionic siloxane-polyurethane fouling-release coatings10.1016/j.porgcoat.2014.07.011 ↗
14. Prevention of bacterial colonization on catheters by a one-step coating process involving an antibiofouling polymer in water10.1021/acsami.7b06899 ↗
15. Non-toxic, non-biocide-release antifouling coatings based on molecular structure design for marine applications10.1039/C5TB00232J ↗
16. Surface structures of pdms incorporated with quaternary ammonium salts designed for antibiofouling and fouling release applications10.1021/la304571u ↗
17. Hydration and chain entanglement determines the optimum thickness of poly(hema-co-peg(1)(0)ma) brushes for effective resistance to settlement and adhesion of marine fouling organisms10.1021/am502084x ↗
18. Contribution of charges in polyvinyl alcohol networks to marine antifouling10.1021/acsami.7b04079 ↗
19. Ultralow-fouling, functionalizable, and hydrolyzable zwitterionic materials and their derivatives for biological applications10.1002/adma.200901407 ↗
20. Antifouling coatings: Recent developments in the design of surfaces that prevent fouling by proteins, bacteria, and marine organisms10.1002/adma.201001215 ↗
21. Engineering high-effective antifouling polyether sulfone membrane with p(peg-pdms-kh570)@sio 2 nanocomposite via in-situ sol-gel process10.1016/j.cej.2017.03.105 ↗
22. Novel silicone hydrogel based on pdms and pegma for contact lens application10.1016/j.colsurfb.2014.10.053 ↗
23. Silica nanoparticles functionalized with zwitterionic sulfobetaine siloxane for application as a versatile antifouling coating system10.1021/acsami.7b04840 ↗
24. Charged hydrophilic polymer brushes and their relevance for understanding marine biofouling10.1080/08927014.2016.1170816 ↗
25. Molecular understanding and design of zwitterionic materials10.1002/adma.201404059 ↗
26. Achieving ultralow fouling under ambient conditions via surface-initiated arget atrp of carboxybetaine10.1021/acsami.7b01530 ↗
27. Effect of sequential layer-by-layer surface modifications on the surface energy of plasma-modified poly(dimethylsiloxane)10.1021/la062281f ↗
28. Modification of silicone elastomer with zwitterionic silane for durable antifouling properties10.1021/la502486e ↗
29. Stability of polyethylene glycol and zwitterionic surface modifications in pdms microfluidic flow chambers10.1021/acs.langmuir.7b03095 ↗
30. Hydrogel brushes grafted from stainless steel via surface-initiated atom transfer radical polymerization for marine antifouling10.1016/j.apsusc.2016.03.223 ↗
31. Microtopographic cues for settlement of zoospores of the green fouling alga enteromorpha10.1080/08927010290014908 ↗
32. Development and testing of hierarchically wrinkled coatings for marine antifouling10.1021/am9000562 ↗
33. Biomimicking micropatterned surfaces and their effect on marine biofouling10.1021/la502006s ↗
34. Engineered antifouling microtopographies - effect of feature size, geometry, and roughness on settlement of zoospores of the green alga ulva10.1080/08927010601136957 ↗
35. Using textured pdms to prevent settlement and enhance release of marine fouling organisms10.1080/08927014.2013.836507 ↗
36. Species-specific engineered antifouling topographies: Correlations between the settlement of algal zoospores and barnacle cyprids10.1080/08927010701393276 ↗
37. Non-elastic glassy coating with fouling release and resistance abilities10.1039/C9TA09794E ↗
38. Ecofriendly antifouling marine coatings10.1021/sc500845n ↗
39. Effect of variations in micropatterns and surface modulus on marine fouling of engineering polymers, ACS Appl10.1021/acsami.6b14262 ↗
40. Design and characterization of sulfobetaine-containing terpolymer biomaterials10.1016/j.actbio.2012.03.052 ↗
41. Thermal processing of silicones for green, scalable, and healable superhydrophobic coatings10.1002/adma.201506446 ↗
42. Surface modification of sylgard-184 poly(dimethyl siloxane) networks by ultraviolet and ultraviolet/ozone treatment10.1006/jcis.2002.8594 ↗
43. Mechanical factors favoring release from fouling release coatings10.1080/08927010009386299 ↗